| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | |
|
Plastcom SLOVAMID 6 GF 30 FRGG2 PA6, 30% glass fibre, flame retardant
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | STN IEC 60243 |
|
Plastcom SLOVAMID 66 GF 25 FRG 5 Polyamide 66, 25% Glass Fiber, Halogen Free Flame Retardant
FeaturesPA 66 for injection moulding, chemical reinforced with 25% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal..
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | |
|
Plastcom SLOVAMID 66 GF 25 FRI 2 PA66, 25% glass fibre, flame retardant
FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non..
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | STN IEC 60243 |
|
Plastcom SLOVAMID 66 GF 25 FRI 3 Polyamide 66, 25% Glass Fiber, Halogen Free Flame Retardant
FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-h..
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | |
|
Plastcom SLOVAMID 66 GF 25 FRI 3 TS PA66, 25% glass fibre, flame retardant
FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non..
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | STN EN 60243-2 |
|
Plastcom SLOVAMID® 6 GF 30 FRG 2 PA6 reinforced with glass fiber, flame retarded
PA 6 for injection molding, reinforced with 30 % glass fiber, flame retarded with halogen free flame retardant. Main features: flammability in accordance with UL 94 5 at 3.2 mm. Application for the ..
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | IEC 60243 |
|
Polimeri Europa Edistir N 1782 Polystyrene
General purpose polystyrene with good flow and high heat resistance. Suggested for direct gassing extrusion of heavy gage insulating boards (XPS) and in blend with high concentration of clear SBS f..
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | IEC 60243 |
|
Polimeri Europa Edistir N 1840 Polystyrene
General purpose polystyrene combining easy flow and medium heat. Edistir N 1840 is suggested in extrusion for glossy capping of HIPS sheets and for blending with HIPS or clear SBS for stiffer therm..
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | IEC 60243 |
|
Polimeri Europa Edistir N 2560 Polystyrene
High molecular weight general purpose polystyrene with good mechanical strength and good thermal resistance. It is recommended for in-line forming of disposable packaging, for sheet
extrusion in ble..
|
|||
| Dielectric Strength | 70.0 - 100 kV/mm | 1780 - 2540 kV/in | ISO.243 DN.53481 |
|
Polimersan Plastics POLIPA® (PA 6) Polyamide
POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc..
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | |
|
Polimeri Europa EDISTIR N1670 Polystyrene
(discontinued **)
Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,E,095-06 General purpose polystyrene with good flow and good heat resistance. Recommended for extrusion in blend with HIP..
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | |
|
Polimeri Europa EDISTIR N1671 Polystyrene
(discontinued **)
Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,095-06 General purpose polystyrene with good flow and good heat resistance for rapid set-up. To be used in injection mol..
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | ASTM D149 |
|
IPB Bicell® Cellular Polypropylene Sheet
Extruded, layered PP sheet, with a cellular core layer. Attributes include:Enhanced strength/thickness ratioOmni-directional flexural stresistanceHigh compression strengthWide variety of finishesRe..
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | DIN 53481 |
|
Schwartz Technical Plastics LAMIGAMID® 600 Polyoxymethylene
Application: friction bearings, wear and sliding linersInformation provided by Schwartz Technical Plastics GmbH
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | Estimated from similar grades. ASTM D149 |
|
Solvay Specialty Polymers Algoflon® F 5 Polytetrafluoroethylene (PTFE)
Algoflon® F 5 is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing. It is designed for filled grades and in particular is recommended for compounds with glass fiber ..
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | Estimated from similar grades. ASTM D149 |
|
Solvay Specialty Polymers Algoflon® F 5/S Polytetrafluoroethylene (PTFE)
Algoflon® F 5/S is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing powder. It is designed for compounds production and in particular it is recommended for use with..
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | IEC 60243 |
|
Borealis Borstar® HE 6068 Natural Bimodal HDPE with very low shrinkage for Submarine and Fiber Optical Cables
Borstar® HE6068 is a natural, UV-stabilized, colorable, bimodal high density (HD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar®..
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | VDE 0303/4 |
|
Polyram PA500 Nylon 6.6, Flame Retardant
Flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | IEC 60250 |
|
Polyram PlusTek PA320G3 Nylon 6.6 for Injection Molding, 15% Glass Fiber Reinforced, Flame Retardant
15% Glass fiber reinforced flame retardant Nylon 6.6 for injection molding applications.Information provided by Polyram.
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | VDE 0303/4 |
|
Polyram PlusTek PA320G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant
25% glass fiber reinforced, flame retardant and high stiffness polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | VDE 0303/4 |
|
Polyram PlusTek PA324G6 Nylon 6.6, UL-94 V-0 30% Glass Fiber
Self extinguishing (UL-94 V-0) 30% glass fiber reinforced polyamide 6.6 for component with high stiffness and dimensional stabilityInformation provided by Polyram Ram On Ind.
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | VDE 0303/4 |
|
Polyram PlusTek PA517 Nylon 6.6, Flame Retardant
Flame retardant halogen free polyamide 6.6 formulated to meet V-0, for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | ASTM D149 |
|
Zeon Chemicals Zeonor® 1060R Cyclo Olefin Polymer
Zeonor® is a line of thermoplastic polyolefin resin with an excellent combination of optical and electronic properties. These unique Cyclo Olefin Polymer (COP) was developed by Zeon Corporation usi..
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | ASTM D149, IEC 243 |
|
EPICHEM Epiryl PPO V0 Polyphenylene oxide
Characteristics: self-extinguishing V0 at 1,6 mm
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | ASTM D149, IEC 243 |
|
EPICHEM Epiryl G2 PPO 20GF Polyphenylene oxide, 20% Glass Fiber
Characteristics: 20% glass fibre filled
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | ASTM D149, IEC 243 |
|
EPICHEM PA 6 GF 30 Polyamide 6, 30% Glass
Characteristics: medium viscosity, 30% glass fibre filled
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | ASTM D149 |
|
Solvay Specialty Polymers Algoflon® F6 PTFE (Polytetrafluoroethylene)
(discontinued **)
Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope..
|
|||
| Dielectric Strength | 70.0 kV/mm | 1780 kV/in | VDE 0303/4 |
|
Polyram PlusTek RA320G3 Nylon 6.6, 15% Glass Fiber, Flame Retardant
15% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||