Polymer Property : Dielectric Strength = 1140 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Dielectric Strength 17.0 - 45.0 kV/mm
432 - 1140 kV/in
Average value: 25.4 kV/mm Grade Count:32
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..
Dielectric Strength 16.1 - 45.0 kV/mm
410 - 1140 kV/in
Average value: 27.8 kV/mm Grade Count:43
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Dielectric Strength 21.0 - 45.0 kV/mm
533 - 1140 kV/in
Average value: 30.4 kV/mm Grade Count:10
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Dielectric Strength 11.8 - 45.0 kV/mm
300 - 1140 kV/in
Average value: 19.3 kV/mm Grade Count:15
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..
Dielectric Strength 18.5 - 45.0 kV/mm
470 - 1140 kV/in
Average value: 27.7 kV/mm Grade Count:23
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Dielectric Strength 5.00 - 45.0 kV/mm
127 - 1140 kV/in
Average value: 30.6 kV/mm Grade Count:18
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Dielectric Strength 17.7 - 45.0 kV/mm
450 - 1140 kV/in
Average value: 27.5 kV/mm Grade Count:3
Overview of materials for Nylon 11 with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ..
Dielectric Strength 17.7 - 45.0 kV/mm
450 - 1140 kV/in
Average value: 37.1 kV/mm Grade Count:16
Overview of materials for Nylon 12, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Dielectric Strength 11.8 - 45.0 kV/mm
300 - 1140 kV/in
Average value: 25.8 kV/mm Grade Count:12
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..
Dielectric Strength 16.1 - 45.0 kV/mm
410 - 1140 kV/in
Average value: 24.1 kV/mm Grade Count:9
Overview of materials for Polycarbonate, 40% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E..
Dielectric Strength 18.0 - 45.0 kV/mm
457 - 1140 kV/in
Average value: 21.4 kV/mm Grade Count:8
Overview of materials for Acrylic, Optical Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of..