Polymer Property : Dielectric Strength = 32.0 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Dielectric Strength 32.0 kV/mm
813 kV/in
IEC 60112
RedEye On Demand ABS for Rapid Prototyping
ABS or Acrylonitrile butadiene styrene is a true industrial thermoplastic that is impact-resistant and structurally strong. ABS parts are built with a layered manufacturing process utilizing Fused D..
Dielectric Strength 32.0 kV/mm
813 kV/in
IEC 60243
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY
Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Dielectric Strength 32.0 kV/mm
813 kV/in
IEC 60243
Solvay TECHNYL® A 238 Black 21 N PA66, DRY
Description: Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 238 offers excellent ..
Dielectric Strength 32.0 kV/mm
813 kV/in
IEC 60243
Solvay TECHNYL® B 238 Black 21 N PA66/6, DRY
Description: Unreinforced and modified copolyamide 66/6, heat stabilized, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 238 is particular..
Dielectric Strength 32.0 kV/mm
813 kV/in
IEC 60112
Stratasys® ABS
ABS is a strong, durable production-grade thermoplastic used across many industries. ABS is an ideal material for conceptual prototyping through design verification through direct digital manufactur..
Dielectric Strength 32.0 kV/mm
813 kV/in
IEC 60243-1
Vyncolit A2990 Glass Fiber Reinforced Novolac Phenolic
Resole resin based, glass fiber reinforced. Good mechanical properties, combined with superior electrical insulation properties. Among others used for commutator applicationsInformation provided by ..
Dielectric Strength 32.0 kV/mm
813 kV/in
Covestro Makrolon® 3158 Polycarbonate
Key Features:Release agentUnfilledSuitable processing methods:Injection moldingExtrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated..
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® L 16 nat PA12
Low viscosity unmodified polyamide 12Information provided by EMS Grivory
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® L 16 W 20 black 9995 PA12
Product Description: Grilamid L 16 W 20 is a semi-flexible low viscosity, heat stabilized PA12 injection molding grade. The main characteristics of this product are: Easy flowing?High impact streng..
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® L 20 G grey 9280 PA12
Product Description: Grilamid L 20 G grey 9280 is a medium viscosity, unreinforced, heat stabilized polyamide 12 for injection molding and cable sheathing. The main features of this product are: Low..
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® L 20 G HL PA12
Product Description: Grilamid L 20 GHL is a, medium viscosity injection molding grade, based on Polyamide 12 (PA12). Grilamid L 20 GHL is UV-stabilized, and heat stabilized The special features of G..
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® L 20 nat PA12
Medium viscosity unmodified Polyamide 12Information provided by EMS Grivory
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® L 20 W 20 grey 9280 PA12
Product Description: Grilamid L 20 W 20 grey 9280 is a semiflexible plasticized medium viscosity polyamide 12 (PA12) extrusion grade. Grilamid L 20 W 20 grey 9280 is heat stabilized. The main featur..
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® L 25 nat 6112 PA12
Product Description: Grilamid L 25 natural 6112 is a high viscous, Polyamide 12 extrusion grade. Grilamid L 25 natural 6112 fulfils the requirements of DIN 73378, Type PA 12-H. Application examples:..
Dielectric Strength 32.0 kV/mm
813 kV/in
AC Rapid Rise; ASTM D149
DuPont™ Nomex® 410 Paper, 12 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® XE 3926 black 9992 PA12
Product description: Grilamid XE 3926 black 9992 is a low viscosity extrusion type, based on Polyamide 12 (PA 12). The special features of Grilamid XE 3926 black 9992 are: Very good chemical resista..
Dielectric Strength 32.0 kV/mm
813 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® XE 4095 black 9225 PA*-GF50
Product description: Grivory XE 4095 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia..
Dielectric Strength 32.0 kV/mm
813 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® XE 4164 black 9225 PA*-GF30
Product description: Grivory XE 4164 black 9225 is a 30% glass fiber reinforced engineering thermoplastic material based on a semicrystalline, partially aromatic copolyamide. ISO polymer designation..
Dielectric Strength 32.0 kV/mm
813 kV/in
IEC 60243-1
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)  (Unverified Data**)
45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du..
Dielectric Strength 32.0 kV/mm
813 kV/in
IEC 60243-1
DuPont Performance Polymers Rynite® 530 BK503 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Polyethylene Terephthalate Rynite 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength stiffness and toughness excellent ..
Dielectric Strength 32.0 kV/mm
813 kV/in
IEC 60243-1
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good ..
Dielectric Strength 32.0 kV/mm
813 kV/in
IEC 60243-1
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)
Unreinforced Renewably Sourced Polytrimethylene Terephthalate with Excellent Impact Resistance Sorona MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably..
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® BGZ-30 PA6-GF30
Product description: Grilon BGZ-30 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 30% glass fibers. Grilon BGZ-30 has the following important properties:..
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® L 25 LM PA12
Product Description: Grilamid L 25 LM is a heat and UV stabilized nylon 12 grade for tube extrusion. According to DIN 73378 Grilamid L 25 LM corresponds to the type PA 12 HL. Grilamid L 25 LM fulfil..
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® L 25 W 10 H X PA12
Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized..
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® L 25 W 40 HL X PA12-I
Product Description: Grilamid L 25 W 40 HLX is a flexible Polyamide 12 grade with an excellent cold impact strength and heat stability. Grilamid L 25 W 40 HLX is specially suitable for flexible tube..
Dielectric Strength 32.0 kV/mm
813 kV/in
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro..
Dielectric Strength 32.0 kV/mm
813 kV/in
IEC 243-1
Azoty Tarnow™ Tarnamid® T-27 GF15 Polyamide 6 - Glass Fiber Reinforced
15% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
Dielectric Strength 32.0 kV/mm
813 kV/in
IEC 243-1
Azoty Tarnow™ Tarnamid® T-27 GF25 Polyamide 6 - Glass Fiber Reinforced
25% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
Dielectric Strength 32.0 kV/mm
813 kV/in
CEI 60243-1
Addiplast Addinyl C2 ZV15 Nylon 66/6, 15% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.