| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
|
Plastcom SLOVAMID 66 GF 13 TS PA66, 13% glass fibre
FeaturesChemically reinforced with 13% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W..
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
|
Plastcom SLOVAMID 66 GF 35 HTS PA66, 355% glass fibre, combined stability
FeaturesPA 66 for injection moulding, chemically reinforced with 35% glass fibre, heat stabilized and stabilized against hydrolysis. Used for cooling water systems in the automotive industry. Delive..
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
|
Kazanorgsintez 102-16 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
|
Kazanorgsintez 107-20 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
|
Kazanorgsintez 153-23 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
|
|||
| Dielectric Strength | >= 40.0 kV/mm | >= 1020 kV/in | Sample of 1 mm thickness, Alternating current |
|
Kazanorgsintez 158-281 Low Density Polyethylene Composition with Improved Processibility
Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
|
Misumi Machinable SiO2-MgO Ceramic
Information provided by MISUMI Corporation.
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
|
Styrolution Terluran® HI-10 ABS
Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
|
Styrolution Terblend® N NG-02 8% Glass Filled ABS/PA6 (Dry)
Terblend N NG-02 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, high impact strength and good surface appearance.Information provided by STYROLUTION, which is a join..
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | ASTM D149 |
|
Zeon Chemicals Zeonex® 690R Cyclo-Olefin Polymer |
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | dry; IEC 60243-1 |
|
DSM EcoPaXX® Q-PG6 PA410-I-GF30
% Glass Reinforced, Impact Modified
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | dry; IEC 60243-1 |
|
EMS-Grivory Grivory® BG-30 S FA PA6-GF30
Product description: Grilon BG-30 S FA is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S FA has the following important properties: Excellent surface finishEasy ..
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 243-1 |
|
CP-Polymer-Technik Wellamid® 6000 GVZ 45 HWCP 45% Glass Fiber Nylon 6, Impact Resistant, Good Surface Finish, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 243-1 |
|
CP-Polymer-Technik Wellamid® 6000 MF 30 HWCP 30% Milled Glass Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 243-1 |
|
CP-Polymer-Technik Wellamid® 6000/58 GV 15 HWUVCP 15% Glass Fiber Nylon 6, Impact Modified Until -40°C, UV Stabilized, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | dry; IEC 60243-1 |
|
EMS-Grivory Grivory® XE 5052 (BGZ-15 FC) PA6-GF15
Product description: Grilon XE 5052 is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber: High impact resistanceGood surface qualityShort cycle timeGood flowabilit..
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | No thickness given |
|
ConocoPhillips Hydroclear® 100 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
|
Accuratus MACOR Machinable Glass Ceramic
Macor is cast as a two phase glass. After casting, it is heat treated causing crystallization of one phase giving rise to its glass-like and ceramic-like characteristics.Key Properties of MACOR: Mac..
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | ASTM D149 |
|
Braskem GD5150K HDPE High Density Extrusion Polyethylene
GD5150K is a high-density polyethylene specially developed for the manufacturing of insulation for wires and cables demanding high extrusion velocity. It has medium molar mass, shows good dielectric..
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
|
Arkema Group Rilsan® AECV T8L Nylon 12, Cable Sheathing Grade (Conditioned)
Designation ISO 1874-PA12,KHL,16-010Extrusion grade for the sheathing of wires and cables. Available colors: black, blue, orange and white. Reinforced light and heat stabilizing agents. Anti-termite..
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 243/1 |
|
BASF Ultradur B 2550 PBT
Ultradur B2550 is an unfilled, very free-flowing grade for coating paper and board with high heat resistance, for example for packaging of frozen goods and ready-prepared meals. Also suitable for in..
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
|
BASF Ultraform N 2320 003 UNC Q600 POM
Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent.
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
|
BASF Ultraform® E 3120 BM POM
Description: Is a POM, high-molecular grade for extrusion blow molding of hollow parts.Information provided by BASF
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
|
BASF Ultraform® N2520 L POM
Description: Is a POM, product having reduced electric surface resistance.Information provided by BASF
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
|
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry)
Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla..
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 243/1 |
|
BASF Ultradur® B 4406 G6 30% Glass Filled PBT
Description: Is a PBT, flame-retardant injection-molding grades, with 30% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh..
|
|||
| Dielectric Strength | 40.0 kV/mm | 1020 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® LBV-50H FWA nat PA12-GF50
Product Description: Grilamid LBV-50H FWA natural is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w..
|
|||