| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength |
>=
19.7
kV/mm <br>@Thickness 0.510 mm
|
>=
500
kV/in <br>@Thickness 0.0201 in
|
Z Direction; IPC-TM-650 2.5.6.2 |
|
Rogers Corporation RO4533 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate
The RO4500™ Series Cost Performance Antenna Grade Laminates are ceramic-filled, glass-reinforced hydrocarbon based materials that provides the controlled dielectric constant, low loss performance a..
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | ASTM D149 |
|
Owens Corning Glass Fiber Reinforced Nylon 6, 30 wt.% glass
Nylons, as a group, are inert to most organic solvents. They resist alkalis and salt solutions and they are attacked by strong mineral acids and oxidizing agents. Data provided by the manufacturer,..
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | Short Term; ASTM D149 |
|
Quadrant EPP Nylatron® MC® 901 Blue, Heat Stabilized, Type 6 (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic ProductsBroadest size range availabilityGood mechanical and electrical propertiesIdeal balance of strength and toughnessCast as finished parts and near ..
|
|||
| Dielectric Strength |
19.7
kV/mm <br>@Thickness 3.17 mm
|
500
kV/in <br>@Thickness 0.125 in
|
|
|
Ineos Nova 3100 General Purpose Crystal Polystyrene
Good balance of flow and set-up properties, Good crack resistanceApplications: Single service cutlery, Single service drinkware, Consumer electronic packagingExposure to gamma radiation in the 2.02-..
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill® PA6/6 GF33 L UV 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceTPCI# 82..
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill® PA6/6 GF43 HS L BK001 43% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc..
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill® PA6/6 GF45 L BK 45% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackProcessing Method: Injection M..
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill® PA6/6 GF55 HS L BK 55% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu..
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill® POM CO GF25 CC 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 25% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc.
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | |
|
Saint-Gobain COHRlastic® CF4451 High Surface Resistivity Reinforced Solid Rubber
Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction..
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES Luriblend® PA6/6 GF30 IM TL15 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resi..
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES Luriblend® PA6/6 GF43 ML2 43% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 43% Filler by WeightAdditive: Molybdenum Disulfide Lubricant(2%)Features: LubricatedInformation provided by TP Composites,..
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES Luriblend® PE 5902
Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingInformation provided by TP Composites, Inc...
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES Luriblend® PE 5903
Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingInformation provided by TP Composites, Inc...
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill FR® PA6 GF13 FR-N BK 13% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu..
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill® PA6/6 LGF60 HS L BK 12 mm
Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass FiberAdditive: Lubricant, UV Stabilized and Heat StabilizerFeatures: Lubricated and Heat StabilizedProcessing Method: Inject..
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | |
|
Saint-Gobain COHRlastic® 700 General Purpose Silicone Solid Rubber
Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome..
|
|||
| Dielectric Strength | >= 19.7 kV/mm | >= 500 kV/in | Compound; ASTM D149 |
|
Borealis Casico™ FR4803 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing
Borstar FR4803 is a natural, thermoplastic polyolefin compound designed for flame retardant low voltage wire insulation and jacketing. As such, FR4803 offers a unique combination of good extrusion p..
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | 1/2" dia spheres; ASTM D877-87 |
|
3M CC-2 Cable Cleaning Preparation Kits
3M CC series Cable Cleaning Solvent is a full strength non-ozone depleting solvent cleaner, degreaser for use as an effective replacement for 1,1,1-Trichloroethane and other hazardous solvents, Form..
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | 1/2" dia spheres; ASTM D877-87 |
|
3M CC-4 Cleaning Solvent
3M CC series Cable Cleaning Solvent is a full strength non-ozone depleting solvent cleaner, degreaser for use as an effective replacement for 1,1,1-Trichloroethane and other hazardous solvents, Form..
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | |
|
3M MDT Tubing
3M MDT Tubing offers increased flexibility in combination with excellent abrasion, corrosion and environmental resistance properties and meets MIL-DTL-23053/15, Class 2. Uncoated product (without se..
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | |
|
Covestro Desmopan® 453 Urethane Thermoplastic Elastomer
(discontinued **)
Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially ..
|
|||
| Dielectric Strength |
19.7
kV/mm <br>@Thickness 3.17 mm
|
500
kV/in <br>@Thickness 0.125 in
|
|
|
Ineos Nova 6260 Super High Impact Polystyrene
(discontinued **)
Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined..
|
|||
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES Luriblend® POM CO GF20 TL20 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: PTFE LubricantFeatures: Lubricated and CopolymerInformation provided by TP Composites, Inc.
|
|||
| Dielectric Strength |
19.7
kV/mm <br>@Thickness 3.17 mm
|
500
kV/in <br>@Thickness 0.125 in
|
|
|
Ineos Nova 6110 Super High Impact Polystyrene
(discontinued **)
Good balance of gloss and impact, High glossApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection molded specimen..
|
|||
| Dielectric Strength | 19.7 - 25.0 kV/mm | 500 - 635 kV/in | Average value: 21.1 kV/mm Grade Count:11 |
|
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..
|
|||