| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | <= 10000 ohm | <= 10000 ohm | ISO D-257 |
|
Premix Thermoplastics PRE-ELEC® PP 1373
PRE-ELEC PP 1373 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
|
|||
| Surface Resistance | 10000 - 1.00e+14 ohm | 10000 - 1.00e+14 ohm | Average value: 1.68e+13 ohm Grade Count:7 |
|
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
|
|||
| Surface Resistance | 10000 - 1.00e+6 ohm | 10000 - 1.00e+6 ohm | ASTM D257 |
|
PolyOne Edgetek® AS- 08CF / 000 ABS - 8% Carbon Fiber Reinforced With ESD Properties
(discontinued **)
Data provided by PolyOne.
|
|||
| Surface Resistance | 10000 - 5.50e+16 ohm | 10000 - 5.50e+16 ohm | Average value: 7.86e+15 ohm Grade Count:8 |
|
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma..
|
|||
| Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-8417 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
|
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5 BK PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
|
Lehmann & Voss LUVOCOM® 19-7276 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
|
Lehmann & Voss LUVOCOM® 80-7555 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
|
|||
| Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
|
Lehmann & Voss LUVOCOM® 1/CF/10/TF/20/GY Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita..
|
|||
| Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
|
Lehmann & Voss LUVOCOM® 1114-0717 PAEK, with carbon fiber and PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Electrically conduct..
|
|||
| Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
|
Lehmann & Voss LUVOCOM® PEEK CLASSIX 7980 PEEK, with carbon fiber
Applications: medical engineeringHigh-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flamm..
|
|||
| Surface Resistance | 10000 - 1.00e+6 ohm | 10000 - 1.00e+6 ohm | ASTM D257 |
|
Techmer ES Electrablend® HDPE 04001 LE BK
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ESD Protection and ConductiveAppearance: BlackProcessing Method: ExtrusionInformation provided by ..
|
|||
| Surface Resistance | 10000 - 1.00e+6 ohm | 10000 - 1.00e+6 ohm | ASTM D 257 |
|
SABIC Innovative Plastics LNP Stat-kon DD0009XQ PC (Europe-Africa-Middle East)
LNP* Stat-Kon* DD0009XQ is a compound based on Polycarbonate containing Carbon Powder and Flame Retardant. Added features include Electrically Conductive, Flame Retardant and Easy Molding.This data..
|
|||
| Surface Resistance | 10000 ohm - 1e+05 | 10000 ohm - 1e+05 | ASTM D257 |
|
Techmer ES Electrafil® J-50/CF/20/TF/15 Polycarbonate, 20% Carbon Fiber Reinforced, 15% PTFE |
|||
| Surface Resistance | 10000 ohm - 1e+05 | 10000 ohm - 1e+05 | ASTM D 257 |
|
SABIC Innovative Plastics LNP Stat-kon DX92440 PC
LNP STAT-KON* DX92440 is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive.This data was supplied..
|
|||
| Surface Resistance | 10000 ohm | 10000 ohm | ESD S11.11 |
|
Lubrizol Hipscon™ M-530 Static Control Polystyrene
Hipscon™ M-530 is a conductive, carbon black filled, polystyrene available as extruded sheet and compound. Thermoformed trays are lightweight and easily formed into deep pockets that maintain unif..
|
|||
| Surface Resistance | <= 10000 ohm | <= 10000 ohm | ASTM D257 |
|
Ensinger Tecapeek® XP-99 Compression Molded PEEK Compound, Bearing Grade Material with 7% Graphite, 8% PTFE, and 15% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
|
|||
| Surface Resistance | <= 10000 ohm | <= 10000 ohm | ISO IEC 61340-5-1 |
|
Premix Thermoplastics PRE-ELEC® PA 1411 Conductive Thermoplastic Compound
PRE-ELEC® PA 1411 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. PRE-ELEC® PA 1411 has a very low electrical resistivity. P..
|
|||
| Surface Resistance | 10000 - 1.00e+6 ohm | 10000 - 1.00e+6 ohm | ASTM D 257 |
|
SABIC Innovative Plastics LNP Stat-kon PX98038 PA 6 (Europe-Africa-Middle East)
LNP* STATKON* PX98038 is a compound based on PA6 resin containing Carbon Fiber, Glass Fiber, Flame Retardant. Added features include : Flame Retardant, Electrically Conductive, Heat Stabilized.This ..
|
|||
| Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
|
Lehmann & Voss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear, with carbon fiber, glass fiber and micro glass spheres
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||