| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Insulation Resistance |
1.00e+10
-
1.00e+11
ohm <br>@Temperature 90.0 - 90.0 °C
|
1.00e+10
-
1.00e+11
ohm <br>@Temperature 194 - 194 °F
|
Average value: 7.75e+10 ohm Grade Count:8 |
|
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..
|
|||
| Insulation Resistance | <= 1.00e+10 ohm | <= 1.00e+10 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-8264 PEEK, with CNT
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect..
|
|||
| Insulation Resistance | <= 1.00e+10 ohm | <= 1.00e+10 ohm | |
|
Lehmann & Voss LUVOCOM® 1850-8322 PBT, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
|
|||
| Insulation Resistance | >= 1.00e+10 ohm | >= 1.00e+10 ohm | |
|
Lehmann & Voss LUVOCOM® 3-8266 Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Insulation Resistance | >= 1.00e+10 ohm | >= 1.00e+10 ohm | |
|
Lehmann & Voss LUVOCOM® 3-8266/BL Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Insulation Resistance | >= 1.00e+10 ohm | >= 1.00e+10 ohm | |
|
Lehmann & Voss LUVOCOM® 3-8363 Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Insulation Resistance | <= 1.00e+10 ohm | <= 1.00e+10 ohm | |
|
Lehmann & Voss LUVOCOM® 80-7653 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Antistatic.No change of electric potential at bearings in case of separation of charge caused b..
|
|||
| Insulation Resistance | >= 1.00e+10 ohm | >= 1.00e+10 ohm | |
|
Lehmann & Voss LUVOCOM® 1100-8401 Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
|
|||
| Insulation Resistance | <= 1.00e+10 ohm | <= 1.00e+10 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-7914 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi..
|
|||
| Insulation Resistance | <= 1.00e+10 ohm | <= 1.00e+10 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-7916-1 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi..
|
|||
| Insulation Resistance | >= 1.00e+10 ohm | >= 1.00e+10 ohm | |
|
Lehmann & Voss LUVOCOM® 1-7180/EG Polyamide 66, with carbon fiber, PTFE, lubricant modified, high viscosity, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Insulation Resistance |
1.00e+10
ohm <br>@Temperature 90.0 °C
|
1.00e+10
ohm <br>@Temperature 194 °F
|
IEC 60167 |
|
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs..
|
|||
| Insulation Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | Dry; IEC 167 |
|
Vyncolit 2923 W Novolac Phenolic
Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group
|
|||
| Insulation Resistance | 1.00e+10 ohm | 1.00e+10 ohm | Dry; IEC 167 |
|
Vyncolit 4523 XB Novolac Phenolic
Organic and inorganic filled phenolic molding compound with good mechanical and thermal properties. Improved heat resistance compared to organic filled compounds.USES: Fuse holders, brush holders, ..
|
|||
| Insulation Resistance |
1.00e+10
ohm <br>@Temperature 90.0 °C,<br> Time 173000 sec
|
1.00e+10
ohm <br>@Temperature 194 °F,<br> Time 48.0 hour
|
95% RH |
|
Chevron Phillips Xtel® XE3035BL Polyphenylene Sulfide Alloy
Xtel® XE3035BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p..
|
|||
| Insulation Resistance |
1.00e+10
ohm <br>@Temperature 90.0 °C,<br> Time 173000 sec
|
1.00e+10
ohm <br>@Temperature 194 °F,<br> Time 48.0 hour
|
95% RH |
|
Chevron Phillips Xtel® XE3035NA Polyphenylene Sulfide Alloy
Xtel® XE3035NA is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p..
|
|||
| Insulation Resistance |
1.00e+10
ohm <br>@Diameter 8.00 - 10.0 mm
|
1.00e+10
ohm <br>@Diameter 0.315 - 0.394 in
|
24hr/50°C+24h in water at 23°C; IEC; IEC/EN 61212-2 6.2 |
|
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes
Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength. Retains electrical properties at high air humidity. High resistance to chemicals.Applications..
|
|||
| Insulation Resistance |
1.00e+10
ohm <br>@Diameter 8.00 - 10.0 mm
|
1.00e+10
ohm <br>@Diameter 0.315 - 0.394 in
|
24hr/50°C+24h in water at 23°C; IEC; IEC/EN 61212-2 6.2 |
|
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Tubes
Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength, even at high temperatures. Retains electrical properties at high air humidity. High resistanc..
|
|||
| Insulation Resistance | >= 1.00e+10 ohm | >= 1.00e+10 ohm | After immersion in water; IEC 1212-2 6.3 |
|
Hippe EP CP 201 Cellulose Paper Reinforced Epoxy Resin - Sheet
Used in electronic applications. Good stability of electrical properties under high humidity. Flame retardant.Information provided by Hippe.
|
|||
| Insulation Resistance | >= 1.00e+10 ohm | >= 1.00e+10 ohm | After immersion in water; IEC 1212-2 6.3 |
|
Hippe EP GC 205 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech..
|
|||
| Insulation Resistance | >= 1.00e+10 ohm | >= 1.00e+10 ohm | After immersion in water; IEC 1212-2 6.3 |
|
Hippe PF CP 204 Cellulose Paper Reinforced Phenolic Resin - Sheet
Used in electrical and electronic applications. Good stability of electrical properties under high humidity. Also available in cold or hot-punching versions.Information provided by Hippe.
|
|||
| Insulation Resistance | >= 1.00e+10 ohm | >= 1.00e+10 ohm | After immersion in water; IEC 1212-2 6.3 |
|
Hippe SI GC 201 Woven Glass Cloth Reinforced Silicone Resin - Sheet
Used in electrical and electronic applications. Extremely good electrical properties under dry conditions; good properties under humid conditions.Information provided by Hippe.
|
|||
| Insulation Resistance |
1.00e+10
ohm <br>@Diameter 8.00 - 10.0 mm
|
1.00e+10
ohm <br>@Diameter 0.315 - 0.394 in
|
24hr/50°C+24h in water at 23°C; IEC; IEC/EN 61212-2 6.2 |
|
Elektro-Isola G-Etronax EP FR Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes
Description: Mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperatures. Very good stability of electrical properties when exposed to high relati..
|
|||
| Insulation Resistance | 1.00e+10 ohm | 1.00e+10 ohm | After Boiling; ASTM D257 |
|
Chang Chun Plastic Longlite PM T310 Impact Phenolic Molding Compound
ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd.
|
|||
| Insulation Resistance | 1.00e+10 ohm | 1.00e+10 ohm | Normal; ASTM D257 |
|
Chang Chun Plastic Longlite PM T33J General Purpose Phenolic Molding Compound
ASTM Grades per ASTM D700 are 2,3.Information provided by Dowell Trading Company Ltd.
|
|||
| Insulation Resistance | >= 1.00e+10 ohm | >= 1.00e+10 ohm | (test voltage = 100 VDC; Mil-I-46058C |
|
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
|
|||
| Insulation Resistance | 1.00e+10 ohm | 1.00e+10 ohm | Normal; ASTM D257 |
|
Chang Chun Plastic Longlite PM T385J General Purpose Phenolic Molding Compound
ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd.
|
|||
| Insulation Resistance | >= 1.00e+10 ohm | >= 1.00e+10 ohm | |
|
Lehmann & Voss LUVOCOM® 1301-8305 PPS, linear, with glass fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam..
|
|||
| Insulation Resistance | >= 1.00e+10 ohm | >= 1.00e+10 ohm | |
|
Lehmann & Voss LUVOCOM® 1-8227 Polyamide 66, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||