Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Surface Resistance = 1.00e+16 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Surface Resistance 1.00e+15 - 1.00e+16 ohm
1.00e+15 - 1.00e+16 ohm
ASTM D257
SABIC Innovative Plastics Lexan® 905 PC Copolymer (Asia Pacific)
Lexan 905 resin is a high flow, opaque, flame retardant polycarbonate resin blend. It is designed with non-chlorinated, non-brominated FR systems with UL-94 listing of both V0 and 5V ratings. Its ex..
Surface Resistance 1000 - 1.00e+16 ohm
1000 - 1.00e+16 ohm
Average value: 7.69e+14 ohm Grade Count:9
Overview of materials for PETG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Surface Resistance 1.00e+15 - 1.00e+16 ohm
1.00e+15 - 1.00e+16 ohm
Average value: 5.50e+15 ohm Grade Count:4
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
Surface Resistance 10000 - 1.00e+16 ohm
10000 - 1.00e+16 ohm
Average value: 5.36e+14 ohm Grade Count:41
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Surface Resistance 10.0 - 1.00e+16 ohm
10.0 - 1.00e+16 ohm
Average value: 3.03e+15 ohm Grade Count:184
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Surface Resistance 1000 - 1.00e+16 ohm
1000 - 1.00e+16 ohm
Average value: 2.33e+15 ohm Grade Count:13
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Surface Resistance 1.00e+14 - 1.00e+16 ohm
1.00e+14 - 1.00e+16 ohm
Average value: 1.00e+15 ohm Grade Count:19
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Surface Resistance 1.00e+9 - 1.00e+16 ohm
1.00e+9 - 1.00e+16 ohm
Average value: 1.03e+15 ohm Grade Count:24
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Surface Resistance 1.00e+15 - 1.00e+16 ohm
1.00e+15 - 1.00e+16 ohm
ASTM D 257
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific)
Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di..
Surface Resistance 10000 - 1.00e+16 ohm
10000 - 1.00e+16 ohm
Average value: 3.92e+15 ohm Grade Count:26
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Surface Resistance 1.00e+9 - 1.00e+16 ohm
1.00e+9 - 1.00e+16 ohm
Average value: 2.84e+15 ohm Grade Count:19
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Surface Resistance 2000 - 1.00e+16 ohm
2000 - 1.00e+16 ohm
Average value: 8.84e+14 ohm Grade Count:35
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Surface Resistance 1.00e+9 - 1.00e+16 ohm
1.00e+9 - 1.00e+16 ohm
Average value: 8.68e+14 ohm Grade Count:29
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Surface Resistance 1000 - 1.00e+16 ohm
1000 - 1.00e+16 ohm
Average value: 1.30e+15 ohm Grade Count:33
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..
Surface Resistance 1.00e+12 - 1.00e+16 ohm
1.00e+12 - 1.00e+16 ohm
Average value: 1.66e+15 ohm Grade Count:10
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Surface Resistance 1.00e+15 - 1.00e+16 ohm
1.00e+15 - 1.00e+16 ohm
Average value: 4.56e+15 ohm Grade Count:5
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..
Surface Resistance 3000 - 1.00e+16 ohm
3000 - 1.00e+16 ohm
Average value: 4.88e+15 ohm Grade Count:24
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..
Surface Resistance 1.00e+10 - 1.00e+16 ohm
1.00e+10 - 1.00e+16 ohm
Average value: 1.56e+15 ohm Grade Count:19
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Surface Resistance 1.00e+10 - 1.00e+16 ohm
1.00e+10 - 1.00e+16 ohm
Average value: 1.45e+15 ohm Grade Count:23
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
Surface Resistance 1.00 - 1.00e+16 ohm
1.00 - 1.00e+16 ohm
Average value: 8.14e+14 ohm Grade Count:69
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Surface Resistance 100 - 1.00e+16 ohm
100 - 1.00e+16 ohm
Average value: 5.18e+14 ohm Grade Count:35
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Surface Resistance 1.00 - 1.00e+16 ohm
1.00 - 1.00e+16 ohm
Average value: 9.40e+14 ohm Grade Count:113
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Surface Resistance 1.00e+10 - 1.00e+16 ohm
1.00e+10 - 1.00e+16 ohm
Average value: 5.11e+14 ohm Grade Count:20
Overview of materials for Nylon 66, 60% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. ..
Surface Resistance 1.00e+8 - 1.00e+16 ohm
1.00e+8 - 1.00e+16 ohm
Average value: 7.50e+15 ohm Grade Count:4
Overview of materials for Nylon 66, 10% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ..
Surface Resistance 1.00e+15 - 1.00e+16 ohm
<br>@Temperature 23.0 °C
1.00e+15 - 1.00e+16 ohm
<br>@Temperature 73.4 °F
ASTM D257
DuPont Performance Polymers VESPEL TP-8054 Polyimide
DuPont Vespel TP-8054 parts are specified for high-temperature applications requiring a balance of mechanical and thermal properties. TP-8054 parts are produced from unreinforced thermoplastic polyi..
Surface Resistance 1.00e+15 - 1.00e+16 ohm
<br>@Temperature 23.0 °C
1.00e+15 - 1.00e+16 ohm
<br>@Temperature 73.4 °F
ASTM D257
DuPont Performance Polymers VESPEL TP-8161 Polyimide
DuPont Vespel TP-8161 parts are specified for high-temperature applications. TP-8161 parts offer a unique balance of mechanical and thermal properties for superior performance in aggressive environm..
Surface Resistance 1.00e+10 - 1.00e+16 ohm
1.00e+10 - 1.00e+16 ohm
Average value: 8.03e+14 ohm Grade Count:15
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Surface Resistance 1.00e+6 - 1.00e+16 ohm
1.00e+6 - 1.00e+16 ohm
Average value: 1.70e+15 ohm Grade Count:20
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
Surface Resistance 1000 - 1.00e+16 ohm
1000 - 1.00e+16 ohm
Average value: 2.31e+15 ohm Grade Count:45
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
Surface Resistance 260 - 1.00e+16 ohm
260 - 1.00e+16 ohm
Average value: 2.08e+15 ohm Grade Count:30
Overview of materials for Acetal Copolymer, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values..
Copyright © lookpolymers.com All Rights Reserved