| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 10.0 - 9.90e+12 ohm | 10.0 - 9.90e+12 ohm | Average value: 5.55e+11 ohm Grade Count:10 |
|
Overview of materials for Styrenic Elastomer (TES)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro..
|
|||
| Surface Resistance | 10.0 - 1.00e+10 ohm | 10.0 - 1.00e+10 ohm | Average value: 8.30e+8 ohm Grade Count:24 |
|
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of ..
|
|||
| Surface Resistance | 10.0 - 1.00e+16 ohm | 10.0 - 1.00e+16 ohm | Average value: 3.03e+15 ohm Grade Count:184 |
|
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
|
|||
| Surface Resistance | 10.0 - 10000 ohm | 10.0 - 10000 ohm | Average value: 3190 ohm Grade Count:3 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte..
|
|||
| Surface Resistance | 10.0 - 1.00e+7 ohm | 10.0 - 1.00e+7 ohm | Average value: 797000 ohm Grade Count:21 |
|
Overview of materials for Polycarbonate, Carbon + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu..
|
|||
| Surface Resistance | 10.0 - 1.00e+6 ohm | 10.0 - 1.00e+6 ohm | Average value: 169000 ohm Grade Count:9 |
|
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu..
|
|||
| Surface Resistance | 10.0 - 3.00e+16 ohm | 10.0 - 3.00e+16 ohm | Average value: 9.09e+14 ohm Grade Count:40 |
|
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
|
|||
| Surface Resistance | 10.0 - 1.00e+17 ohm | 10.0 - 1.00e+17 ohm | Average value: 6.89e+15 ohm Grade Count:37 |
|
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
|
|||
| Surface Resistance | 10.0 - 1.00e+14 ohm | 10.0 - 1.00e+14 ohm | Average value: 1.00e+14 ohm Grade Count:3 |
|
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..
|
|||
| Surface Resistance | 10.0 - 1.00e+6 ohm | 10.0 - 1.00e+6 ohm | Average value: 108000 ohm Grade Count:21 |
|
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be..
|
|||
| Surface Resistance | 10.0 - 1.00e+7 ohm | 10.0 - 1.00e+7 ohm | Average value: 2.59e+6 ohm Grade Count:12 |
|
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
|
|||
| Surface Resistance | 10.0 - 10000 ohm | 10.0 - 10000 ohm | Average value: 2970 ohm Grade Count:6 |
|
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
|
|||
| Surface Resistance | 10.0 - 1.00e+6 ohm | 10.0 - 1.00e+6 ohm | Average value: 335000 ohm Grade Count:6 |
|
Overview of materials for Nylon 6, Stainless Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o..
|
|||
| Surface Resistance | 10.0 - 1.00e+15 ohm | 10.0 - 1.00e+15 ohm | Average value: 5.40e+13 ohm Grade Count:31 |
|
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
|
|||
| Surface Resistance | 10.0 ohm - 1e+05 | 10.0 ohm - 1e+05 | Average value: 5190 ohm Grade Count:9 |
|
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
|
|||
| Surface Resistance | 10.0 - 1.00e+8 ohm | 10.0 - 1.00e+8 ohm | Average value: 1.00e+7 ohm Grade Count:13 |
|
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
|
|||
| Surface Resistance | 10.0 - 100 ohm | 10.0 - 100 ohm | Average value: 70.0 ohm Grade Count:3 |
|
Overview of materials for Nylon 66, 40% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in..
|
|||
| Surface Resistance | 10.0 - 3.10e+15 ohm | 10.0 - 3.10e+15 ohm | Average value: 3.01e+14 ohm Grade Count:17 |
|
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
|
|||
| Surface Resistance | 10.0 - 1.00e+9 ohm | 10.0 - 1.00e+9 ohm | Average value: 6.72e+7 ohm Grade Count:17 |
|
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..
|
|||
| Surface Resistance | 10.0 - 1.00e+12 ohm | 10.0 - 1.00e+12 ohm | Average value: 3.89e+10 ohm Grade Count:26 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..
|
|||