| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | ISO.243 DIN.53481 |
|
Omnia Plastica PTFE Polytetrafluoroethylene
A Fluoropolymer used mainly for its excellent chemical resistance. It has poor mechanical features. The strain, even under low weight, makes it very suitable as a gasket material.Features:Chemical: ..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
|
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data)
Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
|
Permabond HH190 Anaerobic Gasketmaker
Permabond® HH190 Gasketmaker is an anaerobic curing flange sealant that can replace, or be used as a dressing for, conventional pre-cut gaskets. Since HH190 is a flowable paste, it conforms to the ..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
|
Permabond HM129 Anaerobic Threadlocker
Permabond® HM129 is a high strength medium viscosity anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. Cure is fast and reliable on st..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
|
Permabond HM160 Anaerobic Retaining Compound
Permabond® HM160 is a medium viscosity liquid adhesive that cures when confined between metal parts to form a tough, hard plastic. In the uncured, liquid state, the adhesive wets the metal surfaces..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
|
Permabond LH197 Anaerobic Gasketmaker
Permabond® LH197 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is highly flexible, making it ideal for dissimilar surfaces where differential th..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
|
Permabond LM113 Anaerobic Threadlocker
Permabond® LM113 Threadlocker is a medium viscosity product for locking small threaded fasteners, such as screws and bolts or hydraulic fittings that might require disassembly. Due to its thixotrop..
|
|||
| Dielectric Strength |
11.0
kV/mm @Thickness 1.00 mm |
279
kV/in @Thickness 0.0394 in |
in oil; ASTM D149 |
|
SABIC Innovative Plastics LNP KONDUIT PX10322 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compound, with through-plane and in-plane thermal conductivity of 1.7 W/(m*K) and 4.7 W/(m*K) respectively, conforming to ASTM E 1461 test standard.
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
|
Permabond HH040 Pure NSF 61 Approved Anaerobic Retainer
Permabond® HH040 PURE is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure u..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | ASTM D149 |
|
Plenco 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **)
Plaslok 5000 is the replacement material for the former Union Carbide BMM-5000. It is a two-stage, woodflour-filled phenolic molding compound having versatile molding performance and preheating cha..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | 200°C for 1,000 hrs |
|
Fujipoly Industries Sarcon® 30Q Thin-Film QR
Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | 60°C for 500 hrs with 95% RH |
|
Fujipoly Industries Sarcon® 30Q Thin-Film QR
Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | Short-Term; ASTM D149 |
|
Glastic BMC SLC-1000 Glass-Reinforced Polyester
Data provided by Glastic Corporation.Medium strength, V-0, adjustable shrinkage.
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | Wet, short term. ASTM D149 |
|
Sumitomo Bakelite North America 1907-1 / 1907B-1 Glass Reinforced Hardware Grade Epoxy
Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc.
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | ASTM D149 |
|
Toyobo TS101 PPS, Glass Fiber/Mineral Reinforced
Key Feature: High dimensional stabilityHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | Short Time; ASTM D149 |
|
Plenco 4311 Phenolic, Granular, Injection Molded
PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | ASTM D149 |
|
Toyobo TS201 HS PPS, Glass Fiber/Mineral Reinforced
Key Feature: High stiffness, high toughnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excel..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | ASTM D149 |
|
Toyobo TS201 PPS, Glass Fiber/Mineral Reinforced
Key Feature: Standard high stiffness - used for metal replacementHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology devel..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
|
Dow Corning SE 4448 CV KIT PARTS A&B
Excellent thermal conductivity, low volatility (D4-D10 0.03% wt), heat cure, high viscosity.Information provided by Dow Corning
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
|
Dow Corning SLYGARD® 535 THIXOTROPIC DIELECTRIC GEL
Information provided by Dow Corning
|
|||
| Dielectric Strength |
11.0
kV/mm @Thickness 3.00 mm |
279
kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
|
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes
Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength. Retains electrical properties at high air humidity. High resistance to chemicals.Applications..
|
|||
| Dielectric Strength |
11.0
kV/mm @Thickness 3.00 mm |
279
kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
|
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Tubes
Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength, even at high temperatures. Retains electrical properties at high air humidity. High resistanc..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
|
Permabond A1042 Anaerobic Threadlocker
Permabond® A1042 is a rapid curing adhesive designed to lock and seal metal parts that subsequently may need to be dismantled for maintenance. The high vibration resistance makes Permabond A1042 pa..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
|
Permabond A113 Anaerobic Threadlocker
Designed for the locking and sealing of metal parts, Permabond® A113 is ideally suited for use on components that need to be dismantled for maintenance. Giving vibration resistance it can be used ..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
|
Permabond A126 Anaerobic Retainer
Permabond® A126 is a high-strength anaerobic adhesive for permanent assembly of coaxial assemblies or threaded metal components. The exceptionally low viscosity of this product makes it ideal for u..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
|
Permabond A130 Anaerobic Threadlocker
Designed for the locking and sealing of metal parts, Permabond® A130 is ideally suited for use on components that need to be dismantled for maintenance. Giving vibration resistance it can be used t..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
|
Permabond A131 Anaerobic Threadsealant
Permabond® A131 is an anaerobic adhesive designed to seal threaded metal pipe connections carrying a wide variety of gases and liquids, including potable water. Suitable for use on both parallel an..
|
|||
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
|
Permabond A136 Anaerobic Gasketmaker
Permabond® A136 is an anaerobic material designed for making 'formed in situ' gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets thereby offering potent..
|
|||