| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 350 - 599 V | 350 - 599 V | Average value: 464 V Grade Count:6 |
|
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Akulon® K224-HG5 (Dry) 25% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Akulon® K224-HG5 (Cond.) 25% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Akulon® K224-HG8 (Cond.) 40% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Akulon® K224-HG5 Nylon 6-25% Glass Reinforced (European and Asian Grade) (Cond)
(discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Akulon® K224-HG5 Nylon 6-25% Glass Reinforced (European and Asian Grade) (Dry)
(discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Akulon® K224-HG8 Nylon 6-40% Glass Reinforced (European Grade) (Cond)
(discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Akulon® K224-HG8 Nylon 6-40% Glass Reinforced (European Grade) (Dry)
(discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Akulon® K223-HM6 (BLACK) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Akulon® K224-HG3 (Cond.) 15% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Akulon® K224-HG3 Nylon 6-15% Glass Reinforced (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Akulon® K224-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Akulon® K224-HG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Akulon® K224-HG7 Nylon 6-35% Glass Reinforced (European Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Akulon® K224-HG7 Nylon 6-35% Glass Reinforced (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Arnite® TV4 240 PBT-20% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Arnite® TV4 261 PBT-30% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Stanyl® TE200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Akulon® K224-HG3 (Dry) 15% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Comparative Tracking Index |
400
-
599
V @Thickness 3.00 mm |
400
-
599
V @Thickness 0.118 in |
IEC 60112 |
|
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM
Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit..
|
|||
| Comparative Tracking Index |
400
-
599
V @Thickness 3.00 mm |
400
-
599
V @Thickness 0.118 in |
IEC 60112 |
|
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM
Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr..
|
|||
| Comparative Tracking Index |
400
-
599
V @Thickness 3.00 mm |
400
-
599
V @Thickness 0.118 in |
IEC 60112 |
|
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, ..
|
|||
| Comparative Tracking Index |
400
-
599
V @Thickness 3.00 mm |
400
-
599
V @Thickness 0.118 in |
IEC 60112 |
|
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. ..
|
|||
| Comparative Tracking Index |
400
-
599
V @Thickness 3.00 mm |
400
-
599
V @Thickness 0.118 in |
IEC 60112 |
|
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded
Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. ..
|
|||
| Comparative Tracking Index |
400
-
599
V @Thickness 3.00 mm |
400
-
599
V @Thickness 0.118 in |
IEC 60112 |
|
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, ..
|
|||
| Comparative Tracking Index | 175 - 599 V | 175 - 599 V | Average value: 339 V Grade Count:45 |
|
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Akulon® K224-HG8 (Dry) 40% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Comparative Tracking Index |
400
-
599
V @Thickness 3.00 mm |
400
-
599
V @Thickness 0.118 in |
IEC 60112 |
|
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM
Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To..
|
|||
| Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
|
DSM Arnite® TV4 230 PBT-15% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
|
|||
| Comparative Tracking Index |
400
-
599
V @Thickness 3.00 mm |
400
-
599
V @Thickness 0.118 in |
IEC 60112 |
|
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou..
|
|||