| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten, PLC code 6; ASTM D 495 |
|
SABIC Innovative Plastics Cycolac® MG37CR ABS
High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Cycolac® MG47N ABS
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti..
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Asia Pacific)
Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications.
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Asia Pacific)
PC+ABS blend, low gloss and UV-stable, suitable for automotive interior applications.
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | PLC 6 |
|
PTS Tristar® PC-10R-(V) 10 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | PLC 6 |
|
PTS Tristar® PC-20GFR 20% Glass Reinforced Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Lexan® HPH4704 PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril..
|
|||
| Arc Resistance |
60
-
120
sec @Thickness 3.00 mm |
60
-
120
sec @Thickness 0.118 in |
UL Rating PLC 6 (60-120 sec) |
|
Covestro Apec® DP9-9354 High-Heat Polycarbonate, Flame-Retardant
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
|
LG Chemical ER451 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica..
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
|
LG Chemical Lupox® GP2056F PBT+GF5%
Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
|
LG Chemical LUPOY GP5008BFH PC/ABS, Flame Retardance
Description: Injection Molding, PC/ABS, Flame Retardance, High Flow, Heat Resistant, High Impact Application: E&E (Housing)Information provided by LG Chemical
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
|
LG Chemical LUPOY HR5007AE PC/ABS, High Impact
Description: Injection Molding, PC/ABS, High Flow, High ImpactApplication: E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
|
LG Chemical MP211 ABS, Low Gloss, Metal Plating
Feature: Injection Molding, High Flow, Metal PlatingApplication: Decorative Parts (Home Appliance Door Handle Etc)CAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics ULTEM 2100 PEI
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors.
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics ULTEM 2300R PEI (Asia Pacific)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Valox® 553 PBT+PC (Asia Pacific)
30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc.
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Valox® 553U PBT+PC
30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc.
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Valox® 735 PBT+PET
40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Valox® 830 PBT (Asia Pacific)
30% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East)
VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Valox® ENH4550 PBT
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten, PLC code 6; ASTM D 495 |
|
SABIC Innovative Plastics Noryl GFN2L PPE+HIPS (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PS+PA (Asia Pacific)
GR 30%. Highest stiffness of 1200000 psi (8200 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: under the bonnet.
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East)
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics ULTEM 2110R PEI (Asia Pacific)
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Valox® 508 PBT+PC (Asia Pacific)
30% GR PBT+PC. Excellent mechanical and thermal performance. Non-flame retardant. Reduced warpage characteristics. Applications same as VALOX 420.
|
|||
| Arc Resistance |
60
-
119
sec @Thickness 3.00 mm |
60
-
119
sec @Thickness 0.118 in |
ASTM D495 |
|
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM
Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr..
|
|||
| Arc Resistance |
60
-
119
sec @Thickness 3.00 mm |
60
-
119
sec @Thickness 0.118 in |
ASTM D495 |
|
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded
Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe..
|
|||
| Arc Resistance |
60
-
119
sec @Thickness 3.00 mm |
60
-
119
sec @Thickness 0.118 in |
ASTM D496 |
|
Ascend Performance Materials VYDYNE® R533H Nylon, 33% Glass Reinforced, DAM
Vydyne® R533H is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when exposed to anti-free..
|
|||
| Arc Resistance | 60 sec | 60 sec | ASTM D495 |
|
Plenco 6554 Phenolic, Granular, Compression Molded
(discontinued **)