| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycolac® G366 ABS (Europe-Africa-Middle East)
CYCOLAC G366 is a "new technology" grade of ABS exhibiting outstanding property balance, a good flow, medium impact, medium to high heat resistant and an excellent stability during injection mouldin..
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycolac® GPM5500 ABS (Europe-Africa-Middle East)
CYCOLAC GPM5500 is a multi purpose injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC GPM5500 has a wide processing window. It is recommended for application..
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycolac® GPM5500U ABS (Europe-Africa-Middle East)
CYCOLAC GPM5500U is a UV stabilized multi purpose injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC GPM5500U has a wide processing window. It is recommended..
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycolac® S701SU ABS (Europe-Africa-Middle East)
CYCOLAC S701SU is an ABS with improved UV resistance, providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an exce..
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycolac® S703T ABS (Europe-Africa-Middle East)
CYCOLAC S703T is a super high flow ABS developed for thin wall injection/compression moulding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycolac® X37 ABS (Europe-Africa-Middle East)
CYCOLAC X37 is the highest heat material available in the CYCOLAC range of materials and is widely recognized within the automotive industry as being the industry standard for high heat ABS. It comb..
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Europe-Africa-Middle East)
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Europe-Africa-Middle East)
Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications.
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® C3100 PC+ABS (Europe-Africa-Middle East)
C3100 is blow moulding/extrusion grade offering low temperature ductility, high heat resistance and high meltstrength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C6200 is a non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. C6200 has improved processing window and edge crac..
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Asia Pacific)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS
PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Americas region.
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Europe-Africa-Middle East)
PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East re..
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Asia Pacific)
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Europe-Africa-Middle East)
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur..
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Lexan® HF1110R PC (Europe-Africa-Middle East)
LEXAN HF1110R is a high flow grade especially designed for applications that require thin wall sections and high flow lengths.
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® C1100HF PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1100HF is the improved flow version of CYCOLOY C1100 and has been developed to better fill long and complex parts while maintaining still excellent mechanical properties. Its superior flow ..
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS
Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs.
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo..
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® FXC630FE PC+ABS (Europe-Africa-Middle East)
Multi purpose flame retarded PC+ABS injection moulding grade, suitable for those applications that require ferrite colour effects.This data was supplied by SABIC-IP for the Europe-Africa-Middle East..
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Lexan® ML3982 PC (Europe-Africa-Middle East)
LEXAN ML3982 is an UV stabilized grade, with an excellent flow. It contains a release agent to ensure easy processing.
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics ULTEM 2310 PEI (Europe-Africa-Middle East)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics ULTEM 2310R PEI (Europe-Africa-Middle East)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics ULTEM 2400 PEI (Europe-Africa-Middle East)
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics ULTEM 2410 PEI (Europe-Africa-Middle East)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Valox® SHF4960 PBT
Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release.
|
|||
| Dielectric Strength |
35.0
kV/mm @Thickness 0.800 mm |
889
kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Europe-Africa-Middle East)
CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
|
|||