| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 13.0 - 19.0 kV/mm | 330 - 483 kV/in | ASTM D149 |
|
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | ASTM D149 |
|
Premix Premi-Ject® 1102H Fiberglass Reinforced Thermoset BMC
Premi-Ject® 1102H is a fiberglass reinforced thermoset bulk molding compound for coil encapsulation applications.Key features and benefits are:Designed with unique flow properties to encapsulate co..
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | ASTM D149 |
|
Chevron Phillips Ryton® R10 5002C PPS Polyphenylene Sulfide
(discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
|
|||
| Dielectric Strength | 13.0 - 120 kV/mm | 330 - 3050 kV/in | Average value: 25.5 kV/mm Grade Count:20 |
|
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
|
|||
| Dielectric Strength | 13.0 - 70.0 kV/mm | 330 - 1780 kV/in | Average value: 26.1 kV/mm Grade Count:52 |
|
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | ASTM D149 |
|
Plenco 5440 Black General Purpose Phenolic Molding Compound
(discontinued **)
Plaslok 5440 is the replacement material for the former Union Carbide BMRS-5440. It is a two-stage, phenolic molding compound that has been successfully formulated to accommodate a very wide range ..
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | 200°C for 1,000 hrs |
|
Fujipoly Industries Sarcon® 45Q Thin-Film QR
Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov..
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | 200°C for 1,000 hrs |
|
Fujipoly Industries Sarcon® 45U Thin-Film UR
Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov..
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | 150°C for 1,000 hrs; JIS-K-6249 |
|
Fujipoly Industries Sarcon® GR-Fd Gap Filler Pad
Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Fd has a mesh embedded overall.Information provided b..
|
|||
| Dielectric Strength |
13.0
kV/mm <br>@Thickness 3.00 mm
|
330
kV/in <br>@Thickness 0.118 in
|
ASTM D149 |
|
Teknor Apex Beetle® MD21 Nylon 6, Extrusion Grade
Notes: MD21 is a medium viscosity grade of nylon 6, designed for wire coating extrusion. MD21 is heavily pigment and is designed to provide good opacity even with thin coatings. It also features a..
|
|||
| Dielectric Strength |
13.0
kV/mm <br>@Thickness 3.00 mm
|
330
kV/in <br>@Thickness 0.118 in
|
IEC 243 |
|
Sumitomo Bakelite North America RX® 611 Fiberglass Reinforced Phenolic
RXÂ 611 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type MFH.Information supplied by Sumitomo..
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | |
|
Elastomer Engineering Elastamide 100 Elastomer Modified RIM Nylon 6
30% crystallinity. Information supplied by Elastomer Engineering.
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | |
|
Elastomer Engineering Elastamide 150 Elastomer Modified RIM Nylon 6
29% crystallinity. Information supplied by Elastomer Engineering.
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | |
|
Elastomer Engineering Elastamide 200 Elastomer Modified RIM Nylon 6
26% crystallinity. Information supplied by Elastomer Engineering.
|
|||
| Dielectric Strength |
13.0
kV/mm <br>@Thickness 2.00 mm
|
330
kV/in <br>@Thickness 0.0787 in
|
ASTM D149 |
|
Toyobo T-661 Nylon 66, Standard Grade (Conditioned)
Features: Non-reinforced, Standard GradeInformation provided by Toyobo.
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | ASTM D149-95a |
|
Thermoseal KLINGERSIL® C-4324 Compressed Inorganic Fiber Gasketing
Recycled Fiberglass & Aramid BlendNitrile BinderLow Pressure Steam, Water & GasesGood for Oils and FuelsInformation provided by Thermoseal Inc.
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | Short Time; ASTM D149 |
|
Plenco 2571 Phenolic, Granular, Injection Molded
PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde..
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | Wet, Step by Step |
|
Cosmic Plastics E4905 Mineral Filled Epoxy Molding Compound, Encapsulated Grade
Data provided by the manufacturer.
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | DIN 53481 |
|
DSM Fibre Intermediates Nyrim® 1500 (Conditioned)
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | DIN 53481 |
|
DSM Fibre Intermediates Nyrim® 2000 (Conditioned)
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | DIN 53481 |
|
DSM Fibre Intermediates Nyrim® 3000 (Conditioned)
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | DIN 53481 |
|
Brueggemann Chemical Nyrim® 1000 (Conditioned)
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..
|
|||
| Dielectric Strength |
13.0
kV/mm <br>@Thickness 1.00 mm
|
330
kV/in <br>@Thickness 0.0394 in
|
IEC 60243 |
|
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri..
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | Short Time |
|
Bulk Molding Compounds BMC 600 Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 600 molding compound is a mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a general purpose material with medium ..
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | Short Time |
|
Bulk Molding Compounds BMC 2274 Mineral Filled, Glass Reinforced Polyester
BMC 2274 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression transfer and stuffer injection molding. It is a general-purpose material with medium..
|
|||
| Dielectric Strength |
13.0
kV/mm <br>@Thickness 2.00 mm
|
330
kV/in <br>@Thickness 0.0787 in
|
IEC 243-1 |
|
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **)
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | Wet, Step by Step |
|
Cosmic Plastics 6120 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | Wet, Step by Step |
|
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
|
|||