| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength |
21.0
kV/mm <br>@Thickness 1.60 mm
|
533
kV/in <br>@Thickness 0.0630 in
|
in oil; ASTM D149 |
|
SABIC Innovative Plastics Lexan® BFL2000 PC
Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors.
|
|||
| Dielectric Strength |
21.0
kV/mm <br>@Thickness 3.18 mm
|
533
kV/in <br>@Thickness 0.125 in
|
ASTM D149 |
|
Solvay Specialty Polymers Amodel® A-1230 L Polyphthalamide (PPA)
(discontinued **)
Amodel A-1230 L is a 30% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten..
|
|||
| Dielectric Strength |
21.0
kV/mm <br>@Thickness 2.00 mm
|
533
kV/in <br>@Thickness 0.0787 in
|
ASTM D149 |
|
Nilit Nilamid A3 H G6 General Purpose 30% Glass Reinforced PA66
Description: Nilamid A3 H G6 is a general purpose 30% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi..
|
|||
| Dielectric Strength |
21.0
kV/mm <br>@Thickness 1.60 mm
|
533
kV/in <br>@Thickness 0.0630 in
|
in oil; ASTM D149 |
|
SABIC Innovative Plastics Lexan® BFL2000 PC (Europe-Africa-Middle East)
Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors.
|
|||
| Dielectric Strength | 21.0 - 60.0 kV/mm | 533 - 1520 kV/in | Average value: 31.3 kV/mm Grade Count:20 |
|
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
|
|||
| Dielectric Strength |
21.0
kV/mm <br>@Thickness 1.00 mm
|
533
kV/in <br>@Thickness 0.0394 in
|
ASTM D149 |
|
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance
Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical
|
|||
| Dielectric Strength |
21.0
kV/mm <br>@Thickness 1.00 mm
|
533
kV/in <br>@Thickness 0.0394 in
|
ASTM D149 |
|
LG Chemical LUMID GN1001AF PA6, Halogen Free Flame Retardant
Feature: Injection Molding, PA6, Halogen Free Flame RetardantApplication: Electrical & Electronic (Switch)CAS No. 25038-54-4 and 37640-57-6Information provided by LG Chemical
|
|||
| Dielectric Strength |
21.0
kV/mm <br>@Thickness 1.00 mm
|
533
kV/in <br>@Thickness 0.0394 in
|
ASTM D149 |
|
LG Chemical LUMID GP2259AFL PA6+GF25%, Flame Retardant
Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Connector)CAS No. 25038-54-4, 65997-17-3, 1163-19-5, 1309-64-4 and 138265-88-0Information provided by LG Chemical
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149 |
|
Kolon KOPA® KN333G25CRBK G/F Reinforced Nylon 66
EG-resistant, high strength, dimensionally stableApplications Cooling water pipesInformation provided by API-Kolon.
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149 |
|
Kolon KOPA® KN333G30HS G/F Reinforced Nylon 66
High thermal resistant, high strength, dimensionally stableApplications Transmission gear supportersInformation provided by API-Kolon.
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149 |
|
Kolon KOPA® KN333G45 G/F Reinforced Nylon 66
G/F 45% reinforcedApplications Internal gearsInformation provided by API-Kolon.
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | |
|
Momentive Performance Materials TSE3221 Clear Adhesive Sealant, Non-Corrosive Flowable
One-part heat cure. Typical uses: General sealing, potting, and coating when visual clarity is needed.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Perform..
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | |
|
Momentive Performance Materials TSE3940 Flame Retardant Adhesive Sealant, Gray
TSE3940 and TSE3941 flame retardant adhesive/sealants are non-flowable, one-component RTVs that cure quickly by reacting with atmospheric moisture forming a soft elastic silicone rubber. These mater..
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | |
|
Momentive Performance Materials TSE3940 Gray Adhesive Sealant, Fast Cure Paste
One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Flame retardant, no..
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149/DIN 53481 |
|
Kolon KOPA® KN133G15 G/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149/DIN 53481 |
|
Kolon KOPA® KN133G50 G/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | IEC 60243-1 |
|
Lanxess Pocan® BF 8230 000000 PBT, 30% Glass Fiber
PBT, 30% glass spheres/glass fibers, injection molding, flame retardant, low tendency to warp, improved surface finish
|
|||
| Dielectric Strength |
21.0
kV/mm <br>@Thickness 3.20 mm
|
533
kV/in <br>@Thickness 0.126 in
|
ASTM D149 |
|
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)
Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th..
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149 |
|
Samyang Tramid® 210G15 Polyamide, Reinforced
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210G15 is a reinforced grade.Applications:Automotive gear level housingConnectors..
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149 |
|
Samyang Tribit® 1500G15K PBT, Reinforced Impact
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G15K is a reinforced, impact grade.Appl..
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | IEC 243 |
|
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre..
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | IEC 60243-1 |
|
Polyplastics Duranex® 7400F Polybutylene Terephthalate (PBT), Low friction, Low wear, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | AC rapid rise in air; ASTM D149 |
|
DuPont™ Nomex® Type 993, 40 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ..
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® TSG-30/4 PA666-GF30
Product description: Grilon TSG-30/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30/4 has the following important properties: Good flo..
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® TSG-30/4 W PA666-GF30
Product description: Grilon TSG-30/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® TSM-30/2 PA666-MD30
Product description: Grilon TSM-30/2 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral filler. Grilon TSM-30/2 has the following important properties: Excell..
|
|||
| Dielectric Strength |
21.0
kV/mm <br>@Thickness 2.00 mm
|
533
kV/in <br>@Thickness 0.0787 in
|
ASTM D149 |
|
Beijing Chemical Industry KAIFA® 304-GO0 PBT Resin
Flame retardant, low bleeding, UV-resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Dielectric Strength | 21.0 kV/mm | 533 kV/in | IEC 60243-1 |
|
DSM Arnitel® PM581 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||