Polymer Property : Arc Resistance = 125 sec Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Arc Resistance 125 - 300 sec
125 - 300 sec
Average value: 190 sec Grade Count:6
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..
Arc Resistance 125 sec
125 sec
ASTM D495
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, Dry As Molded &nbs
AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di..
Arc Resistance 125 sec
125 sec
ASTM D495
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide Compound  (Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® R-4-230NA is an advanced 40% fiberglass reinforced polyphenylene sulfide compound which provides reduced flash and improved processability compare..
Arc Resistance 125 sec
125 sec
ASTM D495
Solvay Specialty Polymers Ryton® R-4-220BL Polyphenylene Sulfide Compound  (Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® R-4-220BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound formulated for enhanced hydrolytic stability in applications requiring ..
Arc Resistance 125 sec
125 sec
ASTM D495
Solvay Specialty Polymers Ryton® R-4 02XT Polyphenylene Sulfide Compound  (Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® R-4 02XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve ducti..
Arc Resistance 125 - 130 sec
125 - 130 sec
Average value: 128 sec Grade Count:4
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Arc Resistance 125 sec
125 sec
ASTM D495
Kolon KOPA® KN173HI4 High Impact Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Arc Resistance 125 sec
125 sec
ASTM D495
Kolon KOPA® KN333HI4 High Impact Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Arc Resistance 125 sec
125 sec
ASTM D495
Kolon KOPA® KN333HI5BL High Impact Nylon 66
Middle viscosity, Impact -resistantApplications A variety of fuse boxes, relax boxesInformation provided by API-Kolon.
Arc Resistance 125 sec
125 sec
ASTM D495
Solvay Specialty Polymers Ryton® R-4-02 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e..
Arc Resistance 125 sec
125 sec
ASTM D495
Solvay Specialty Polymers Ryton® R-4-02XT Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even..
Arc Resistance 125 sec
125 sec
ASTM D495
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi..
Arc Resistance 125 sec
125 sec
ASTM D495
Samyang Tripet® 2500G30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced
TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll informati..
Arc Resistance 125 sec
125 sec
ASTM D495
Sumitomo Bakelite North America E 264H Long Glass Fiber Reinforced Epoxy
E 264H is a high strength, long fiberglass reinforced epoxy molding compound, which features improved flow in transfer molding.Information provided by Sumitomo Bak North America, Inc.
Arc Resistance 125 sec
125 sec
ASTM D495
Solvay Specialty Polymers Ryton® R-4-220NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur..
Arc Resistance 125 sec
125 sec
Absolute Drying; ASTM-D495
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Arc Resistance 125 sec
125 sec
Tungsten electrode; ASTM D495
Toyobo VYLOPET® EMC307 Injection Molding Polyester Resin, High Cycles
Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesInformation provided by Toyobo.
Arc Resistance 125 sec
125 sec
ASTM D495
Unitika P-3001 Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..
Arc Resistance 125 sec
125 sec
Conditioned; ASTM D495
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0...
Arc Resistance 125 sec
125 sec
ASTM D495
Plenco 7579 Phenolic, Granular, Injection Molded
PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40..
Arc Resistance 125 sec
125 sec
ASTM D495
Owens Corning Glass Fiber Reinforced Polyphenylene Sulfide, 40 wt.% glass
Polyphenylene Sulfide provides excellent resistance to organic solvents (below 375°F). It is unaffected by strong alkalis or aqueous organic salt solutions. Data provided by the manufacturer, Owen..
Arc Resistance 125 sec
125 sec
Cosmic Plastics 224 Dacron Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Arc Resistance 125 sec
125 sec
ASTM D495
Solvay Specialty Polymers Ryton® R-4-220NA Polyphenylene Sulfide Compound  (Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® R-4-220NA is an advanced 40% fiberglass reinforced polyphenylene sulfide compound formulated for enhanced hydrolytic stability in applications re..
Arc Resistance 125 sec
125 sec
ASTM D495
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of ..
Arc Resistance 125 sec
125 sec
ASTM D495
Samyang Tripet® 2500G45 Polyethylene Terephthalate, 45% Glass Fiber Reinforced
TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll information..