Polymer Property : Dielectric Strength = 16.9 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Dielectric Strength 16.9 kV/mm

@Thickness 3.17 mm
430 kV/in

@Thickness 0.125 in
in air; ASTM D149
Ravago Manufacturing Americas Hylex® P1010G30 HB Polycarbonate, 30% Fiberglass Reinforced
Information provided by Ravago.
Dielectric Strength 16.9 kV/mm

@Thickness 3.17 mm
430 kV/in

@Thickness 0.125 in
in air; ASTM D149
Ravago Manufacturing Americas Hylex® P1310G30 HB Polycarbonate, 30% Fiberglass Reinforced, UV Stabilized
Information provided by Ravago.
Dielectric Strength 16.9 kV/mm
429 kV/in
Short Time; ASTM D149
Plenco 50015 PET, Pellet, Injection Molded Natural Color  (discontinued **)
PLENCO 50015 is an engineering grade glass reinforced polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL recognized and available in white, natu..
Dielectric Strength 16.9 - 49.0 kV/mm
430 - 1240 kV/in
Average value: 26.3 kV/mm Grade Count:46
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Dielectric Strength 16.9 - 19.0 kV/mm
430 - 483 kV/in
Average value: 17.8 kV/mm Grade Count:7
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl..
Dielectric Strength 16.9 kV/mm
429 kV/in
ASTM D149
IDI Composites C-204 Thermoset Polyester, Sheet
CORROSION - (Patent pending). Versatile family of compounds designed for pressurized and thermo-mechanically stressed applications. Excellent corrosion resistance and high strength.Data provided by ..
Dielectric Strength >= 16.9 kV/mm
>= 430 kV/in
ASTM D149
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet
High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines..
Dielectric Strength 16.9 kV/mm

@Thickness 3.20 mm
429 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® EH7020 PBT
MINERAL FILLED, METALLIZABLE
Dielectric Strength 16.9 kV/mm
430 kV/in
Saint-Gobain CHR® G569 Glass Cloth Backing Acrylic Adhesive Pressure Sensitive Tape
Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°..
Dielectric Strength 16.9 kV/mm
430 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Luriblend® PSU GF20 TL5 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Dielectric Strength 16.9 kV/mm
430 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Luriblend® TPX-PA6/6-01072
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceInformation provided b..
Dielectric Strength 16.9 kV/mm
430 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill FR® PC FR HS GY154
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and UV StabilizerFeatures: Flame Retardant and Heat StabilizedAppearance: GreyInformation provided by TP Composites, Inc.
Dielectric Strength 16.9 kV/mm
430 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill FR® PC FR RD064
Availability: North AmericaForms: PelletsFeatures: Flame Retardant UL File Number: E157318Appearance: RedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Dielectric Strength 16.9 kV/mm
430 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill FR® PC FR SFX-GREEN 1.0
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantAppearance: GreenInformation provided by TP Composites, Inc.
Dielectric Strength 16.9 kV/mm
430 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® PSU GF20 BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Dielectric Strength 16.9 kV/mm

@Thickness 3.00 mm
430 kV/in

@Thickness 0.118 in
ASTM D149
Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated
Notes: General Purpose; U.L. 94 V-O at 0.57 mm; Colorable; Flame Retardant Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex
Dielectric Strength 16.9 kV/mm
430 kV/in
Tra-Con Tra-Bond 2110 High Impact Epoxy Staking Compound
TRA-BOND 2110 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, n..
Dielectric Strength 16.9 kV/mm
430 kV/in
Tra-Con Tra-Bond 2115 Clear High Strength Epoxy Adhesive
TRA-BOND 2115 is a clear, low viscosity epoxy formulation used in the fabrication of lasers. It is capable of withstanding 30 seconds of 60 watt direct laser energy. The low cure shrinkage (using a ..
Dielectric Strength 16.9 kV/mm
430 kV/in
Tra-Con Tra-Bond F109CLR Fiber Optic Epoxy Adhesive
TRA-BOND F109CLR is a clear, low viscosity epoxy specially designed for terminating plastic fibers. This blush free epoxy is an excellent choice for high humidity environments where absolute clarity..
Dielectric Strength 16.9 kV/mm
430 kV/in
Trelleborg Emerson & Cuming Stycast® 1269A Two-Component Easy Mix Ratio Encapsulant
Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, ..
Dielectric Strength 16.9 kV/mm

@Thickness 1.65 mm
428 kV/in

@Thickness 0.0650 in
3M RJS--1 3/C Phase Rejacketing System
3M RJS Series Rejacking Sleeves are dinged so that 3M Cold Shrink QTII and QTIII Silicone Rubber Termination applications can be used on 3/C (three conductor) medium voltage shielded power cables of..
Dielectric Strength 16.9 kV/mm

@Thickness 1.65 mm
428 kV/in

@Thickness 0.0650 in
3M RJS-3 3/C Phase Rejacketing System
3M RJS Series Rejacking Sleeves are dinged so that 3M Cold Shrink QTII and QTIII Silicone Rubber Termination applications can be used on 3/C (three conductor) medium voltage shielded power cables of..
Dielectric Strength 16.9 kV/mm

@Thickness 1.65 mm
428 kV/in

@Thickness 0.0650 in
3M RJS-5 3/C Phase Rejacketing System
3M RJS Series Rejacking Sleeves are dinged so that 3M Cold Shrink QTII and QTIII Silicone Rubber Termination applications can be used on 3/C (three conductor) medium voltage shielded power cables of..
Dielectric Strength 16.9 kV/mm
430 kV/in
Atom Adhesives AA-BOND F113 Epoxy Adhesive
AA-BOND F113 is an Optically Clear, low viscosity , High impact epoxy adhesives developed for bonding and small volume potting of plastic or glass optical fibers, lenses and prisms, LED displays, an..
Dielectric Strength 16.9 kV/mm
430 kV/in
Arlon-SQA-TMS-020
Arlon 31560R015 0.015" (0.381 mm) Uncured Silicone Rubber on Release Carrier
Design/Construction: Interleave: PolyethyleneProduct: Uncured Silicone Rubber Release Carrier: HDPE Carrier This data represents typical values for the production material. The data should not be us..
Dielectric Strength 16.9 kV/mm
429 kV/in
Short Time; ASTM D149
Plenco 51015 PET, Pellet, Injection Molded, White  (discontinued **)
PLENCO 51015 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL listed.Information supplied by..