| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-7835 PEEK, with glass fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Low warpage, isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts,..
|
|||
| Insulation Resistance | <= 1.00e+12 ohm | <= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-8157 PEEK, with CNT
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-8292 PEEK, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1301-8386 PPS, linear, with aramid reinforcement and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1700-8541 PPO, unreinforced
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Isotropic shrinkage characteristics.Superheated steam sterilizable.Infor..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1-7985 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o..
|
|||
| Insulation Resistance | <= 1.00e+12 ohm | <= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1-8490 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1850-7942 PBT, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 19-7221/OR Polyamide 46, with glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 19-8250 Polyamide 46, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Highly dimensionally stable at elevated tem..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 50-8276 Polycarbonate, with PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 80-0837 Polyacetal-copolymer, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 80-7655/RD Polyacetal-copolymer, with aramid reinforcement and PTFE, toughness-modified, high viscosity
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | Between adjacent Conductive wire |
|
Fujipoly Industries Gold 8000 Type B Connector
Gold 8000 elastomeric connector elements are D-shaped with low durometer silicone rubber cores around which flat metallic golf=plated conductors are vulcanized in a row parallel to each other. The t..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-0950/RD PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-7310 PEEK, with glass fiber, easy flowing, low-warpage
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High dimensionally stable precision parts, high continuous use temperature.Superheated ste..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-7826/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1301-8060 PPS, linear, with glass fiber and PTFE, high viscosity
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Improved friction and wear be..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1-7032-B Polyamide 66, with aramid reinforcement and PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Improved heat resistance.Control disks, cams, sliding elem..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1-7701 Polyamide 66, with glass fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, ..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1850/PL/15/BK PBT, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Parts for electric and electro..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 50/TF/15/BK Polycarbonate, with PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 100-7846 Thermoplastic polyurethane, with aramid reinforcement
Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1100-8049 Polyether sulfone, with glass fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1105/TF/20/NAT PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Insulation Resistance |
1.00e+12
ohm <br>@Temperature 90.0 °C
|
1.00e+12
ohm <br>@Temperature 194 °F
|
IEC 60167 |
|
Solvay Specialty Polymers Ryton® R-4-240NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat..
|
|||
| Insulation Resistance | 1.00e+12 ohm | 1.00e+12 ohm | Average value: 1.00e+12 ohm Grade Count:12 |
|
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..
|
|||
| Insulation Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1106-7742 Polyether imide, with glass fiber, demolding aid
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||