| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 90 sec | 90 sec | Dry; ASTM D495 |
|
Rogers Corporation Bisco™ BF-1000 Cellular Silicone Foam
Soft, low compression set silicone foam often specified to meet safely-conscious requirements. UL recognized for flame retardance.Applications: Low closure-force gaskets and seals, Vibration and sh..
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
Owens Corning Glass Fiber Reinforced Polyester (PET), 30 wt.% glass
Thermoplastic Polyesters are resistant to most organic solvents, weak acids and alkalis. They are not recommended with strong acids and alkalis or for prolonged use in hot water. Data provided by t..
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
Plenco 50015 PET, Pellet, Injection Molded, Black
(discontinued **)
PLENCO 50015 is an engineering grade glass reinforced polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL recognized and available in white, natu..
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant
Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
LG Chemical LUMID GP2259AFL PA6+GF25%, Flame Retardant
Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Connector)CAS No. 25038-54-4, 65997-17-3, 1163-19-5, 1309-64-4 and 138265-88-0Information provided by LG Chemical
|
|||
| Arc Resistance |
90
sec <br>@Thickness 3.17 mm
|
90
sec <br>@Thickness 0.125 in
|
ASTM D495 |
|
Industrial Laminates/Norplex NP610 Paper Base Laminate
Description: Phenolic paper based grade for mechanical applications. Good tensile, compressive and flexural strength. Primarily a machining material, but may be hot punched up to .093" thick.Thickne..
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
Gromax CCP PBT 1100-220S
Product Description: PBT unreinforced and impact-modified injection molding grade. Characteristics:Low warp age, high toughness and excellent dimensional stabilityExcellent glossy surface and less-g..
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
Gromax PBT 4115-104D 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
Gromax PBT 4130-104D 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
Gromax PBT 4130-201D 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
Gromax PBT 4140-201D 40% Glass Fiber Filled
Product Description: A glass fiber 40% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
|
|||
| Arc Resistance |
90
sec <br>@Thickness 3.17 mm
|
90
sec <br>@Thickness 0.125 in
|
ASTM D495 |
|
Industrial Laminates/Norplex NP625 Paper Base Laminate
Description: Paper phenolic grade with better moisture resistance than NP612. Requires less heat to punch and shear than NP611.
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
Samyang Trirex® 3015NF Polycarbonate, Flame Retardancy
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3015NF is a flame retardant grade.Applications: Mobile Phone - battery caseInformation..
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
Samyang Trirex® 3025N1 Polycarbonate, Flame Retardant
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
|
|||
| Arc Resistance | 90 sec | 90 sec | Practical Use (Water Absorption 3.0%); ASTM-D495 |
|
Toyobo GLAMIDE® T-400G15 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
|
|||
| Arc Resistance | 90 sec | 90 sec | Practical Use (Water Absorption 2.5%); ASTM-D495 |
|
Toyobo GLAMIDE® T-402 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
|
|||
| Arc Resistance | 90 sec | 90 sec | Practical Use (Water Absorption 1.7%); ASTM-D495 |
|
Toyobo GLAMIDE® T-602G30 MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
|
|||
| Arc Resistance | 90 sec | 90 sec | Practical Use (Water Absorption 2.1%); ASTM-D495 |
|
Toyobo GLAMIDE® T-663G15 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
|
|||
| Arc Resistance | 90 sec | 90 sec | Absolute Drying; ASTM-D495 |
|
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
|
|||
| Arc Resistance | 90 sec | 90 sec | Tungsten electrode; ASTM D495 |
|
Toyobo VYLOPET® EMC605P PBT/PET Alloy, Anti-microbial
Applications: Gas equipment partsFeatures: Good anti-microbialGood appearanceFlame resistantInformation provided by Toyobo.
|
|||
| Arc Resistance | 90 sec | 90 sec | Tungsten electrode; ASTM D495 |
|
Toyobo VYLOPET® EMC618P PBT/PET Alloy, Anti-microbial
Applications: Gas equipment partsFeatures: Good anti-microbialWarpagelessFlame resistantInformation provided by Toyobo.
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
Entec Hylex® P1310FR Polycarbonate
Information provided by Ravago
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
Entec Hylex® P1010FR Polycarbonate
Information provided by Ravago.
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
Chang Chun Plastic PBT4815 Fire Retardant & 15% Glass Fiber Enforced Grade PBT
Information provided by Dowell Trading Company Ltd.
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
Chang Chun Plastic PBT4115 Fire Retardant & 15% Glass Fiber Enforced Grade PBT
Information provided by Dowell Trading Company Ltd.
|
|||
| Arc Resistance | 90 sec | 90 sec | Practical Use (Water Absorption 2.8%); ASTM-D495 |
|
Toyobo GLAMIDE® T-401 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
Gromax CCP PBT 3010-104 10% Glass Fiber Filled
Product Description: PBT glass fiber 10% reinforced injection molding grade.Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent..
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
Gromax CCP PBT 4815-NCB 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
|
|||
| Arc Resistance | 90 sec | 90 sec | ASTM D495 |
|
Gromax PBT 4115-201D 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
|
|||