| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Asia Pacific)
PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | PLC code 2; UL 746A |
|
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP ..
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Lexan® 124 PC (Asia Pacific)
17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not ..
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Lexan® 131 PC
Nonhalogenated. 3.5 MFR.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Lexan® 131R PC (Asia Pacific)
Nonhalogenated. 3.5 MFR.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Lexan® 153 PC (Asia Pacific)
Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Lexan® 223R PC (Asia Pacific)
17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Lexan® 920A PC
Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Lexan® 144R PC (Asia Pacific)
LEXAN 144R is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information..
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Lexan® 955A PC (Europe-Africa-Middle East)
Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A is available in transparen..
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | PLC 2 |
|
PTS Tristar® PC-10FR-(V) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | PLC 2 |
|
PTS Tristar® PC-10R-(V18) 18 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | PLC 2 |
|
PTS Tristar® PC-10R-(V8) 8 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Lexan® HP2NR PC
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no..
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | |
|
LG Chemical AF360 ABS, TBBA-free Flame Retardant
Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b..
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics NORYL RN0401 PPE+PS
Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics LNP LUBRICOMP Noryl_SPN422L PPE+HIPS (Europe-Africa-Middle East)
LNP* Lubricomp Noryl_SPN422L is a wear resistant, fluorocarbon alloy, 235F (113C) HDT. UL94 HB rated. Check surface aesthetics prior to material specification.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | PLC code 2; UL 746A |
|
SABIC Innovative Plastics Prevex VFAX PPE+PS
High impact strength. 180F (82C) HDT. Improved productivity/reliability.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Valox® 4521 PBT
VALOX 4521 is a high flow, 20% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific)
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Valox® IQ420 PBT
Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PS+PA
30% Glass Reinforced PPE+PA Alloy.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics NORYL N850 PPE+PS
ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East)
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | PLC code 2; UL 746A |
|
SABIC Innovative Plastics Noryl PC180X PPE+PS
Nonbrominated, nonchlorinated flame retardant. V-1/5VA rated; 175F (90C) HDT. Improved productivity and reliability.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Valox® 815 PBT (Asia Pacific)
15% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
DuPont Performance Polymers Rynite® FR531 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**)
36% Reinforced Flame Retardant Polyethylene Terephthalate Information provided by DuPont Performance Polymers
|
|||
| Comparative Tracking Index | 15.0 - 400 V | 15.0 - 400 V | Average value: 225 V Grade Count:20 |
|
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
|
|||
| Comparative Tracking Index | 175 - 400 V | 175 - 400 V | Average value: 247 V Grade Count:7 |
|
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Lexan® HP4NR PC (Europe-Africa-Middle East)