| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance |
<=
1.00e+6
ohm <br>@Thickness 0.400 mm
|
<=
1.00e+6
ohm <br>@Thickness 0.0157 in
|
ISO IEC 61340-5-1 |
|
Premix Thermoplastics PRE-ELEC® PS 1331 Carbon Black Filled Conductive Thermoplastic Compound
PRE-ELEC® PS 1331 is a carbon black filled conductive thermoplastic compound based on polystyrene. In addition to a low electrical resistivity PRE-ELEC® PS 1331 has excellent mechanical properties..
|
|||
| Surface Resistance |
1.00e+6
-
1.00e+7
ohm <br>@Thickness 2.00 mm
|
1.00e+6
-
1.00e+7
ohm <br>@Thickness 0.0787 in
|
sheet; IEC 61340-5-1 |
|
Panipol Oy DXH-PP Inherently Conductive Polymer
Panipol DXH-PP composition is conductive masterbatch for melt processing mainly with polypropylene. It is based on conductive Polyaniline and resin. Main benefits of Panipol DXH-PP grade are contr..
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+15 ohm | 1.00e+6 - 1.00e+15 ohm | Average value: 4.54e+14 ohm Grade Count:17 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
|
|||
| Surface Resistance |
1.00e+6
-
1.00e+7
ohm <br>@Thickness 2.00 mm
|
1.00e+6
-
1.00e+7
ohm <br>@Thickness 0.0787 in
|
sheet; IEC 61340-5-1 |
|
Panipol Oy DXH Inherently Conductive Polymer
Panipol DXH composition is conductive masterbatch for melt processing with commodity polymers such as polypropylene. It is based on doped and plasticized Polyaniline. Benefits of Panipol DXH grade..
|
|||
| Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | ISO D-257 |
|
Premix Thermoplastics PRE-ELEC® PPE 1462
(discontinued **)
PRE-ELEC PPE 1462 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric..
|
|||
| Surface Resistance | 1.00e+6 ohm | 1.00e+6 ohm | IEC 60093 |
|
3M Dyneon™ TF 4215 PTFE 25% Electrocarbon Filled
(discontinued **)
Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon.
|
|||
| Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-8199 PEEK, with CNT
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect..
|
|||
| Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | |
|
Lehmann & Voss LUVOCOM® 1106-7622 Polyether imide, with carbon fiber
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical..
|
|||
| Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | |
|
Lehmann & Voss LUVOCOM® 1-7395 Polyamide 66, with carbon fiber, aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Emergency running property, for highest tribologic needs.R..
|
|||
| Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | |
|
Lehmann & Voss LUVOCOM® 19-7816 Polyamide 46, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical..
|
|||
| Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | |
|
Lehmann & Voss LUVOCOM® 19-8094 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | |
|
Lehmann & Voss LUVOCOM® 1-7817 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical..
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+8 ohm | 1.00e+6 - 1.00e+8 ohm | ASTM D 257 |
|
SABIC Innovative Plastics Ultem JD7902 PEI (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+10 ohm | 1.00e+6 - 1.00e+10 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Europe-Africa-Middle East)
LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, ..
|
|||
| Surface Resistance | 1.00e+6 ohm | 1.00e+6 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC1508 PPE+HIPS (Europe-Africa-Middle East)
LNP* Stat-kon* Noryl_HMC1508 compound is a static dissipative NORYL resin.
|
|||
| Surface Resistance | 1e+05 - 1.00e+6 ohm | 1e+05 - 1.00e+6 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP THERMOCOMP EC002XXQ PEI
LNP* THERMOCOMP* EC002XXQ is a compound based on Polyetherimide containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive.
|
|||
| Surface Resistance | 1.00e+6 ohm | 1.00e+6 ohm | ASTM D257 |
|
Techmer ES Statiblend® ABS FR AS BN
Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and Flame RetardantInformation provided by TP Composites, Inc.
|
|||
| Surface Resistance | 1e+05 - 1.00e+6 ohm | 1e+05 - 1.00e+6 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON EX07311P PEI (Asia Pacific)
LNP Stat-kon* EX07311P is an easy flowing ESD-safe compound based on Polyetherimide resin. This compound is developed for good dimensional stability for use in ESD Tray for Backend Semicon and HDD t..
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | Dry; ASTM D257 |
|
Westlake Plastics Propylux® SD-X7 Polypropylene (static dissipative)
Low carbon black content (1-2%) reduces contamination problems from sloughing - clean room compatible. Also feature low leachable ion levels and low outgassing.Information provided by Westlake Plas..
|
|||
| Surface Resistance | 1.00e+6 ohm | 1.00e+6 ohm | IEC 60093 |
|
EMS-Grivory Grivory® L 25 W 40 ESD PA12
Product Description: Grilamid L 25 W 40 ESD is a high viscosity, anti-static highly flexible extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 ESD is plasticized and heat stabilized The inh..
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+16 ohm | 1.00e+6 - 1.00e+16 ohm | Average value: 1.70e+15 ohm Grade Count:20 |
|
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+10 ohm | 1.00e+6 - 1.00e+10 ohm | ASTM D257 |
|
PolyOne Stat-Tech™ RA-06CF-07GF/000 EM Polyarylsulfone - 7% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications - Flow Enhanced Grade
Data provided by PolyOne.
|
|||