| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistivity per Square | <= 0.50 ohm | <= 0.50 ohm | |
|
Parker Chomerics CHO-SHIELD® 4076 Conductive Coating
CHO-SHIELD® 4076 nickel-filled polyurethane is recommended for shielding an entire room. This durable coating adheres well to plaster, wood, glass, concrete, drywall and most metals.Information pro..
|
|||
| Surface Resistivity per Square | 0.50 ohm | 0.50 ohm | @ 1 mil |
|
Parker Chomerics CHO-SHIELD® 4076-50A Conductive Coating
Conductive Nickel-Filled Coating. This is an electrically conductive waterborne nickel-filled polyurethane coating that provides excellent shielding against radiated EMI. It bonds well to plaster, c..
|
|||
| Surface Resistivity per Square | 0.50 ohm | 0.50 ohm | |
|
Parker Chomerics PREMIER™ A230-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
|
|||
| Surface Resistivity per Square | 0.50 ohm | 0.50 ohm | Using a 156 mesh stainless steel screen, 13 micron emulsion |
|
Gwent Electronic Materials C2030812D3 Silver/Silver Chloride Paste
Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 60/40. Applications in medical diagnostics, environmentalScreen Printing Equipment: semi-automatic, manualScreen Types: polye..
|
|||
| Surface Resistivity per Square |
0.50
ohm @Thickness 0.0160 mm |
0.50
ohm @Thickness 0.000630 in |
Using a 156 stainless steel mesh, 13 micron emulsion |
|
Gwent Electronic Materials C2090225D7 Silver/Silver Chloride Paste
Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 70/30. The paste is in a ready to use form at a viscosity suitable for automatic or semi-automatic screen printing. The paste..
|
|||
| Surface Resistivity per Square | 0.50 ohm | 0.50 ohm | cured film; 16 microns thick |
|
Gwent Electronic Materials C61003P7 Silver / Silver Chloride Paste
C61003P7 has a ratio of Silver to Silver Chloride of 60/40. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a fa..
|
|||
| Surface Resistivity per Square | <= 0.50 ohm | <= 0.50 ohm | |
|
Abatron AboWeld 8201-14/AboCure 50-12 Carbon-Filled Electrically Conductive Epoxy Compound
AboWeld 8201-14/AboCure 50-12 is a very conductive carbon-epoxy paste. It is preferred where higher heat and chemical resistance more important. As the size of the conductive particles is relatively..
|
|||