Polymer Property : Comparative Tracking Index = 249 V Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Comparative Tracking Index 150 - 249 V
150 - 249 V
Average value: 191 V Grade Count:20
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Comparative Tracking Index 100 - 249 V
100 - 249 V
Average value: 178 V Grade Count:16
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Comparative Tracking Index 150 - 249 V
150 - 249 V
Average value: 182 V Grade Count:20
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Comparative Tracking Index 175 - 249 V
175 - 249 V
PLC 3; UL 746A
Mitsubishi Xantar® G2F 23 R Polycarbonate-10% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 175 - 249 V
175 - 249 V
PLC 3; UL 746A
Mitsubishi Xantar® G2F 23 UR Polycarbonate-10% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 175 - 249 V
175 - 249 V
PLC 3; UL 746A
Mitsubishi Xantar® G4F 22 R Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 175 - 249 V
175 - 249 V
PLC 3; UL 746A
Mitsubishi Xantar® G4F 22 UR Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 175 - 249 V
175 - 249 V
PLC 3; UL 746A
Mitsubishi Xantar® G4F 23 UR Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 175 - 249 V
175 - 249 V
PLC 3; UL 746A
Mitsubishi Xantar® G4F 25 R Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 175 - 249 V
175 - 249 V
PLC 3; UL 746A
Mitsubishi Xantar® G4F 25 UR Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 175 - 249 V
175 - 249 V
PLC 3; UL 746A
Mitsubishi Xantar® G6F 23 R Polycarbonate-30% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 175 - 249 V
175 - 249 V
PLC 3; UL 746A
Mitsubishi Xantar® G8F 23 UR Polycarbonate-40% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 175 - 249 V
175 - 249 V
PLC 3; UL 746A
Mitsubishi Xantar® MX 1081 Polycarbonate-10% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 175 - 249 V
175 - 249 V
PLC 3; UL 746A
Mitsubishi Xantar® MX 1094 Polycarbonate-9% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 175 - 249 V
175 - 249 V
PLC 3; UL 746A
Mitsubishi Xantar® MX 1082 Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 175 - 249 V
175 - 249 V
IEC Pub1.112, class 3; IEC Method
Toyobo VYLOPET® EMC132-01 Injection Molding Polyester Resin, Flame Resistant
Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo.
Comparative Tracking Index 175 - 249 V
175 - 249 V
IEC Pub1.112, class 3; IEC Method
Toyobo VYLOPET® EMC132-02 Injection Molding Polyester Resin, Flame Resistant
Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo.
Comparative Tracking Index 175 - 249 V
175 - 249 V
IEC Pub1.112, class 3; IEC Method
Toyobo VYLOPET® EMC133 Injection Molding Polyester Resin, Hydrolysis Resistant
Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo.
Comparative Tracking Index 175 - 249 V
175 - 249 V
IEC Pub1.112, class 3; IEC Method
Toyobo VYLOPET® EMC333 Injection Molding Polyester Resin, Hydrolysis Resistant
Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo.
Comparative Tracking Index 175 - 249 V
175 - 249 V
IEC Pub1.112, class 3; IEC Method
Toyobo VYLOPET® EMC355 Injection Molding Polyester Resin, Glass Reinforced
Applications: HousingsBracketsGear casesFeatures: High RigidityGlass fiber reinforcementInformation provided by Toyobo.
Comparative Tracking Index 175 - 249 V
175 - 249 V
IEC Pub1.112, class 3; IEC Method
Toyobo VYLOPET® EMC605P PBT/PET Alloy, Anti-microbial
Applications: Gas equipment partsFeatures: Good anti-microbialGood appearanceFlame resistantInformation provided by Toyobo.
Comparative Tracking Index 175 - 249 V
175 - 249 V
IEC Pub1.112, class 3; IEC Method
Toyobo VYLOPET® EMC330 Injection Molding Polyester Resin, Hydrolysis Resistant
Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo.
Comparative Tracking Index 175 - 249 V
175 - 249 V
IEC Pub1.112, class 3; IEC Method
Toyobo VYLOPET® EMC618P PBT/PET Alloy, Anti-microbial
Applications: Gas equipment partsFeatures: Good anti-microbialWarpagelessFlame resistantInformation provided by Toyobo.
Comparative Tracking Index 175 - 249 V
175 - 249 V
PLC 3; UL 746A
DSM Stanyl® TE250F3 Nylon 46-15% Glass Reinforced (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Comparative Tracking Index 175 - 249 V
175 - 249 V
PLC 3; UL 746A
DSM Stanyl® TE250F3 Nylon 46-15% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Comparative Tracking Index 175 - 249 V
175 - 249 V
PLC 3; UL 746A
DSM Arnite® TV4 440 KL PBT/PET Blend-20% Glass Reinforced (European Grade)  (discontinued **)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Comparative Tracking Index 175 - 249 V
175 - 249 V
UL 746
Techmer ES HiFill FR® PBT 0166 B FR
Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc.