Polymer Property : Comparative Tracking Index = 450 V Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Comparative Tracking Index 450 V
450 V
Plastcom SLOVAMID 66 GB 30 GF 20 PA66, 20% glass fibre, 30% glass beads
FeaturesPA 66 chemically reinforced with 20% glass fibre and with the content of 30 % glass beads. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical properties can b..
Comparative Tracking Index 450 V
450 V
Plastcom SLOVAMID 66 GF 20 GF 10 PA66, 20% glass fibre, glass beads
FeaturesPA 66 chemically reinforced with 20% glass fibre and with the content of 10 % glass beads. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical properties can b..
Comparative Tracking Index 450 V
450 V
Plastcom SLOVAMID 66 GF 25 FRA 5 PA66, 25% glass fibre, flame retardant
FeaturesPA 66 for injection moulding, reinforced with 25% glass fibre and halogen flame retardant. Application in electrical industry: breakers, coilforms, covers, terminals. Slightly decreased flam..
Comparative Tracking Index 450 V
450 V
STN 34 6468
Plastcom SLOVAMID 66 GF 30 FRA 3 Polyamide 66, 30% Glass Fiber, Halogen Flame Retardant
FeaturesPA 66 for injection moulding, reinforced with 30% glass fiber and halogen flame retardant. Application in electrical industry: breakers, coil forms, covers, terminals. Slightly decreased f..
Comparative Tracking Index 450 V
450 V
IEC 60112
SABIC Innovative Plastics Cycolac® S157 ABS (Europe-Africa-Middle East)
CYCOLAC S157 is a high flow flame retardant ABS with good processability developed for applications requiring UL94 V0 at reduced wall thickness.This data was supplied by SABIC-IP for the Europe-Afri..
Comparative Tracking Index 450 V
450 V
Plastcom SLOVALEN PH 56 T FRD 1 PP, flame retardant
FeaturesModified homopolymer PP for injection moulding with decreased flammability. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil forms, guides, co..
Comparative Tracking Index 450 V
450 V
Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, Dry As Molded &
Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high ..
Comparative Tracking Index 450 V
450 V
IEC 60112
SABIC Innovative Plastics Cycolac® CRT3370 ABS (Europe-Africa-Middle East)
CYCOLAC CRT3370 is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow char..
Comparative Tracking Index 450 V
450 V
CTI 100; IEC 112
Nilit FRIANYL B63 SG 10 Nylon 6 for injection molding, 10% mineral filled
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Comparative Tracking Index 450 V
450 V
Ineos ABS NOVODUR® L3FR ABS, Injection Grade  (discontinued **)
Injection molding grade, flame retardant, very easy flow. Contains no polyhalogenated diphenyls or diphenyl ethers.Applications: Television and computer housings.Information provided by the manufact..
Comparative Tracking Index 450 V
450 V
Solution A; IEC 60112
Solvay TECHNYL® A 218 S40 Black 21 N PA66, 40% glass spheres, DRY
Description: Polyamide 66, reinforced with 40% of glass spheres, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 218 S40 is used in all sectors of ind..
Comparative Tracking Index 450 V
450 V
Solution A; IEC 60112
Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, DRY
Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail..
Comparative Tracking Index 450 V
450 V
Solution A; IEC 60112
Solvay TECHNYL® A 218 V20 Black 21N PA66, 20% glass fiber, DRY
Description: Polyamide PA66, reinforced with 20% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 218 V20 is used in all sectors of industry..
Comparative Tracking Index 450 V
450 V
Solution B; IEC 60112
Solvay TECHNYL® 27010ST PA66, DRY
Description: Polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2710ST is used in all sector of..
Comparative Tracking Index >= 450 V
>= 450 V
KA Method; IEC 112; DIN 53480
Zell-Metall Engineering Plastics Zellamid 1400 (PET)
Zellamid® 1400 is the registered trademark of Zell-Metall’s partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, ..
Comparative Tracking Index >= 450 V
>= 450 V
KA Method; IEC 112; DIN 53480
Zell-Metall Engineering Plastics Zellamid 1400 (PET) at 50% RH
Zellamid® 1400 is the registered trademark of Zell-Metall’s partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, ..
Comparative Tracking Index 450 V
450 V
IEC 60112
Ter Hell Plastic Terez® PBT 6750 T Polybutylene Terephthalate, Impact Modified
Description: Impact modified PBT.Application: For impact stressed, injection molding parts.Information provided by Ter Hell Plastic GMBH.
Comparative Tracking Index 450 V
450 V
IEC 60112
Ter Hell Plastic Terez® PBT 7100 GF 30 Polybutylene Terephthalate, 30% Glass Fiber
Description: PBT, 30% glass fiber reinforced.Application: Suitable for injection molding applications.Information provided by Ter Hell Plastic GMBH.
Comparative Tracking Index 450 V
450 V
conditioned; IEC 60112
EMS-Grivory Grivory® BK-50 PA6-GB50
Information provided by EMS Grivory
Comparative Tracking Index 450 V
450 V
Stufe; IEC 112
CP-Polymer-Technik Wellamid® 6000 GX 350 HWCP Combination Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Comparative Tracking Index 450 V
450 V
Stufe; IEC 112
CP-Polymer-Technik Wellamid® 6600 MR 309 HWCP 30% Mineral Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Comparative Tracking Index 450 V
450 V
Stufe; IEC 112
CP-Polymer-Technik Wellamid® 6600 MZ 315 CP Combination Nylon 66, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Comparative Tracking Index 450 V
450 V
M; IEC 60112
Eurostar Staramide AG3K PA66, 15% Glass Filled, Injection Molded
AG3K is a Heat and Hydrolytically Stabilized, 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl..
Comparative Tracking Index 450 V
450 V
Test Liquid B; IEC 112
BASF Ultradur B 4500 PBT
Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660.
Comparative Tracking Index 450 V
450 V
Test Solution A; IEC 60112
BASF Ultramid® A3WG5 25% Glass Filled PA66 (Conditioned)
Ultramid A3WG5 is a 25% glass fiber reinforced and heat resistance injection molding PA66 grade.
Comparative Tracking Index 450 V
450 V
Test solution A; IEC 60112
BASF Ultramid® A3WG6 BK 00564 30% Glass Filled PA66 (Conditioned)
Description: 30% glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of high stiffness and dimensional stability such as lamp socket housings, f..
Comparative Tracking Index 450 V
450 V
Test solution A; IEC 60112
BASF Ultradur S 4090 G4 High Speed Unc. 20% Glass Filled PBT
Ultradur S 4090 G4 High Speed Unc. is a high flow, fast cycling with low warpage, 20% glass filled injection molding PBT for industrial parts, rigid tough and dimensional stable applications.
Comparative Tracking Index 450 V
450 V
IEC 60112
Lanxess Durethan® BM 25 FN20 DUS013 000000 Nylon 6, 25% Mineral
PA 6, injection molding grade, 25% mineral, UL94V-2 off 0.75 mm, max. temp. glow wire test:960°C off 0.8 mm, free from halogen, optimized for laser marking at 1064 nm,
Comparative Tracking Index 450 V
450 V
Test solution A; IEC 60112
BASF Ultramid® B3WG5 BK 00654 PA6 25% Glass Filled BK (Dry)
Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el..
Comparative Tracking Index 450 V
450 V
Test Solution A; IEC 60112
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Dry)
Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade.