Electrical Properties Metric English Comments
Dielectric Strength 19.0 kV/mm

@Thickness 2.00 mm
483 kV/in

@Thickness 0.0787 in
ASTM D149
Nilit Nilitop BT FR C3 Unfilled, Flame Retardant PBT
Description: Nilitop BT FR C3 is an unfilled, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive.Key characteristics: Go..
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA.
Dielectric Strength 19.0 kV/mm

@Thickness 2.00 mm
483 kV/in

@Thickness 0.0787 in
IEC 243-1
LATI LARPEEK 10 G/30 30% Glass Reinforced Polyetheretherketone (PEEK)  (Unverified Data**)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East)
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA.
Dielectric Strength 19.0 - 43.0 kV/mm
483 - 1090 kV/in
Average value: 25.5 kV/mm Grade Count:8
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
Dielectric Strength 19.0 kV/mm

@Thickness 2.00 mm
483 kV/in

@Thickness 0.0787 in
IEC 243-1
LATI LATAN 3E71 Polyoxymethylene Copolymer (POM) with Elastomer  (Unverified Data**)
Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea..
Dielectric Strength 19.0 kV/mm
483 kV/in
ASTM D149
Gharda Chemicals Gafone S S1430SP60 Polysulfone (PS)  (discontinued **)
Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Elec..
Dielectric Strength 19.0 kV/mm
483 kV/in
ASTM D149
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU)  (Unverified Data**)
Udel GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resista..
Dielectric Strength 19.0 - 35.0 kV/mm
483 - 889 kV/in
Average value: 26.6 kV/mm Grade Count:12
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Dielectric Strength 19.0 kV/mm
483 kV/in
ASTM D149
Kingfa JH710 G10D Flame Retardant & 10% Glass Fiber Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:Exact mechanism partsElectrical and elect..
Dielectric Strength 19.0 kV/mm
483 kV/in
JIS-K-6249; ASTM D-149
Fujipoly Industries Sarcon® GR-Hm Gap Filler Pad
Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and ..
Dielectric Strength 19.0 kV/mm
483 kV/in
ASTM D149
Kolon KOCETAL® K200 Standard Grade Acetal Resin
Suitable for both injection and extrusion.Applications: Injection and extruded use such as rod and sheetInformation provided by API Kolon.
Dielectric Strength 19.0 kV/mm
483 kV/in
ASTM D149
Kolon KOCETAL® K500 Standard Grade Acetal Resin
General injection molding grade. Easy flow grade for hard-to fill molds and mechanical thin-wall parts.Applications: General injection molding products.Information provided by API-Kolon.
Dielectric Strength 19.0 kV/mm
483 kV/in
ASTM D149
Kolon Kocetal® K700 General Purpose Grade Acetal Copolymer
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Dielectric Strength 19.0 kV/mm
483 kV/in
ASTM D149
Kolon KOPET® KP133G15BL G/F Reinforced Polyester Compound Resin (PET)
Dimensionally stable, high elastic, high flowApplications: Ink CartridgeInformation provided by API-Kolon.
Dielectric Strength 19.0 kV/mm
483 kV/in
ASTM D149
KEP Kepital® F10 Standard Grade/High Viscosity Acetal Homopolymer
Extrusion: electrical parts, machine/mechanical parts, industrial parts, automotive parts, applications, electronic data processing parts, thick-walledKepital® is a registered trademark of Korea ..
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
ASTM D149
Solvay Specialty Polymers Acudel® 22000 Polyphenylsulfone, Modified (PPSU, Modified)
Acudel® 22000 is a modified polyphenylsulfone. It is a high-heat, high-performance resin formulation exhibiting very good hydrolytic stability, excellent resistance to acids and bases and good re..
Dielectric Strength 19.0 kV/mm
483 kV/in
IEC 60243-1
Polyplastics Tepcon M450 Acetal-copolymer (POM), Super High Fluidity, High Cycle
Information provided by PolyPlastics.
Dielectric Strength 19.0 kV/mm
483 kV/in
IEC 60243-1
Vyncolit BXE7665 Glass Filled Phenolic Molding Compound
Novolac resin based, mainly glass fiber filled. Excellent electrical properties combined with very good mechanical properties. Grade especially suitable for electrical applications.Information pro..
Dielectric Strength 19.0 kV/mm
483 kV/in
AC rapid rise in air; ASTM D149
DuPont™ Nomex® Type 993, 160 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ..
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
Short time; ASTM D149
Daikin POLYFLON M-139 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding and automatic compression molding.Features: Excellent fluidity. Apparent density is large and ideal for automated compression molding proces..
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
Short time; ASTM D149
Daikin POLYFLON MG-1431F PTFE 20% Glass Fiber and 5% MoS2 Filled Molding Powder, High Apparent Density, Free Flow
15% glass fiber and 5% MoS2 filled. High apparent density and free-flowing properties. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanica..
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
Eurostar Staramide AG10 PA66, 50% Glass Filled, Injection Molded
AG10 is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
Eurostar Staramide AG7K PA66, 35% Glass Filled, Injection Molded
AG7 is a Heat and Hydrolytically Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
Eurostar Staramide AG7 PA66, 35% Glass Filled, Injection Molded
AG7 is a 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Dielectric Strength 19.0 kV/mm
483 kV/in
Insulating Strength
China-Yixing Longly Refractories 99 Alumina Ceramic Tubes & Rods
LONGLY's alumina ceramic tubes and rods (the tolerances of +/- 0.02mm could be reached by mechanical or electronic finishing or mirror surface finishing) have high hardness, wear resistance, insulat..
Dielectric Strength 19.0 kV/mm

@Thickness 2.00 mm
483 kV/in

@Thickness 0.0787 in
IEC 243-1
LATI LARTON G/30 30% Glass Fiber Filled Polyphenylene sulfide (PPS)  (discontinued **)
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..
Dielectric Strength 19.0 kV/mm
483 kV/in
ASTM D149
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA)  (Unverified Data**)
Amodel HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a broad..
Dielectric Strength 19.0 kV/mm
483 kV/in
IEC 60243-1
Polyplastics Duracon® HP270X Acetal Co-polymer (POM), High stiffness, High flow
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Copyright © lookpolymers.com All Rights Reserved