| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 10000 - 1.00e+6 ohm | 10000 - 1.00e+6 ohm | 10 volts; ASTM D4496 |
|
Omni Plastics OmniTech™ CPP XE72-A BK17 ESD Polypropylene Conductive
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and ..
|
|||
| Surface Resistance | 1.00 - 1.00e+6 ohm | 1.00 - 1.00e+6 ohm | Average value: 75200 ohm Grade Count:7 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte..
|
|||
| Surface Resistance | 3.00 - 1.00e+6 ohm | 3.00 - 1.00e+6 ohm | Average value: 376000 ohm Grade Count:5 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m..
|
|||
| Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | Average value: 72900 ohm Grade Count:14 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini..
|
|||
| Surface Resistance | 1.00 - 1.00e+6 ohm | 1.00 - 1.00e+6 ohm | Average value: 48800 ohm Grade Count:16 |
|
Overview of materials for Polyphenylene Sulfide (PPS), Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum ..
|
|||
| Surface Resistance | 1.00 - 1.00e+6 ohm | 1.00 - 1.00e+6 ohm | Average value: 117000 ohm Grade Count:10 |
|
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim..
|
|||
| Surface Resistance | 10000 - 1.00e+6 ohm | 10000 - 1.00e+6 ohm | ASTM D257 |
|
Techmer ES Electrablend® ABS SS5 FR 5% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Compo..
|
|||
| Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
|
Techmer ES Electrablend® PA12 CF13 L 13% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 13% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and lubricatedInformation provided by TP Composi..
|
|||
| Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON CD000I PS (Asia Pacific)
LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
|
|||
| Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
|
Techmer ES Electrablend® PA6/6 C20 BK 20% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf..
|
|||
| Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Europe-Africa-Middle East)
LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
|
|||
| Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON DD0009P PC (Asia Pacific)
LNP STAT-KON* DD0009P is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
|
|||
| Surface Resistance | 10000 - 1.00e+6 ohm | 10000 - 1.00e+6 ohm | ASTM D 257 |
|
SABIC Innovative Plastics LNP Stat-kon DD0009XQ PC (Europe-Africa-Middle East)
LNP* Stat-Kon* DD0009XQ is a compound based on Polycarbonate containing Carbon Powder and Flame Retardant. Added features include Electrically Conductive, Flame Retardant and Easy Molding.This data..
|
|||
| Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON DE0026E PC (Europe-Africa-Middle East)
LNP* Stat-kon* DE0026E is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
|
|||
| Surface Resistance | 1000 - 1.00e+6 ohm | 1000 - 1.00e+6 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON DE0029 PC (Asia Pacific)
LNP* Stat-kon* DE0029 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
|
|||
| Surface Resistance | 1000 - 1.00e+6 ohm | 1000 - 1.00e+6 ohm | ASTM D4496 |
|
Techmer ES Electrafil® PP-61/EC Copolymer Polypropylene, Conductive Carbon Filled
Conductive Carbon, Powder Modified
|
|||
| Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ROA; IEC 60093 |
|
SABIC Innovative Plastics LNP STAT-KON DEL22P PC
LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 10% PTFE. Added features of this material include: Electrically Conductive. Exceptional Processing, Wear..
|
|||
| Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC (Asia Pacific)
LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.
|
|||
| Surface Resistance | 10 - 1.00e+6 ohm | 10 - 1.00e+6 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON DSL229 PC (Asia Pacific)
LNP* Stat-kon* DSL229 is a compound based on Polycarbonate resin containing PTFE, Stainless Steel. Added features of this material include: Electrically Conductive, Internally Lubricated.
|
|||
| Surface Resistance | 1000 - 1.00e+6 ohm | 1000 - 1.00e+6 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON DX12411C PC
LNP* STAT-KON* DX12411C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System.
|
|||
| Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON EX99689C PEI
LNP* STAT-KON* EX99689C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
|
|||
| Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON IS000XXL PA6.12
LNP* STAT-KON* IS000XXL is a compound based on Nylon 6/12 containing Stainless Steel Fibers. Added features of this material include: Food Contact Compliant Raw Materials, Metal Detectable, Electr..
|
|||
| Surface Resistance | 1000 - 1.00e+6 ohm | 1000 - 1.00e+6 ohm | ASTM D 257 |
|
SABIC Innovative Plastics LNP Stat-kon RX08408_NA1D004 PA 66
LNP* Stat-Kon* RX08404_NA1D004 is a compound based on Nylon 66 containing Carbon Powder. Characteristics of this grade include: Electrically Conductive, High Impact.This data was supplied by SABI..
|
|||
| Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON WE002 PBT
LNP STAT-KON* WE002 is a compound based on PBT resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D 257 |
|
SABIC Innovative Plastics LNP Thermocomp EC002E PEI (Asia Pacific)
LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac..
|
|||
| Surface Resistance | 10000 - 1.00e+6 ohm | 10000 - 1.00e+6 ohm | ASTM D257 |
|
Techmer ES Electrablend® PA6/6 03005 CF Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact..
|
|||
| Surface Resistance | 10000 - 1.00e+6 ohm | 10000 - 1.00e+6 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON DX06500 PC
LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy ..
|
|||
| Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | Dry; ASTM D257 |
|
Westlake Plastics Lennite® CN-P UHMW Polyethylene (conductive)
Carbon-powder-filled, self-lubricating, conductive material with excellent abrasion-resistance and high impact strength. This material is light weight and easily machined, has good chemical and str..
|
|||
| Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D4496 |
|
LNP Stat-Kon® SS- Polyamide 12, Stainless Steel Fiber
(discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
|
|||