| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
|
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Europe-Africa-Middle East)
XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
|
|||
| Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
|
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Europe-Africa-Middle East)
XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
|
|||
| Surface Resistance |
1.00e+17
ohm @Temperature 23.0 °C |
1.00e+17
ohm @Temperature 73.4 °F |
IEC 60093 |
|
DuPont Performance Polymers Crastin® HR5315HF BK503 PBT
(Unverified Data**)
Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis..
|
|||
| Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | IEC 60093 |
|
3M Dyneon™ TFM™ 1605 Modified PTFE Powder
(discontinued **)
Type III, gr. 2 PTFE. Second-generation PTFE that is a chemically modified to allow new designs and processing methods. Very good free-flowing powder properties.Data provided by Dyneon.
|
|||
| Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | IEC 60093 |
|
3M Dyneon™ TF 2071 PTFE Paste Extrusion Powder
(discontinued **)
Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 1600. Average particle size 500 µm. Used for tubing, wire/cable insulation, 'spaghetti tubing' production.Dyneon offers a..
|
|||
| Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | IEC 60093 |
|
3M Dyneon™ TF 2072 PTFE Paste Extrusion Powder
(discontinued **)
Type I PTFE. Free flowing powder. Minimum reduction ratio is 50; Max is 3000. Average particle size 500 µm. Used for wire/cable insulation, 'spaghetti tubing' production.Dyneon offers a family ..
|
|||
| Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
|
Manifattura Cattaneo PTFE Polytetrafluoroethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
|
|||
| Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | IEC 60093 |
|
Lanxess Pocan® BF 4232 000000 PBT, 30% Glass Fiber
PBT, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS.
|
|||
| Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
|
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
|
|||
| Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
|
Techmer ES HiFill FR® PC FR SFX-ORANGE 1.0
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantAppearance: OrangeInformation provided by TP Composites, Inc.
|
|||
| Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
|
Techmer ES HiFill FR® PC FR SFX-GREEN 1.0
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantAppearance: GreenInformation provided by TP Composites, Inc.
|
|||
| Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM3020 PPE+HIPS (Europe-Africa-Middle East)
LNP* Thermocomp* Noryl_HM3020 compound is a 30% Glass/Mineral filled, high modulus grade. DTUL 248F (120C). UL94 V-1/5VA rated in black and gray.
|
|||
| Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
|
Cosmic Plastics 6220 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||
| Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
|
Cosmic Plastics K77 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||
| Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
|
Dalau Dalcon 086 100% Virgin PTFE modified polymer
Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal ..
|
|||
| Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | IEC 60093 |
|
Polyplastics FR-PET® BLR6001MZ Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET)
Information provided by PolyPlastics.
|
|||
| Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | IEC 60093 |
|
Polyplastics FR-PET® C3015FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
Information provided by PolyPlastics.
|
|||
| Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | IEC 60093 |
|
Polyplastics FR-PET® C3030FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
Information provided by PolyPlastics.
|
|||
| Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | IEC 60093 |
|
Polyplastics FR-PET® CN9015 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose
Information provided by PolyPlastics.
|
|||
| Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
|
Cosmic Plastics D72 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||
| Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | IEC 60093 |
|
Polyplastics Duranex® 701SA Polybutylene Terephthalate (PBT), Low density, Low wear, GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
|
|||
| Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
|
Cosmic Plastics 6120F Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||
| Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
|
Cosmic Plastics 224 Dacron Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||
| Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
|
Cosmic Plastics 6130 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||