| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149-97a |
|
Rogers Corporation Poron® 4701-30-20 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which ena..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149-97a |
|
Rogers Corporation Poron® 4701-30-20064 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement. Standard available thickness 0.064"Features and Benefits of PORON Products: Excelle..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149-97a |
|
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft
Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149-97a |
|
Rogers Corporation Poron® 4701-30-25037 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149-97a |
|
Rogers Corporation Poron® 4701-30-25047 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149-97a |
|
Rogers Corporation Poron® 4701-41-15 Urethane Foam, Soft, Enhanced Sealability
Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031"..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149-97a |
|
Rogers Corporation Poron® 4701-41-20 Urethane Foam, Soft, Enhanced Sealability
Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031"..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149-97a |
|
Rogers Corporation Poron® 4701-41-30 Urethane Foam, Soft, Enhanced Sealability
Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031"..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149-97a |
|
Rogers Corporation Poron® 4701-50 Supported Urethane Foam, Firm, PET Supported
Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149-97a |
|
Rogers Corporation Poron® 4701-50 Thin as Cast Urethane Foam, Firm, Thin as Cast
Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149-97a |
|
Rogers Corporation Poron® 4790-92-15 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force.Features and Benefits of PORON Products: Excellent compression set resistance which enables durable, long-term performance for gasketing, seali..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149-97a |
|
Rogers Corporation Poron® 4790-92-15 Urethane Foam, Extra Soft, Slow Rebound
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149-97a |
|
Rogers Corporation Poron® 4790-92-20 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149-97a |
|
Rogers Corporation Poron® 4701-30-25 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which enab..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149-97a |
|
Rogers Corporation Poron® 4790-92-25 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | S/T in Air |
|
Glastic GLASTHERM HT200 Insulation Sheet
HT200 features:High Hot Compressive StrengthLow Thermal ConductivityOil and Moisture ResistantReduces Heat LossHelps Control TemperatureFaster Mold StartupDesigned for reducing heat losses from plas..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill FR® PA6/6 GF33 FR-N BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame Retardant and Halogen FreeAppearance: BlackInformation provided by TP Composites, Inc...
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill FR® PA6/6 GF50 FR BK 50% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 50% Filler by WeightFeatures: Flame Retardant Appearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D877 |
|
Chesterton 274 Industrial Degreaser
Description: Chesterton® 274 Industrial Degreaser is an industrial strength, hard surface degreaser which will dissolve grease, oil, tar and other similar water insoluble soils generally encountere..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149 |
|
3M 4504 Single-Coated Foam Tape
3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149 |
|
3M 4104 Single-Coated Foam Tape
3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149 |
|
3M 4714 Single-Coated Foam Tape
3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | ASTM D149 |
|
Saint-Gobain Korel® K60 Firm Micro-cellular Polyurethane Foam
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill FR® PA6/6 GF50 FR UV X BK 50% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 50% Filler by WeightAdditive: Flame Retardant and UV StabilizerFeatures: Flame RetardantAppearance: BlackProcessing Method..
|
|||
| Dielectric Strength | 1.97 kV/mm | 50.0 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill FR® PA6/6 GF50 FR-N BK 50% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 50% Filler by WeightFeatures: Flame Retardant and Halogen FreeAppearance: BlackInformation provided by TP Composites, Inc...
|
|||