Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Arc Resistance = 100 sec Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Arc Resistance 100 sec
100 sec
IPC-TM-650.2.5.1
Park Electrochemical Nelco® N7000-2 HT/N7000-3 Toughened Polyimide Laminate and Prepreg
The Nelco N7000-2 HT laminate and N7000-3 prepreg are a series of toughened polyimide materials for use in high-reliability multilayers. This combined resin system provides excellent thermal perform..
Arc Resistance 100 - 116 sec
100 - 116 sec
Average value: 108 sec Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor..
Arc Resistance 100 - 120 sec
100 - 120 sec
Average value: 110 sec Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..
Arc Resistance 100 sec
100 sec
ASTM D495
Plenco 7300 Phenolic, Nodular, Injection Molded  (discontinued **)
Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file..
Arc Resistance 100 - 130 sec
100 - 130 sec
Average value: 119 sec Grade Count:6
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
Arc Resistance 100 - 120 sec
100 - 120 sec
Average value: 112 sec Grade Count:9
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values..
Arc Resistance 100 sec
100 sec
ASTM D495
Kolon KOPET® KP132G30VO FR-PET Resin
KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of..
Arc Resistance 100 sec

@Thickness 3.17 mm
100 sec

@Thickness 0.125 in
ASTM D495
Industrial Laminates/Norplex NP130 Glass Fabric
Description: Woven glass fabric combined with a halogenated epoxy resin system. Produced to printed circuit board quality standards. Flame retardant, meets UL-94 flammability classification V-0.Thic..
Arc Resistance 100 sec

@Thickness 3.17 mm
100 sec

@Thickness 0.125 in
ASTM D495
Industrial Laminates/Norplex NP504 Glass Fabric
Description: Woven glass fabric with high temperature phenolic resin. Good flexural, compressive and impact strengths at elevated temperatures. Capable of continuous operation at 175° C, see note..
Arc Resistance 100 sec

@Thickness 3.17 mm
100 sec

@Thickness 0.125 in
ASTM D495
Industrial Laminates/Norplex NP680 Paper Base Laminate
Description: Hot punching grade with electrical properties between NP611 to NP631.Thickness Tested: 0.062", 0.125" & 0.500"
Arc Resistance 100 sec

@Thickness 3.17 mm
100 sec

@Thickness 0.125 in
ASTM D495
Industrial Laminates/Norplex NP691 Paper Base Laminate
Description: Flame resistant, room temperature punching grade. NP691 is very similar to NP612 in electrical properties and mechanical strength, with improved moisture resistance.Thickness Tested: 0...
Arc Resistance 100 sec
100 sec
ASTM D495
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber
Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low ..
Arc Resistance 100 sec
100 sec
Practical Use (Water Absorption 2.5%); ASTM-D495
Toyobo GLAMIDE® T-521 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Arc Resistance 100 sec
100 sec
Absolute Drying; ASTM-D495
Toyobo GLAMIDE® T-663G30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Arc Resistance 100 sec
100 sec
Absolute Drying; ASTM-D495
Toyobo GLAMIDE® T-663G50 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Arc Resistance >= 100 sec
>= 100 sec
ASTM D495
Chengdu Polyster KLX-G42 PC Film & Sheet
PC film, high transparency, one side is velvet the other side is matte.Information provided by Chengdu Polyster Co., Ltd.
Arc Resistance 100 sec
100 sec
Tungsten; ASTM D495
Asahi Kasei Xyron® 100V Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Arc Resistance 100 sec
100 sec
Tungsten; ASTM D495
Asahi Kasei Xyron® 140V Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Arc Resistance 100 sec
100 sec
ASTM D495
Chang Chun Plastic PBT4830 Fire Retardant & 30% Glass Fiber Enforced Grade PBT
Information provided by Dowell Trading Company Ltd.
Arc Resistance 100 sec
100 sec
Tungsten; ASTM D495
Asahi Kasei Xyron® 220V Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Arc Resistance 100 sec
100 sec
ASTM D495
Gromax CCP PBT 3030-200HR 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Arc Resistance 100 sec
100 sec
ASTM D495
Gromax CCP PBT 3040-201 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Arc Resistance 100 sec
100 sec
ASTM D495
Gromax PBT 3015-104 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Arc Resistance 100 - 134 sec
100 - 134 sec
Average value: 126 sec Grade Count:33
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..
Arc Resistance 100 sec
100 sec
ASTM D495
Gromax CCP PET 9130-200 30% Glass Filled
Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell..
Arc Resistance 100 sec
100 sec
ASTM D495
Plenco 50045 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s..
Arc Resistance 100 sec
100 sec
ASTM D495
Plenco 51015 PET, Pellet, Injection Molded, White  (discontinued **)
PLENCO 51015 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL listed.Information supplied by..