| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Insulation Resistance | 1.00e+8 - 1.00e+11 ohm | 1.00e+8 - 1.00e+11 ohm | Average value: 1.94e+10 ohm Grade Count:6 |
|
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
|
|||
| Insulation Resistance | 1.00e+8 - 1.00e+9 ohm | 1.00e+8 - 1.00e+9 ohm | Average value: 4.00e+8 ohm Grade Count:3 |
|
Overview of materials for Phenolic/Glass Fiber SMC
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Glass Fiber SMC". Each property range of values reported is minimum and maximum values of appro..
|
|||
| Insulation Resistance | <= 1.00e+8 ohm | <= 1.00e+8 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-7185 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
|
|||
| Insulation Resistance | <= 1.00e+8 ohm | <= 1.00e+8 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-7760 PEEK, with carbon fiber, PTFE, lubricant modified, high viscosity
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
|
|||
| Insulation Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-8168 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
|
|||
| Insulation Resistance | <= 1.00e+8 ohm | <= 1.00e+8 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-8350 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
|
|||
| Insulation Resistance | <= 1.00e+8 ohm | <= 1.00e+8 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-8422 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
|
|||
| Insulation Resistance | >= 1.00e+8 ohm | >= 1.00e+8 ohm | |
|
Lehmann & Voss LUVOCOM® 1-8181 Polyamide 66, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Reduced moment of inertia compared with metal parts.Elec..
|
|||
| Insulation Resistance | >= 1.00e+8 ohm | >= 1.00e+8 ohm | |
|
Lehmann & Voss LUVOCOM® 1-8218 Polyamide 66, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Reduced moment of inertia compared with metal parts.Elec..
|
|||
| Insulation Resistance | >= 1.00e+8 ohm | >= 1.00e+8 ohm | |
|
Lehmann & Voss LUVOCOM® 1850-7431 PBT, with carbon fiber and glass spheres
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low warpage.Low waterabsorbtion, for dimensional stable precision parts.Par..
|
|||
| Insulation Resistance | >= 1.00e+8 ohm | >= 1.00e+8 ohm | |
|
Lehmann & Voss LUVOCOM® 1-8520 Polyamide 66, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Reduced moment of inertia compared with metal parts.Elec..
|
|||
| Insulation Resistance | <= 1.00e+8 ohm | <= 1.00e+8 ohm | |
|
Lehmann & Voss LUVOCOM® 1-0889-5 Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
|
|||
| Insulation Resistance |
1.00e+8
ohm @Diameter 8.00 - 10.0 mm |
1.00e+8
ohm @Diameter 0.315 - 0.394 in |
24hr/50°C+24h in water at 23°C; IEC; IEC/EN 61212-2 6.2 |
|
Elektro-Isola Etronax MF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes
Description: Mechanical applications. Impact-resistant, noise-reducing and wear-resistant material. Well suited as a low-friction material. High wear resistance in aggressive and dust-filled environ..
|
|||
| Insulation Resistance |
1.00e+8
ohm @Diameter 8.00 - 10.0 mm |
1.00e+8
ohm @Diameter 0.315 - 0.394 in |
24hr/50°C+24h in water at 23°C; IEC; IEC/EN 61212-2 6.2 |
|
Elektro-Isola Etronit B67 Phenolic, Paper Reinforcement, Dark Brown, Tubes
Description: For mechanical and electrical low-voltage applications. Very good electrical properties at high air humidity. Applications: Winding tubes in the foil and metal foil industries and carri..
|
|||
| Insulation Resistance |
1.00e+8
ohm @Thickness >=3.00 mm |
1.00e+8
ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
|
Elektro-Isola Etronit II Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Mechanical and electrical applications used at normal air humidity. Very good electrical values.Information provided by Elektro-Isola
|
|||
| Insulation Resistance |
1.00e+8
ohm @Thickness >=3.00 mm |
1.00e+8
ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
|
Elektro-Isola Etronit IIQ R Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition..
|
|||
| Insulation Resistance |
1.00e+8
ohm @Thickness >=3.00 mm |
1.00e+8
ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
|
Elektro-Isola Etronit IIQ R XX Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition..
|
|||
| Insulation Resistance |
1.00e+8
ohm @Thickness >=3.00 mm |
1.00e+8
ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
|
Elektro-Isola Etronit IIQ S Phenolic, Paper Reinforcement, Black, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Material is black throughout. Elegant surface finish combined with good ..
|
|||
| Insulation Resistance |
1.00e+8
ohm @Thickness >=3.00 mm |
1.00e+8
ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
|
Elektro-Isola Etronit IR Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: High-voltage insulation material at mains frequency. High breakdown voltage in oil and reasonable breakdown voltage in air at normal air humidity. Very low water absorption.Application:..
|
|||
| Insulation Resistance |
1.00e+8
ohm @Thickness >=3.00 mm |
1.00e+8
ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
|
Elektro-Isola Etronit IS Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Very good high-voltage insulation material. Very high breakdown voltage, in particular parallel to the layers. Dimensionally stable.Application: Insulation material in high-voltage tap ..
|
|||
| Insulation Resistance |
1.00e+8
ohm @Thickness >=3.00 mm |
1.00e+8
ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
|
Elektro-Isola Etronit IV C Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Grade for mechanical electrotechnical and high frequency purposes. Tropical grade, well suited for areas where high air humidity can be expected and lasting electrical properties despit..
|
|||
| Insulation Resistance |
1.00e+8
ohm @Thickness >=3.00 mm |
1.00e+8
ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
|
Elektro-Isola Etronit IV Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Grade for mechanical electrotechnical and high frequency purposes. Tropical grade, well suited for areas where high air humidity can be expected. Suitable as high-frequency insulation o..
|
|||
| Insulation Resistance |
1.00e+8
ohm @Thickness >=3.00 mm |
1.00e+8
ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
|
Elektro-Isola Etronit MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets
Description: The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. The surfaces are grey as standard, but other colors can be selected from the color chart..
|
|||
| Insulation Resistance |
1.00e+8
ohm @Thickness >=3.00 mm |
1.00e+8
ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
|
Elektro-Isola G-Etronax M Melamine, Glass Fabric Reinforcement, White, Sheets
Description: Melamine-based composite material reinforced with glass fabric. High arc resistance and tracking resistance. Flame-resistant. Self-extinguishing.Information provided by Elektro-Isola
|
|||
| Insulation Resistance |
1.00e+8
ohm @Diameter 8.00 - 10.0 mm |
1.00e+8
ohm @Diameter 0.315 - 0.394 in |
24hr/50°C+24h in water at 23°C; IEC; IEC/EN 61212-2 6.2 |
|
Elektro-Isola G-Etronax M Melamine, Glass Fabric Reinforcement, White, Tubes
Description: Mechanical and electrical applications. Arc-resistant and tracking-resistant material. Good flame resistance. Self-extinguishing. Halogen-free. Lower high-voltage values and insulation ..
|
|||
| Insulation Resistance |
>=
1.00e+8
ohm @Diameter 8.00 - 10.0 mm |
>=
1.00e+8
ohm @Diameter 0.315 - 0.394 in |
After immersion in water; IEC 1212-2 5.2 |
|
Hippe EP MP 21 Mica Paper Reinforced Epoxy Resin - Round, Rolled Tube
Used in mechanical, electrical and electronic applications. Good stability of electrical properties when exposed to high relative humidity. Good heat resistance.Information provided by Hippe.
|
|||
| Insulation Resistance | 1.00e+8 ohm | 1.00e+8 ohm | After Boiling; ASTM D257 |
|
Chang Chun Plastic Longlite PM T33J General Purpose Phenolic Molding Compound
ASTM Grades per ASTM D700 are 2,3.Information provided by Dowell Trading Company Ltd.
|
|||
| Insulation Resistance | 1.00e+8 ohm | 1.00e+8 ohm | After Boiling; ASTM D257 |
|
Chang Chun Plastic Longlite PM T373J Electrical Phenolic Molding Compound
ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd.
|
|||
| Insulation Resistance | >= 1.00e+8 ohm | >= 1.00e+8 ohm | After immersion in water; IEC 1212-2 6.3 |
|
Hippe PF GC 201 Woven Glass Cloth Reinforced Phenolic Resin - Sheet
Used in mechanical and electrical applications. High mechanical strength and good electrical properties under normal humidity. Heat resistant. Information provided by Hippe.
|
|||
| Insulation Resistance | 1.00e+8 ohm | 1.00e+8 ohm | After Boiling; ASTM D257 |
|
Chang Chun Plastic Longlite PM T385J General Purpose Phenolic Molding Compound
ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd.
|
|||