| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1000 ohm - 1e+05 | 1000 ohm - 1e+05 | ASTM D257 |
|
PolyOne LubriOne™ SF-30CF/15T Polyphenylene Sulfide (PPS)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Surface Resistance | <= 1000 ohm | <= 1000 ohm | IEC 60093 |
|
PolyOne Trilliant™ HC HC6200-5001 XR Grey Polyamide 12 (Nylon 12)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
|
|||
| Surface Resistance | <= 1000 ohm | <= 1000 ohm | ISO D-257 |
|
Premix Thermoplastics PRE-ELEC® PP 1383
PRE-ELEC PP 1383 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
|
|||
| Surface Resistance | 1000 - 1.00e+8 ohm | 1000 - 1.00e+8 ohm | ASTM D 257 |
|
SABIC Innovative Plastics Lexan® LCG0820 PC (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Surface Resistance | 1000 - 1.00e+17 ohm | 1000 - 1.00e+17 ohm | Average value: 5.23e+15 ohm Grade Count:27 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
|
|||
| Surface Resistance | 1000 - 1.00e+12 ohm | 1000 - 1.00e+12 ohm | Average value: 4.65e+11 ohm Grade Count:11 |
|
Overview of materials for Nylon 12, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
|
|||
| Surface Resistance | <= 1000 ohm | <= 1000 ohm | |
|
Lehmann & Voss LUVOCOM® 19-7900 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Surface Resistance | <= 1000 ohm | <= 1000 ohm | |
|
Lehmann & Voss LUVOCOM® 1-RG 1 Polyamide 66, with PAN-carbon fiber, RG-standard
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Surface Resistance | <= 1000 ohm | <= 1000 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-7141 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolys..
|
|||
| Surface Resistance | 1000 ohm - 1e+05 | 1000 ohm - 1e+05 | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON REF42XXP PA 66 (Europe-Africa-Middle East)
LNP* Stat-kon* REF42XXP is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Surface Resistance | 1000 ohm - 1e+05 | 1000 ohm - 1e+05 | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Europe-Africa-Middle East)
LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Surface Resistance | 1000 ohm - 1e+05 | 1000 ohm - 1e+05 | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON WEF32ISP PBT (Europe-Africa-Middle East)
LNP * Stat-kon* WEF32ISP is a compound based on Polybutylene Terephalate resin containing Glass Fiber and Carbon Fiber. Added features include High Impact, Heat Stabilized and Electrically Conduct..
|
|||
| Surface Resistance | 1000 ohm - 1e+05 | 1000 ohm - 1e+05 | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-LOY 9X03508 PPO+PA66 (Asia Pacific)
LNP* Stat-loy* 9X03508 is a compound based on PPO+PA66 resin containing Flame Retardant, Anti-Static. Added features of this material include: Antistat, Flame Retardant, High Impact.
|
|||
| Surface Resistance | 1000 ohm - 1e+05 | 1000 ohm - 1e+05 | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON CD000 PS (Europe-Africa-Middle East)
LNP* Stat-kon* CD000 is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
|
|||
| Surface Resistance | 1000 ohm | 1000 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON RE006 PA6.6 (Asia Pacific)
LNP STAT-KON RE006 is a compound based on Nylon 66 containing carbon fiber. Added features of this material include: Electrically Conductive. Also known as STAT-KON RC-1006
|
|||
| Surface Resistance | 1000 ohm | 1000 ohm | IEC 60093 |
|
EMS-Grivory Grivory® TSC-30/4 LF 15 black 9832 PA666-(CF+Z)45
Product description: Grilon TSC-30/4 LF 15 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers and 15% of a combination of PTFE and silicone oil. Grilon ..
|
|||
| Surface Resistance | 1000 - 10000 ohm | 1000 - 10000 ohm | |
|
A. Schulman ComAlloy Comshield® 215 High Impact Polystyrene, Electrically Conductive - Carbon Black Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Surface Resistance | 1000 ohm | 1000 ohm | ASTM D257 |
|
Adamas Adalon® 131 PTFE, 25% Soft Carbon Filled
Information provided by Adamas, HPM
|
|||
| Surface Resistance | 1000 ohm - 1e+05 | 1000 ohm - 1e+05 | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10 (Asia Pacific)
LNP STAT-KON* QEL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.
|
|||
| Surface Resistance | 1000 ohm - 1e+05 | 1000 ohm - 1e+05 | ASTM D257 |
|
PolyOne Stat-Tech™ NJ-20CF/000 Black Polyamide 12 (Nylon 12)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
|
|||