| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Insulation Resistance | 100 - 1.00e+9 ohm | 100 - 1.00e+9 ohm | Average value: 3.41e+8 ohm Grade Count:21 |
|
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of ..
|
|||
| Insulation Resistance | 100 - 1.00e+9 ohm | 100 - 1.00e+9 ohm | Average value: 2.86e+8 ohm Grade Count:14 |
|
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
|
|||
| Insulation Resistance | 100 - 1.00e+12 ohm | 100 - 1.00e+12 ohm | Average value: 7.14e+10 ohm Grade Count:28 |
|
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
|
|||
| Insulation Resistance | 100 - 1.00e+11 ohm | 100 - 1.00e+11 ohm | Average value: 1.67e+10 ohm Grade Count:6 |
|
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 1105-8048 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Insulation Resistance | 100 - 100000 ohm | 100 - 100000 ohm | |
|
Lehmann & Voss LUVOCOM® 1-7305/BK Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 1800-8449 PET, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous d..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 1-8357 Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Electrically conductive, suitable for continuous dischar..
|
|||
| Insulation Resistance | 100 ohm | 100 ohm | |
|
Lehmann & Voss LUVOCOM® 19-7748 Polyamide 46, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 20-0659 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 20-7970 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 3-8351 Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated el..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 6/CF/30 Polyamide 12, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s..
|
|||
| Insulation Resistance | 100 - 100000 ohm | 100 - 100000 ohm | |
|
Lehmann & Voss LUVOCOM® 65-7712/GY PP-copolymer, with carbon fiber and glass fiber, electrically conducting
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Information provided by Lehmann & Voss & Co.KG..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 65-8378 PP-copolymer, with carbon fiber
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & ..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 6-8395 Polyamide 12, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 80-7489 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 80-7727 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 80-7752 Polyacetal-copolymer, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 80-7884 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 80-7917 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 80-8082 Polyacetal-copolymer, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
|
|||
| Insulation Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | |
|
Lehmann & Voss LUVOCOM® 1200-7116-1 ABS, with carbon fiber
Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff ..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 1301-0825 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 1-7956 Polyamide 66, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 1850-7581-1 PBT, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 80-8072 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
|
|||
| Insulation Resistance | 100 - 100000 ohm | 100 - 100000 ohm | |
|
Lehmann & Voss LUVOCOM® TPE-7711/GY Thermoplastic elastomer, with carbon fiber, electrically conducting
Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Dynamic stressed parts.Bearings, sleeves, sliding elements, chair rollers, handles.Info..
|
|||
| Insulation Resistance | <= 100 ohm | <= 100 ohm | |
|
Lehmann & Voss LUVOCOM® 1-0890 Polyamide 66, with carbon fiber, low-warpage, heat stabilized