| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® C2100 PC+ABS (Asia Pacific)
CYCOLOY C2100 is a flame retardant blend, specifically developed to meet the stringent requirements of mains current carrying applications. CYCOLOY C2100 combines
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according ..
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® CY8540 PC+ABS (Europe-Africa-Middle East)
CYCOLOY CY8540 is a PC+ABS blend, especially designed for textile backmolding in automotive interior applications. High flow grade, which allows low temperature processing to maintain fabric integri..
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Asia Pacific)
PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Europe-Africa-Middle East)
CYCOLOY LG9000 is a low gloss PC+ABS injection moulding grade. LG9000 combines good impact / heat and UV resistance with a low gloss surface appearence. It is suitable for automotive interior applic..
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® XCY620HS PC+ABS
PC+ ABS General Purpose Non-FR
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Lexan® 121R PC (Europe-Africa-Middle East)
LEXAN 121R is a low viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 121R is available in transparent, translucent and opaque colours.
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Lexan® 161R PC (Europe-Africa-Middle East)
LEXAN 161R is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 161R is available in transparent, translucent and opaque colours.
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Lexan® 2034 PC (Europe-Africa-Middle East)
LEXAN 2034 is a medium viscosity flame retardant grade. The material is UV-stabilized. Glow wire at 960C also satisfies EDF spec HN 60-S-02.
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Lexan® 2814R PC (Europe-Africa-Middle East)
LEXAN 2814R is a high viscosity, 10% glass reinforced, flame retardant grade, especially developed to meet the CSTB M2 flammability rating.
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Lexan® 920A PC (Europe-Africa-Middle East)
LEXAN 920A is a medium viscosity flame retardant grade, especially suitable for electrical applications.
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Lexan® HP2NR PC (Europe-Africa-Middle East)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no..
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Lexan® HPS1R PC (Europe-Africa-Middle East)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains..
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Lexan® LS2 PC (Europe-Africa-Middle East)
LEXAN LS2 is a medium viscosity grade especially designed for applications with high optical requirements in terms of clarity and light transmission.
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® C1100HF PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1100HF is the improved flow version of CYCOLOY C1100 and has been developed to better fill long and complex parts while maintaining still excellent mechanical properties. Its superior flow ..
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1200HF is the improved version of CYCOLOY C1200 and has been developed to provide enhanced productivity and surface appearance for
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS
UV stabilized, non-FR PC/ABS of excellent flow and impact performance
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Lexan® 143 PC (Europe-Africa-Middle East)
LEXAN 143 is a medium viscosity U.V. stabilized multi purpose grade. LEXAN 143 is available in transparent, translucent and opaque colours.
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Lexan® 221R PC (Europe-Africa-Middle East)
LEXAN 221R is a low viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.4 mm approved.
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 1.00 mm
|
432
kV/in <br>@Thickness 0.0394 in
|
short time; IEC 60243-1 |
|
SABIC Innovative Plastics Lexan® 940 PC (Europe-Africa-Middle East)
LEXAN 940 is a medium viscosity flame retardant grade, especially suitable for electrical applications.
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.00 mm
|
432
kV/in <br>@Thickness 0.118 in
|
ASTM D149 |
|
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)
AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. ..
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East)
VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures.
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East)
VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Europe-Africa-Middle East)
Unreinforced PBT+PC alloy. Improved retention of mechanical properties under UV. Excellent low temperature/chemical
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Europe-Africa-Middle East)
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Xenoy® CL101 PBT+PC
Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica..
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 2.00 mm
|
432
kV/in <br>@Thickness 0.0787 in
|
Practical Use (Water Absorption 3.0%); ASTM-D149 |
|
Toyobo GLAMIDE® T-808-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
|
|||
| Dielectric Strength |
17.0
kV/mm <br>@Thickness 3.20 mm
|
432
kV/in <br>@Thickness 0.126 in
|
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics Lexan® ML3260 PC (Europe-Africa-Middle East)
LEXAN ML3260 is a medium viscosity, 15% glass reinforced, flame retardant grade especially designed for applications like computer cartridges.
|
|||