| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM
Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit..
|
|||
| Arc Resistance | 60 - 119 sec | 60 - 119 sec | ASTM D495 |
|
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
|
|||
| Arc Resistance | 60 - 119 sec | 60 - 119 sec | ASTM D495 |
|
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM
Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
|
|||
| Arc Resistance | 60 - 119 sec | 60 - 119 sec | ASTM D495 |
|
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded
Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties ..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D496 |
|
Ascend Performance Materials VYDYNE® R533H Nylon, 33% Glass Reinforced, DAM
Vydyne® R533H is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when exposed to anti-free..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM
Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM
Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn..
|
|||
| Arc Resistance | 60 - 119 sec | 60 - 119 sec | ASTM D495 |
|
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM
Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® 64C-R Nylon 66, DAM
Vydyne® 64C-R is a medium-viscosity PA66 resin suitable for injection-molding, extrusion and compounding applications. It is available in natural color only. Vydyne 64C-R resin offers high strength..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM
Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To..
|
|||
| Arc Resistance | 60 - 119 sec | 60 - 119 sec | ASTM D495 |
|
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D496 |
|
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM
Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded
Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
|
|||
| Arc Resistance | 20.0 - 119 sec | 20.0 - 119 sec | Average value: 48.4 sec Grade Count:7 |
|
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass Reinforced". Each property range of values reported is..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D496 |
|
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM
Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri..
|
|||
| Arc Resistance |
60
-
119
sec <br>@Thickness 3.00 mm
|
60
-
119
sec <br>@Thickness 0.118 in
|
ASTM D495 |
|
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
|
|||