Polymer Property : Dielectric Strength = 340 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Dielectric Strength 13.4 kV/mm
340 kV/in
Short Time; Dry; ASTM D149
Resinoid 1340 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Dielectric Strength 13.4 - 138 kV/mm
340 - 3500 kV/in
Average value: 37.9 kV/mm Grade Count:51
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..
Dielectric Strength 13.4 - 16.0 kV/mm
340 - 406 kV/in
Average value: 14.9 kV/mm Grade Count:10
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report..
Dielectric Strength 13.4 kV/mm
340 kV/in
Short Time; ASTM D149
Rostone Rosite® 3950ES SMC Thermoset Polyester, 25% Glass Reinforced  (discontinued **)
Key Features: High Strength; High DielectricElectrical grade material that provides higher flexural and impact strength than Rosite 3550 composites with comparable glass fiber content. 3950ES is fo..
Dielectric Strength 13.4 kV/mm
340 kV/in
ASTM D149
Plenco 304 Black Impact Grade Woodflour/Cellulose Filled Phenolic Molding Compound  (discontinued **)
Plaslok 304 is a two-stage, woodflour and cellulose-filled phenolic molding compound having improved impact strength. It is suitable for automatic molding, and is recommended for thin-walled parts ..
Dielectric Strength 13.4 kV/mm
340 kV/in
ASTM D149
IDI Composites E-206 Thermoset Polyester, Sheet
ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista..
Dielectric Strength 13.4 kV/mm
340 kV/in
ASTM D149
IDI Composites M-207 Thermoset Polyester, Sheet
MECHANICAL - Versatile family of compounds designed to meet a variety of mechanical, electro-mechanical, and corrosion applications. Outstanding structural properties at lowest possible costs.Data p..
Dielectric Strength 13.4 kV/mm
340 kV/in
ASTM D149
ITW Devcon Flexane® Rubber Repair / Castable Urethane Brushable, Black
Information provided by ITW Devcon
Dielectric Strength 13.4 kV/mm
340 kV/in
60Hz, Step-by-Step, wet; ASTM D149
Sumitomo Bakelite North America RX® 3-1-530-P Long-Glass Reinforced Diallyl Phthalate
Long glass fiber reinforced, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type GDI-30F.Information provided by Vyncolit, a Sumitomo Bak Group
Dielectric Strength 13.4 kV/mm
340 kV/in
ASTM D149
Plastics Group Polifil® 89MRGFHS Glass Fiber and Mineral Reinforced Nylon 6 (DAM)
Polifil® GFN/MRN 6 reinforced series of compounds provide good heat and dimensional stability and offer extended or continuous stability under high temperatures. These have been found useful in ind..
Dielectric Strength 13.4 kV/mm
340 kV/in
ASTM D149
Devcon Combo Wear FC Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Dielectric Strength 13.4 kV/mm
340 kV/in
ASTM D149
Devcon Wear Guard (Fine Load) Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Dielectric Strength 13.4 kV/mm

@Thickness 0.0508 mm
340 kV/in

@Thickness 0.00200 in
500 vac, rms. [60 Hz]/sec; ASTM D149-92
3M 9458 Adhesive Transfer Tapes with Adhesive 300
3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f..
Dielectric Strength 13.4 kV/mm

@Thickness 0.0508 mm
340 kV/in

@Thickness 0.00200 in
500 vac, rms. [60 Hz]/sec; ASTM D149-92
3M 9471 Adhesive Transfer Tapes with Adhesive 300
3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f..
Dielectric Strength 13.4 kV/mm

@Thickness 0.0508 mm
340 kV/in

@Thickness 0.00200 in
500 vac, rms. [60 Hz]/sec; ASTM D149-92
3M 9472 Adhesive Transfer Tapes with Adhesive 300
3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f..
Dielectric Strength 13.4 kV/mm

@Thickness 0.0508 mm
340 kV/in

@Thickness 0.00200 in
500 vac, rms. [60 Hz]/sec; ASTM D149-92
3M 9671 Adhesive Transfer Tapes with Adhesive 300
3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f..
Dielectric Strength 13.4 kV/mm

@Thickness 0.0508 mm
340 kV/in

@Thickness 0.00200 in
500 vac, rms. [60 Hz]/sec; ASTM D149-92
3M 9672 Adhesive Transfer Tapes with Adhesive 300
3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f..
Dielectric Strength 13.4 kV/mm

@Thickness 0.0508 mm
340 kV/in

@Thickness 0.00200 in
500 vac, rms. [60 Hz]/sec; ASTM D149-92
3M 9673 Adhesive Transfer Tapes with Adhesive 300
3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f..
Dielectric Strength 13.4 kV/mm

@Thickness 0.0508 mm
340 kV/in

@Thickness 0.00200 in
500 vac, rms. [60 Hz]/sec; ASTM D149-92
3M 9674 Adhesive Transfer Tapes with Adhesive 300
3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f..
Dielectric Strength 13.4 kV/mm
340 kV/in
ASTM D149
Arlon LW401R##-P0 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length i..
Dielectric Strength 13.4 kV/mm
340 kV/in
ASTM D149
Arlon LW401R##-P1 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length i..
Dielectric Strength 13.4 kV/mm
340 kV/in
ASTM D149
Arlon LW401R##-P2 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length i..
Dielectric Strength 13.4 - 14.2 kV/mm
340 - 360 kV/in
Step by Step
Bulk Molding Compounds BMC 102 Glass Filled Thermoset Polyester
BMC 102 is a medium strength, glass fiber reinforced molding compound that meets Ford Specification ESF-M3D56-A. It can be supplied in bulk or extruded in pre-weighed slugs and is well suited for in..
Dielectric Strength 13.4 kV/mm
340 kV/in
Short Time
Bulk Molding Compounds BMC 5436 Mineral Filled, Glass Reinforced Polyester
BMC 5436 molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda..
Dielectric Strength 13.4 kV/mm
340 kV/in
Short Time
Bulk Molding Compounds BMC 604 Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 604 molding compound is a low-cost, mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose material wit..
Dielectric Strength 13.4 - 15.0 kV/mm
340 - 380 kV/in
short time
Bulk Molding Compounds BMC 6241 Glass Reinforced BMC
BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availab..
Dielectric Strength 13.4 kV/mm
340 kV/in
ASTM D149
Ashley Polymers Ashlene® 78MGS Nylon 6, 40% Glass Mineral reinforced
A 40% glass mineral reinforced Nylon 6 with good dimensional stability, stiffness, sink and warp resistance.Data provided by the manufacturer
Dielectric Strength 13.4 kV/mm
340 kV/in
ASTM D149
Devcon Wear Guard (High Load) Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Dielectric Strength 13.4 kV/mm
340 kV/in
ASTM D149
Plaslok 304 Black Impact Grade Woodflour/Cellulose Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 304 is a two-stage, woodflour and cel..