| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | IEC 60093 |
|
PolyOne Trilliant™ HC HC0200-5001 XR Grey Thermoplastic Elastomer (TPE)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ISO IEC 61340-5-1 |
|
Premix Thermoplastics PRE-ELEC® PE 1295
PRE-ELEC PE 1295 is a dissipative thermoplastic compound based on PE-HD. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resistance bet..
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ISO IEC 61340-5-1 |
|
Premix Thermoplastics PRE-ELEC® PP 1395
PRE-ELEC PP 1395 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resist..
|
|||
| Surface Resistance | 1.00e+8 - 1.00e+9 ohm | 1.00e+8 - 1.00e+9 ohm | 10 volts; ASTM D4496 |
|
Omni Plastics OmniTech™ CPP XE65 BK12 ESD Polypropylene Dissipative
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and ..
|
|||
| Surface Resistance | 1000 - 1.00e+9 ohm | 1000 - 1.00e+9 ohm | Average value: 1.23e+8 ohm Grade Count:5 |
|
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum..
|
|||
| Surface Resistance | 10000 - 1.00e+9 ohm | 10000 - 1.00e+9 ohm | IEC 60093 |
|
LG Chemical LUCON CP2100-KA02 PC+CF
Description Injection Molding Grade, PC+CF, Electrostatic Dissipation, Low Surface ResistanceApplication: LCD Tray, HDD BracketCAS No. 103598-77-2 and 7440-44-0Information provided by LG Chemical
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | IEC 60093 |
|
LG Chemical LUCON CP510F PC/ABS+CNT
Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, High Flow, Good ProcessabilityApplication: Copy Machine Paper GuideCAS No. 103598-77-2 and 7440-44-0Information provided b..
|
|||
| Surface Resistance | 1.00e+7 - 1.00e+9 ohm | 1.00e+7 - 1.00e+9 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON DEL339XF PC
LNP* STAT-KON* DEL339XF is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive, Flame Retardant, Wear Resistant.
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON DFD029 PC (Europe-Africa-Middle East)
LNP* Stat-kon* DFD029 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Reta..
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON DX04403 PC
LNP STAT-KON* DX04403 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Flame Retardant.
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON DX04462C PC
LNP STAT-KON* DX04462C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
|
|||
| Surface Resistance | 1.00e+7 - 1.00e+9 ohm | 1.00e+7 - 1.00e+9 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66
LNP* STAT-KON* REP349 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone, 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Wear Resistant.
|
|||
| Surface Resistance | 1.00e+7 - 1.00e+9 ohm | 1.00e+7 - 1.00e+9 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 (Asia Pacific)
LNP* Stat-kon* REP349 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS (Asia Pacific)
LNP* Stat-loy* AF306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Antistat.
|
|||
| Surface Resistance | 1.00e+7 - 1.00e+9 ohm | 1.00e+7 - 1.00e+9 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-LOY AX11421 ABS
LNP* STAT-LOY* AX11421 is a compound based on ABS resin. Added feature of this material is: Antistatic.
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ASTM D257 |
|
Techmer ES Statiblend® PA6/6 02013
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforAdditive: Impact ModifierFeatures: Conductive and Impact ModifiedUL File Number: E157318TPCI# 1039101Informati..
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ASTM D257 |
|
Techmer ES Statiblend® PBT 03003
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass FiberFeatures: Conductive, Antistatic and ESD ProtectionInformation provided by TP Composites, Inc.
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ASTM D257 |
|
Techmer ES Statiblend® PBT GF10 SS5 MB
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: AntistaticFeatures: Conductive, Antistatic and ESD ProtectionInformation provided by TP Comp..
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON DX04462C PC (Asia Pacific)
LNP* STAT-KON* DX04462C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Clean Compounding System.
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | Dry; ASTM D257 |
|
Westlake Plastics Propylux® SD-X7 Polypropylene (static dissipative)
Low carbon black content (1-2%) reduces contamination problems from sloughing - clean room compatible. Also feature low leachable ion levels and low outgassing.Information provided by Westlake Plas..
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ASTM D257 |
|
Daelim H&L Plavis-ESD CM Polyimide Bearing
Compression Molded. Plavis-ESD: Electrostatic dissipative, Electrostatic dissipative, high thermal resistance and superior mechanical properties. And surface resistivity 10²-10³ OhmGeneral Plavis..
|
|||
| Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ASTM D257 |
|
Daelim H&L Plavis-ESD DF Polyimide Bearing
Direct Formed. Plavis-ESD: Electrostatic dissipative, Electrostatic dissipative, high thermal resistance and superior mechanical properties. And surface resistivity 10²-10³ OhmGeneral Plavis info..
|
|||
| Surface Resistance | 10.0 - 1.00e+9 ohm | 10.0 - 1.00e+9 ohm | Average value: 6.72e+7 ohm Grade Count:17 |
|
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..
|
|||