Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 600 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 23.6 kV/mm
600 kV/in
in oil; ASTM D149
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced
Polyetherimide, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
Dielectric Strength 23.6 kV/mm
600 kV/in
Short Term; ASTM D149
Quadrant EPP Duratron® PAI T4503 Compression Molded, Polyamide-imide, Eelectrical Grade (ASTM Product Data Sheet)
Dielectric Strength 23.6 kV/mm
600 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® HDPE TM10 10% Talc Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightInformation provided by TP Composites, Inc.
Dielectric Strength 23.6 kV/mm
600 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® HTN GF HS L High Temp Nylon 50% Glass Filled
Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Heat ResistanceInformation provided by TP Composit..
Dielectric Strength 23.6 kV/mm
600 kV/in
Saint-Gobain CHR® SG03-05(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Dielectric Strength 23.6 kV/mm
600 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill FR® PA4/6 GF15 FR HS L 15% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat St..
Dielectric Strength 23.6 kV/mm

@Thickness 3.17 mm
600 kV/in

@Thickness 0.125 in
Master Bond MasterSil 707FR Flame Retardant Silicone Adhesive
Description: MasterSil 707FR is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It is UL listed with a flame classification for 94V-1 for thicknesses of ..
Dielectric Strength 23.6 kV/mm

@Thickness 3.17 mm
600 kV/in

@Thickness 0.125 in
Master Bond MasterSil 708FR One Part, Flame Resistant Silicone
Description: MasterSil 708FR is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It is UL listed with a flame classification for 94V.1 for thicknesses of ..
Dielectric Strength 23.6 kV/mm
600 kV/in
ASTM D149
Westlake Plastics Propylux® Polypropylene
Propylux is made from polypropylene resin. Among its most notable characteristics are its mechanical toughness, chemical resistance and resistance it abrasion. These properties makes it suitable f..
Dielectric Strength 23.6 kV/mm
600 kV/in
Test run on 1/8" specimens.
Loctite® Durabond® E-20NS Epoxy Adhesive
Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli..
Dielectric Strength 23.6 kV/mm
600 kV/in
Cytec (Conap) FR-1080 Conapoxy® Resin / Conacure® Hardener
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an..
Dielectric Strength 23.6 kV/mm

@Thickness 1.59 mm,
Temperature 25.0 °C
600 kV/in

@Thickness 0.0625 in,
Temperature 77.0 °F
Cytec EN-12 (Conap) Casting, Potting, and Molding Compound
High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable..
Dielectric Strength 23.6 kV/mm
600 kV/in
ASTM D149
Arlon 51106RB015D Silicone Rubber/Fiberglass Laminate
Interleave 2: 3 mil PE; Side 2: cured silicone rubber; Substrate: 7628 fiberglass; Side 1: uncured silicone rubber, Interleave 1: 3 mil PE
Dielectric Strength 23.6 kV/mm
600 kV/in
ASTM D149
Arlon 51586R015H 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production mat..
Dielectric Strength 23.6 kV/mm
600 kV/in
ASTM D149
Arlon R35928R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: ..
Dielectric Strength 23.6 kV/mm
600 kV/in
ASTM D149
Arlon R35948R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberThis data re..
Dielectric Strength 23.6 kV/mm
600 kV/in
3M Scotch-Weld™ 183 B/A Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flowable product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent e..
Dielectric Strength 23.6 kV/mm
600 kV/in
ASTM D149
Arlon 51228R015 Silicone Rubber/Fiberglass Laminate
Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber
Dielectric Strength 23.6 kV/mm
600 kV/in
ASTM D149
Arlon 51228R025 Silicone Rubber/Fiberglass Laminate
Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber
Dielectric Strength 23.6 kV/mm
600 kV/in
ASTM D149
Arlon 55638R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic..
Dielectric Strength 23.6 kV/mm
600 kV/in
3M Temflex™ 2155 Rubber Splicing Tape
Temflex 2155 Rubber Splicing Tape is a conformable self-fusing rubber electrical insulating tape. It is designed for low voltage electrical insulating and moisture sealing applications. Temflex 2155..
Dielectric Strength 23.6 kV/mm
600 kV/in
Fluid Resistance
3M TMW Tubing
3M TMW Tubing is a semi-rigid translucent heat-shrinkable polyolefin tubing that is co-extruded and selectively cross-linked with an integral, meltable inner wall. When heated in excess of 135°C th..
Dielectric Strength 23.6 kV/mm
600 kV/in
Average value: 23.6 kV/mm Grade Count:5
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma..
Copyright © lookpolymers.com All Rights Reserved