Polymer Property : Surface Resistance = 100 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
PolyOne Edgetek® NY-20CF/000 BLACK Polyamide 6 (Nylon 6)
Information provided by PolyOne
Surface Resistance 100 - 2.00e+17 ohm
100 - 2.00e+17 ohm
Average value: 8.00e+15 ohm Grade Count:88
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D4496
LNP Stat-Kon® LC-1003 Polyetheretherketone, Carbon Fiber Reinforcement  (discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
PolyOne LubriOne™ NJ-30CF/15T-2S Nylon 12  (discontinued **)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Surface Resistance 100 - 1.00e+16 ohm
100 - 1.00e+16 ohm
Average value: 5.18e+14 ohm Grade Count:35
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Surface Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 204-8468 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Surface Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 50-7807 Polycarbonate, with carbon fiber and demolding aid
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Surface Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 50-7844 Polycarbonate, with carbon fiber
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts; low thermal coefficient of expansion.Redu..
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257
Techmer ES Electrablend® PC/ABS
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Electrically Conductive and ESD ProtectionInformation provided by TP Composites, Inc.
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DE0021E PC (Asia Pacific)
LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Easy Molding.
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DX00887C PC
LNP STAT-KON* DX00887C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
Surface Resistance 100 ohm - 1e+05
100 ohm - 1e+05
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DX11411 PC
LNP* STAT-KON* DX11411 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON EE003XXC PEI
LNP STAT-KON* EE003XXC is a compound based on Polyetherimide resin containing 15% Carbon Fiber. Added features of this material include: Clean Compound System, Electrically Conductive.
Surface Resistance 100 ohm - 1e+05
100 ohm - 1e+05
ASTM D 257
SABIC Innovative Plastics LNP Stat-kon EE005 PEI (Asia Pacific)
LNP STAT-KON* EE005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON IS000XXL PA6.12
LNP* STAT-KON* IS000XXL is a compound based on Nylon 6/12 containing Stainless Steel Fibers. Added features of this material include: Food Contact Compliant Raw Materials, Metal Detectable, Electr..
Surface Resistance 100 ohm - 1e+05
100 ohm - 1e+05
ASTM D257
SABIC Innovative Plastics LNP STAT-KON RE006 PA 66
LNP STAT-KON* RE006 is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON SX90398 PA 12
LNP STAT-KON* SX90398 is a compound based on Nylon 12 resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON WE002 PBT
LNP STAT-KON* WE002 is a compound based on PBT resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON WE002 PBT (Asia Pacific)
LNP STAT-KON* WE002 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Surface Resistance 100 - 1000 ohm
100 - 1000 ohm
ASTM D 257
SABIC Innovative Plastics LNP Stat-kon ZX05009 PPE+PS (Europe-Africa-Middle East)
LNP* Stat-kon* ZX05009 is a compound based on PPE+PS Blend resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the..
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC
LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive.
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D 257
SABIC Innovative Plastics LNP Thermocomp EC002E PEI (Asia Pacific)
LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac..
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
SABIC Innovative Plastics NORYL NC220 PPE+HIPS (Asia Pacific)
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON AE002 ABS (Europe-Africa-Middle East)
LNP* STAT-KON* AE002 is a compound based on Acrylonitrile Butadiene Styrene resin containg Carbon Fiber. Added features include: Electrically Conductive
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC
LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D 257
SABIC Innovative Plastics LNP Stat-kon DEF13 PC (Asia Pacific)
LNP* Stat-kon* DEF13 is a compound based on Polycarbonate resin containing Glass Fiber, Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup..
Surface Resistance 100 ohm - 1e+05
100 ohm - 1e+05
ASTM D257
Techmer ES Electrablend® PA6 GF20 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight/Unspecified Filler/Reinfor.Additive: LubricantFeatures: Conductive and LubricatedAppear..
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257
Eurostar Star C BX6088 ABS, 20% Carbon Filled, Injection Molding
Star C BX06008 is a 20% Carbon Fiber Reinforced ABS Injection Molding ResinInformation provided by Eurostar.
Surface Resistance 100 - 1.00e+16 ohm
100 - 1.00e+16 ohm
Average value: 2.52e+15 ohm Grade Count:4
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..
Surface Resistance 100 - 1.10e+11 ohm
100 - 1.10e+11 ohm
Average value: 1.56e+10 ohm Grade Count:12
Overview of materials for Polypropylene, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o..