Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Static Decay = 1.0 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Static Decay <= 1.0 sec
<= 1.0 sec
ISO IEC 61340-5-1
Premix Thermoplastics PRE-ELEC® ESD 5300 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5300 is a static dissipative thermoplastic compound based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance valu..
Static Decay <= 1.0 sec
<= 1.0 sec
ISO IEC 61340-5-1
Premix Thermoplastics PRE-ELEC® ESD 5500 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5500 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5500 can be injectio..
Static Decay <= 1.0 sec
<= 1.0 sec
ISO IEC 61340-5-1
Premix Thermoplastics PRE-ELEC® ESD 5510 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5510 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5510 can be injectio..
Static Decay <= 1.0 sec

@Thickness 1.00 mm
<= 1.0 sec

@Thickness 0.0394 in
ISO IEC 61340-5-1
Premix Thermoplastics PRE-ELEC® ESD 6300 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6300 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD6300 has be..
Static Decay <= 1.0 sec

@Thickness 1.00 mm
<= 1.0 sec

@Thickness 0.0394 in
ISO IEC 61340-5-1
Premix Thermoplastics PRE-ELEC® ESD 6600 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6000 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6000 has b..
Static Decay <= 1.0 sec

@Thickness 1.00 mm
<= 1.0 sec

@Thickness 0.0394 in
ISO IEC 61340-5-1
Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6610 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6610 has b..
Static Decay <= 1.0 sec
<= 1.0 sec
400 um thick sheet; ISO IEC 61340-5-1
Premix Thermoplastics PRE-ELEC® ESD 1100  (discontinued **)
PRE-ELEC ESD 1100 is a static dissipative thermoplastic compound based on PETG. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 1100 has been developed for the e..
Static Decay <= 1.0 sec
<= 1.0 sec
5000V to <50V; FTMS101B
SABIC Innovative Plastics LNP STAT-LOY 93000LTH Acrylic
LNP* STAT-LOY* 93000LTH is a compound based on Acrylic resin. Added features of this material include: Antistatic, Transparent and Formulation Locked.
Static Decay <= 1.0 sec
<= 1.0 sec
5000V to <50V; FTMS101B
SABIC Innovative Plastics LNP STAT-LOY A3000TXB ABS
LNP* STAT-LOY* A3000TXB is a compound based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives and Bioassessed to ISO 10993...
Static Decay <= 1.0 sec
<= 1.0 sec
5000V to <50V; FTMS101B
SABIC Innovative Plastics LNP STAT-LOY A3000TXJ ABS
LNP* STAT-LOY* A3000TXJ is a product based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives.
Static Decay <= 1.0 sec

@Temperature 23.0 °C
<= 1.0 sec

@Temperature 73.4 °F
50% RH; JIS L1049
Samsung Cheil Industries Infino® EM-8240C MPPE, Glass Filled
MPPE/GF material that is used in the main frame of banknote sortersInformation provided by Samsung Cheil Industries.
Static Decay <= 1.0 sec

@Temperature 23.0 °C
<= 1.0 sec

@Temperature 73.4 °F
50% RH; JIS L1049
Samsung Cheil Industries Infino® EM-8240C MPPE, Glass Filled
MPPE/GF material that is used in the main frame of banknote sortersInformation provided by Samsung Cheil Industries.
Static Decay <= 1.0 sec
<= 1.0 sec
MIL B-81705
Arkema Group Pebax® MH 1657 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MH 1657 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MH 1657 is an inherently dissipative polymer and can be dry blended or compounded w..
Static Decay <= 1.0 sec
<= 1.0 sec
MIL B-81705
Arkema Group Pebax® MV 1074 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MV 1074 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MV 1074 SA 01 is an inherently dissipative polymer and can be dry blended or ..
Static Decay <= 1.0 sec
<= 1.0 sec
MIL B-81705
Arkema Group Pebax® MV 1074 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MV 1074 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MV 1074 SP 01 is an inherently dissipative polymer and can be dry blended or ..
Copyright © lookpolymers.com All Rights Reserved