| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 150 V | 150 V | ASTM D3638 |
|
Gharda Chemicals GATONE™ 5630GF Polyetheretherketone (PEEK)
(discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
|
|||
| Comparative Tracking Index | 150 V | 150 V | ASTM D3638 |
|
Gharda Chemicals Gafone™ 3100 Polyethersulfone (PES)
(discontinued **)
Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl..
|
|||
| Comparative Tracking Index | 150 V | 150 V | IEC 60112 |
|
SABIC Innovative Plastics Lexan® 3412R PC (Europe-Africa-Middle East)
LEXAN 3412R is a high viscosity, 20% glass reinforced grade. It offers excellent flame retardancy and is especially designed for applications requiring high rigidity together with high heat.
|
|||
| Comparative Tracking Index | 150 V | 150 V | IEC 60112 |
|
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
|
|||
| Comparative Tracking Index | 150 V | 150 V | IEC 60112 |
|
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, ..
|
|||
| Comparative Tracking Index | 150 V | 150 V | IEC 60112 |
|
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c..
|
|||
| Comparative Tracking Index | 150 V | 150 V | |
|
Radici Radilon® A RCF3505 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
|
|||
| Comparative Tracking Index | 150 V | 150 V | ASTM D3638 |
|
Gharda Chemicals Gafone S 1320GF Polysulfone (PS)
(discontinued **)
Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Elec..
|
|||
| Comparative Tracking Index | 150 - 175 V | 150 - 175 V | Average value: 167 V Grade Count:3 |
|
Overview of materials for Phenolic/Rubber; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp..
|
|||
| Comparative Tracking Index | 150 V | 150 V | UL 746A |
|
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide Compound
(Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® R-4-200BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound developed to provide high strength, fast cycles, and low maintenance mol..
|
|||
| Comparative Tracking Index | 150 V | 150 V | UL 746A |
|
Chevron Phillips Ryton® BR42C Polyphenylene Sulfide Compound
(discontinued **)
Black Polyphenylene Sulfide CompoundRyton® BR42C is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surface fric..
|
|||
| Comparative Tracking Index |
150
V @Thickness 3.17 mm |
150
V @Thickness 0.125 in |
ASTM D3638 |
|
Industrial Laminates/Norplex NP504 Glass Fabric
Description: Woven glass fabric with high temperature phenolic resin. Good flexural, compressive and impact strengths at elevated temperatures. Capable of continuous operation at 175° C, see note..
|
|||
| Comparative Tracking Index | 150 V | 150 V | IEC 60112 |
|
SABIC Innovative Plastics ULTEM 1010M PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant.
|
|||
| Comparative Tracking Index | 150 V | 150 V | IEC 60112 |
|
SABIC Innovative Plastics ULTEM 1285 PEI (Europe-Africa-Middle East)
Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact compliant in recognized colors.
|
|||
| Comparative Tracking Index | 150 V | 150 V | UL 746 |
|
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat..
|
|||
| Comparative Tracking Index | 150 V | 150 V | UL 746 |
|
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat..
|
|||
| Comparative Tracking Index | 150 V | 150 V | UL 746 |
|
Solvay Specialty Polymers Ryton® R-4-232NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-232NA 40% glass fiber reinforced polyphenylene sulfide compound complies with United States Food and Drug Administration (FDA) and European Union (EU 10/2011 and 1183/2012) regulations..
|
|||
| Comparative Tracking Index | >= 150 V | >= 150 V | IEC 60112 |
|
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
|
|||
| Comparative Tracking Index | 150 V | 150 V | ASTM D3638 |
|
Plenco 2311 Phenolic, Granular, Compression Molded
PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr..
|
|||
| Comparative Tracking Index | 150 V | 150 V | ASTM D3638 |
|
Plenco 7487 Phenolic, Granular, Transfer Molded
PLENCO 07487 is a rubber modified organic reinforced phenolic molding compound offering improved mechanical strength and lower modulus. Plenco 07487 is available in black.Information supplied by Ple..
|
|||
| Comparative Tracking Index | 150 V | 150 V | UL 746A |
|
Chevron Phillips Xtel® XE3035BL Polyphenylene Sulfide Alloy
Xtel® XE3035BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p..
|
|||
| Comparative Tracking Index | 150 V | 150 V | A solution |
|
LATI Latilon 28D G/30 PC, 30% Glass Fiber Reinforced
Polycarbonate (PC) based compound. Glass fibers. Low smoke density and low toxicity index. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..
|
|||
| Comparative Tracking Index | 150 V | 150 V | IEC 60112 |
|
Victrex® PEEK 650G Polyetheretherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta..
|
|||
| Comparative Tracking Index | 150 V | 150 V | ASTM D3638 |
|
Gharda Chemicals Gafone™ B2300 Polysupersulfone (PSS)
(discontinued **)
Characteristics: Excellent Dimensional properties Transparent Improved Impact Strength and Toughness as compared to PES Excellent Hydorlytic Stability High Stress Cracking Resistance Good Chemical..
|
|||
| Comparative Tracking Index | 150 V | 150 V | IEC 60112 |
|
Quadrant EPP Quadrant PSU unfilled, extruded (ISO Data)
Quadrant 1000 PSU is a slightly yellow, translucent (non-optical quality) amorphous thermoplastic material, offering a combination of excellent mechanical, thermal and electrical properties. It ofte..
|
|||
| Comparative Tracking Index | 150 V | 150 V | ISO 60112 |
|
Victrex® PEEK 381G Medium Viscosity
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD..
|
|||