Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Insulation Resistance = 1.00e+11 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Insulation Resistance 10.0 - 1.00e+11 ohm
10.0 - 1.00e+11 ohm
Average value: 4.63e+9 ohm Grade Count:24
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
Insulation Resistance 1.00e+8 - 1.00e+11 ohm
1.00e+8 - 1.00e+11 ohm
Average value: 1.94e+10 ohm Grade Count:6
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Insulation Resistance 1.00e+8 - 1.00e+11 ohm
1.00e+8 - 1.00e+11 ohm
Average value: 2.78e+10 ohm Grade Count:10
Overview of materials for Phenolic; Unreinforced; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of..
Insulation Resistance 1.00e+9 - 1.00e+11 ohm
1.00e+9 - 1.00e+11 ohm
Average value: 4.52e+10 ohm Grade Count:5
Overview of materials for Phenolic, Novolac, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values..
Insulation Resistance 1.00e+11 - 1.00e+11 ohm

@Temperature 90.0 - 90.0 °C
1.00e+11 - 1.00e+11 ohm

@Temperature 194 - 194 °F
Average value: 1.00e+11 ohm Grade Count:1
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..
Insulation Resistance 1.00e+10 - 1.00e+11 ohm

@Temperature 90.0 - 90.0 °C
1.00e+10 - 1.00e+11 ohm

@Temperature 194 - 194 °F
Average value: 7.75e+10 ohm Grade Count:8
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..
Insulation Resistance 100 - 1.00e+11 ohm
100 - 1.00e+11 ohm
Average value: 1.67e+10 ohm Grade Count:6
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Insulation Resistance 1.00e+9 - 1.00e+11 ohm
1.00e+9 - 1.00e+11 ohm
Lehmann & Voss LUVOCOM® 6-8438-1 Polyamide 12, with glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Suitable for discharging of statically generated electricity.Dynamic stressed parts.Low waterab..
Insulation Resistance 1.00e+9 - 1.00e+11 ohm
1.00e+9 - 1.00e+11 ohm
Lehmann & Voss LUVOCOM® 6-8548 Polyamide 12, with glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Suitable for discharging of statically generated electricity.Dynamic stressed parts.Low waterab..
Insulation Resistance 1.00e+10 - 1.00e+11 ohm
1.00e+10 - 1.00e+11 ohm
Dry; IEC 167
Vyncolit 2923 W Novolac Phenolic
Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group
Insulation Resistance 1.00e+10 - 1.00e+11 ohm
1.00e+10 - 1.00e+11 ohm
Dry; IEC 167
Vyncolit 2920 W Novolac Phenolic
Mineral and organic filled molding compound with good dimensional stability and heat resistance.USES: Carburettor and intake manifold thermal insulator.Information provided by Vyncolit, a Sumitomo B..
Insulation Resistance 1.00e+9 - 1.00e+11 ohm
1.00e+9 - 1.00e+11 ohm
Dry; IEC 167
Vyncolit X682 Novolac Phenolic
Glass fiber, glass bead and graphite filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction.USES: Water pump seals and self-lubricating bearings.Info..
Insulation Resistance 10000 - 1.00e+11 ohm
10000 - 1.00e+11 ohm
Average value: 3.33e+10 ohm Grade Count:3
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Copyright © lookpolymers.com All Rights Reserved