| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics Lexan® 925 PC (Asia Pacific)
Lexan* 925 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating. Lexan resin 925 is available in various opa..
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics Lexan® 940ASR PC
More robust design of standard 900 series flame retardant grade. Internal mold release.
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics Lexan® 945A PC (Asia Pacific)
Lexan* 945A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and ti..
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | surface, PLC code 3; UL 746A |
|
SABIC Innovative Plastics Lexan® PPC4701 PPC
High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi.This data was supplied by SABIC-IP for the Americas region.
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | surface, PLC code 3; UL 746A |
|
SABIC Innovative Plastics Lexan® PPC4701R PPC
High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. Internal mold release.This data was supplied by SABIC-IP for the Americas region.
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics Lexan® 920A PC (Asia Pacific)
Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors.
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics Lexan® 925A PC (Asia Pacific)
Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran..
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics Lexan® HPH4704 PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril..
|
|||
| High Amp Arc Ignition, HAI |
<=
15
arcs <br>@Thickness 1.50 mm
|
<=
15
arcs <br>@Thickness 0.0591 in
|
UL Rating PLC 4 (<15 arcs) |
|
Covestro Apec® DP9-9351 High-Heat Polycarbonate, General Purpose
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
|
|||
| High Amp Arc Ignition, HAI |
15
-
30
arcs <br>@Thickness 6.00 mm
|
15
-
30
arcs <br>@Thickness 0.236 in
|
UL Rating PLC 3 (15-30 arcs) |
|
Covestro Makrolon® SF-800 Polycarbonate, Structural Foam
(discontinued **)
Properties based on foam density of 0.90 g/cc.Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially..
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 1000RV PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 1010 PEI
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer b..
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 1010F PEI
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer b..
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | surface, PLC code 3; UL 746A |
|
SABIC Innovative Plastics Ultem 1010RV PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacif..
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | surface, PLC code 3; UL 746A |
|
SABIC Innovative Plastics Ultem 1010V PEI (Asia Pacific)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa..
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | surface, PLC code 3; UL 746A |
|
SABIC Innovative Plastics Ultem 1100FV PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM HU1000 PEI (Asia Pacific)
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM MD131A PEI
Transparent, enhanced flow Polyetherimide (Tg 217C). US FDA and EU Food Contact compliant.
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics Valox® 508 PBT+PC
30% GR PBT+PC. Excellent mechanical and thermal performance. Non-flame retardant. Reduced warpage characteristics. Applications same as VALOX 420.
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics Valox® 553 PBT+PC
30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc.
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics Valox® 735 PBT (Asia Pacific)
40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics Xenoy® 6370 PBT+PC
30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility.
|
|||
| High Amp Arc Ignition, HAI |
15
-
29
arcs <br>@Thickness 1.57 mm
|
15
-
29
arcs <br>@Thickness 0.0618 in
|
UL PLC 3 (15-29 arcs) |
|
Sumitomo Bakelite North America 51-01 CAFR-P Mineral Filled Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ..
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
|
|||
| High Amp Arc Ignition, HAI | <= 15 arcs | <= 15 arcs | |
|
DuPont Teijin Films Mylar® A Polyester Film, 200 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
|
|||
| High Amp Arc Ignition, HAI | <= 15 arcs | <= 15 arcs | |
|
DuPont Teijin Films Mylar® A Polyester Film, 75 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
|
|||
| High Amp Arc Ignition, HAI | <= 15 arcs | <= 15 arcs | |
|
DuPont Teijin Films Mylar® LBTW Polyester Film, 48 Gauge
Mylar® LBTW is an uncoated, transparent polyester film that has been corona treated on one side to provide superior wetting and adhesion of inks, primers, and adhesives. Mylar® LBTW is commerciall..
|
|||
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
|
SABIC Innovative Plastics ULTEM 1000 PEI
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in natural color. Effective June, 20..
|
|||