| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 30.0 - 50.0 kV/mm | 762 - 1270 kV/in | ASTM D149 |
|
Permabond TA4202 Toughened Acrylic Adhesive
PERMABOND® TA4202 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni..
|
|||
| Dielectric Strength | 30.0 - 50.0 kV/mm | 762 - 1270 kV/in | ASTM D149 |
|
Permabond TA430 Acrylic Adhesive & Initiator
PERMABOND TA430 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics, wood, and some thermoplastics. This adhesive may be used in a variety of structural bondin..
|
|||
| Dielectric Strength | 30.0 - 50.0 kV/mm | 762 - 1270 kV/in | ASTM D149 |
|
Permabond TA4300 Toughened Acrylic Adhesive
PERMABOND® TA4300 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue...
|
|||
| Dielectric Strength | 30.0 - 50.0 kV/mm | 762 - 1270 kV/in | ASTM D149 |
|
Permabond TA4310 Toughened Acrylic Adhesive
PERMABOND® TA4310 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue...
|
|||
| Dielectric Strength | 30.0 - 50.0 kV/mm | 762 - 1270 kV/in | ASTM D149 |
|
Permabond TA435 Toughened Acrylic Adhesive & Initiator
PERMABOND TA435 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This adhesive may be used in a variety of structural bonding appli..
|
|||
| Dielectric Strength | 30.0 - 50.0 kV/mm | 762 - 1270 kV/in | ASTM D149 |
|
Permabond TA436 Toughened Acrylic Adhesive
PERMABOND TA436 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. Permabond TA436 is a no-mix system which obtains handling strength..
|
|||
| Dielectric Strength | 30.0 - 50.0 kV/mm | 762 - 1270 kV/in | ASTM D149 |
|
Permabond TA437 Toughened Acrylic Adhesive
PERMABOND TA437 is a single component structural acrylic adhesive designed primarily for bonding metals, ferrites and ceramics. The typical fixture time of TA437 when used with Initiator 41 is 30 –..
|
|||
| Dielectric Strength | 30.0 - 50.0 kV/mm | 762 - 1270 kV/in | ASTM D149 |
|
Permabond TA439 Toughened Acrylic Adhesive
Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f..
|
|||
| Dielectric Strength | 30.0 - 50.0 kV/mm | 762 - 1270 kV/in | ASTM D149 |
|
Permabond TA440 Toughened Acrylic Adhesive
PERMABOND TA440 is a two component structural acrylic adhesive suitable for bonding metals, glass, wood, ferrites, ceramics and some rigid plastics. This adhesive may be used in a variety of structu..
|
|||
| Dielectric Strength | 30.0 - 50.0 kV/mm | 762 - 1270 kV/in | ASTM D149 |
|
Permabond TA4810 Toughened Acrylic Adhesive
PERMABOND TA4810 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites. TA4810 has excellent adhesion to as received metal surfac..
|
|||
| Dielectric Strength | 30.0 - 50.0 kV/mm | 762 - 1270 kV/in | ASTM D149 |
|
Permabond TA4820 Structural Acrylic Adhesive
PERMABOND TA4820 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites. TA4820 has excellent adhesion to as received metal surfac..
|
|||
| Dielectric Strength | 24.0 - 50.0 kV/mm | 610 - 1270 kV/in | Average value: 29.9 kV/mm Grade Count:57 |
|
Overview of materials for Styrenic Elastomer (TES)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro..
|
|||
| Dielectric Strength | 18.9 - 50.0 kV/mm | 480 - 1270 kV/in | Average value: 25.2 kV/mm Grade Count:13 |
|
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
|
|||
| Dielectric Strength | 19.0 - 50.0 kV/mm | 483 - 1270 kV/in | Average value: 30.8 kV/mm Grade Count:13 |
|
Overview of materials for Polyphenylene Ether, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap..
|
|||
| Dielectric Strength | 18.0 - 50.0 kV/mm | 457 - 1270 kV/in | Average value: 33.2 kV/mm Grade Count:16 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
|
|||
| Dielectric Strength | 30.0 - 50.0 kV/mm | 762 - 1270 kV/in | ASTM D149 |
|
Permabond TA4246 Toughened Acrylic Adhesive
PERMABOND® TA4246 is a 2-part, no-mix, room temperature curing structural adhesive. It is ideal for use on a wide variety of substrate materials and forms a very high strength structural bond with ..
|
|||
| Dielectric Strength | 30.0 - 50.0 kV/mm | 762 - 1270 kV/in | ASTM D149 |
|
Permabond TA4302 Toughened Acrylic Adhesive
PERMABOND® TA4302 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni..
|
|||
| Dielectric Strength | 18.0 - 50.0 kV/mm | 457 - 1270 kV/in | Average value: 32.0 kV/mm Grade Count:4 |
|
Overview of materials for PVC, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW..
|
|||
| Dielectric Strength | 20.0 - 50.0 kV/mm | 508 - 1270 kV/in | Average value: 34.2 kV/mm Grade Count:3 |
|
Overview of materials for PVC, Uncompounded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate ..
|
|||
| Dielectric Strength | 7.00 - 50.0 kV/mm | 178 - 1270 kV/in | Average value: 29.0 kV/mm Grade Count:6 |
|
Overview of materials for Nylon 12, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr..
|
|||
| Dielectric Strength | 24.0 - 50.0 kV/mm | 610 - 1270 kV/in | Average value: 34.7 kV/mm Grade Count:21 |
|
Overview of materials for Nylon 12, Extrusion/Tubing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values ..
|
|||
| Dielectric Strength | 35.0 - 50.0 kV/mm | 889 - 1270 kV/in | DIN 53481 |
|
Isoflon PVC Polyvinyl Chloride
Good mechanical propertiesThermoformableGood impact resistanceInformation provided by Isoflon.
|
|||
| Dielectric Strength | 18.0 - 50.0 kV/mm | 457 - 1270 kV/in | DIN 53481 |
|
Isoflon PVDF Polyvinylidene fluoride
Electrical and thermal insulating products with food slipping propertiesChemically inertInformation provided by Isoflon.
|
|||
| Dielectric Strength | 15.0 - 50.0 kV/mm | 381 - 1270 kV/in | |
|
Goodfellow Ruby, Al2O3
Ruby exhibits identical properties to those of sapphire. Small amounts of impurities, especially chromium oxide, give ruby a red coloration. Useful optical range from 150 - 5500 nm.Information pro..
|
|||
| Dielectric Strength | 20.0 - 50.0 kV/mm | 508 - 1270 kV/in | ASTM D149 |
|
Adamas Adalon® 401 PTFE, 10% Polyimide
Information provided by Adamas, HPM
|
|||
| Dielectric Strength | 20.0 - 50.0 kV/mm | 508 - 1270 kV/in | ASTM D149 |
|
Adamas Adalon® 403 PTFE, 15% Polyimide
Information provided by Adamas, HPM
|
|||
| Dielectric Strength | 20.0 - 50.0 kV/mm | 508 - 1270 kV/in | ASTM D149 |
|
Adamas Adalon® 410 PTFE+ PEEK
Information provided by Adamas, HPM
|
|||
| Dielectric Strength |
30.0
-
50.0
kV/mm @Thickness 1.00 mm |
762
-
1270
kV/in @Thickness 0.0394 in |
bulk |
|
Goodfellow Cellophane, Rayophane Regenerated Cellulose Fiber
All forms of cellulose degrade before they melt but natural cellulose can be regenerated by the xanthate process to manufacture fibres, commonly called rayon or viscose, and film, commonly called by..
|
|||
| Dielectric Strength |
30.0
-
50.0
kV/mm @Thickness 1.00 mm |
762
-
1270
kV/in @Thickness 0.0394 in |
|
|
Goodfellow Cellophane, Rayophane Regenerated Cellulose Film
All forms of cellulose degrade before they melt but natural cellulose can be regenerated by the xanthate process to manufacture fibres, commonly called rayon or viscose, and film, commonly called by..
|
|||
| Dielectric Strength | 15.0 - 50.0 kV/mm | 381 - 1270 kV/in | Average value: 28.9 kV/mm Grade Count:12 |
|
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..
|
|||