| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 225 V | 225 V | STN 34 6468 |
|
Plastcom SLOVASTER® B GF 30 FRK 3 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant
FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol..
|
|||
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
|
SABIC Innovative Plastics Lexan® 940A PC (Europe-Africa-Middle East)
LEXAN 940A is a medium viscosity flame retardant grade, especially suitable for electrical applications.
|
|||
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
|
SABIC Innovative Plastics Lexan® 943A PC (Europe-Africa-Middle East)
LEXAN 943A is a medium viscosity flame retardant, UV-stabilized grade. UL-94 V0 listed and available in transparent and tints.
|
|||
| Comparative Tracking Index | 225 - 600 V | 225 - 600 V | Average value: 513 V Grade Count:12 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
|
|||
| Comparative Tracking Index | 225 V | 225 V | ASTM D3638 |
|
Plenco 51240 PET, Pellet, Injection Molded, Natural Color
(discontinued **)
PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P..
|
|||
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
|
SABIC Innovative Plastics Lexan® 945U PC (Europe-Africa-Middle East)
Lexan* 945U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio..
|
|||
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
|
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Asia Pacific)
Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA.
|
|||
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
|
Mitsubishi Xantar® 19 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
|
Mitsubishi Xantar® 22 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
|
Mitsubishi Xantar® 24 SR FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
|
Mitsubishi Xantar® F 23 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
|
Mitsubishi Xantar® MX 2015 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
|
Mitsubishi Xantar® MX 2042 FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Comparative Tracking Index | 225 V | 225 V | A solution |
|
LATI Laril 13 G/30-V1 PPOm, 30% Glass Fiber Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good thermal..
|
|||
| Comparative Tracking Index | 225 V | 225 V | UL 746 |
|
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs..
|
|||
| Comparative Tracking Index | 225 V | 225 V | Test Liquid A; IEC 60112 |
|
Styrolution Luran® S KR 2864 C Colored ASA+PC
Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr..
|
|||
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
|
Polyplastics FR-PET® B3015FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
Information provided by PolyPlastics.
|
|||
| Comparative Tracking Index | 225 V | 225 V | Solution A; IEC 60112 |
|
Covestro Apec® FR1892 High-Heat Polycarbonate
This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along..
|
|||
| Comparative Tracking Index | 225 V | 225 V | Solution A; IEC 60112 |
|
Covestro Makrolon® 2665 MAS071 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
|
|||
| Comparative Tracking Index | 225 V | 225 V | Solution A; IEC 60112 |
|
Covestro Makrolon® 2667 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
|
|||
| Comparative Tracking Index | 225 V | 225 V | |
|
Covestro Makrolon® 6870 Polycarbonate
Pseudoplastic behavior and high viscosity extrusion and injection molding grade, less resistant to UV than e.g. MAKROLON 6555.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScie..
|
|||
| Comparative Tracking Index | 225 V | 225 V | Solution A; IEC 60112 |
|
Eurotec® Tecodur® PB70 GR30 NL XA60 PBT, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Comparative Tracking Index | 225 V | 225 V | Solution A; IEC 60112 |
|
Covestro Makroblend® UT5205 PC/PBT Blend
Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Impact modified•..
|
|||
| Comparative Tracking Index | 225 V | 225 V | Solution A; IEC 60112 |
|
Eurotec® Tecotek® PC40 NL FA70 PC, unfilled, flame retardant - (RoHS compliant), natural
Information provided by Eurotec®
|
|||
| Comparative Tracking Index | 225 V | 225 V | Solution A; IEC 60112 |
|
Eurotec® Tecotek® PC43 GR003 TD70 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, light grey
Information provided by Eurotec®
|
|||
| Comparative Tracking Index | 225 V | 225 V | ASTM D3638 |
|
Plenco 50240 PET, Pellet, Injection Molded, Green
(discontinued **)
PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black..
|
|||
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
|
SABIC Innovative Plastics Lexan® 943 PC (Europe-Africa-Middle East)
LEXAN 943 is a medium viscosity flame retardant, UV-stabilized grade, especially suitable for electrical applications.
|
|||
| Comparative Tracking Index | 225 V | 225 V | ASTM D3638 |
|
Plenco 51015 PET, Pellet, Injection Molded, White
(discontinued **)
PLENCO 51015 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL listed.Information supplied by..
|
|||