Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 660 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Dielectric Strength 26.0 kV/mm
660 kV/in
IEC 60243
Polimeri Europa Edistir RKL Polystyrene  (discontinued **)
UL94 V-0, flame retarded, high impact polystyrene. This grade is designed for the extrusion of flame retardant sheets, foils and profiles. Designation: Thermoplastics ISO 2897-PS-I,E,093-06-04-18App..
Dielectric Strength 26.0 kV/mm

@Thickness 2.50 mm
660 kV/in

@Thickness 0.0984 in
IEC 60243-1
Victrex® PEEK 450FE20 Polyetheretherketone, 20% PTFE
Product Description:High performance thermoplastic material, 20% filled with PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA foo..
Dielectric Strength 26.0 kV/mm

@Thickness 1.00 mm
660 kV/in

@Thickness 0.0394 in
ASTM D149
LG Chemical KEYFLEX BT 1047D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Dielectric Strength 26.0 kV/mm

@Thickness 1.00 mm
660 kV/in

@Thickness 0.0394 in
ASTM D149
LG Chemical KEYFLEX BT 1068D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Dielectric Strength 26.0 kV/mm
660 kV/in
ASTM D149
Kolon SPESIN® KP213G15HIBL Impact Resistant PBT Compound resin
G/F 15% + Impact resistantApplications: SwitchesInformation provided by API-Kolon.
Dielectric Strength 26.0 kV/mm

@Thickness 1.00 mm
660 kV/in

@Thickness 0.0394 in
ASTM D149
LG Chemical Lupox® GP2156FL PBT+GF15%
Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by..
Dielectric Strength 26.0 kV/mm
660 kV/in
IEC 60243
Solvay TECHNYL® A 221 PA66, Conditioned
Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef..
Dielectric Strength 26.0 kV/mm
660 kV/in
CEI 93
Solvay TECHNYLSTARâ„¢ A205 F Natural S PA66, Eh 50
TECHNYLSTAR A205 F NATURAL S is a polyamide 6.6 with low viscosity for fast cycle molding.Colors: it is supplied in natural color.Available in: Latin America and North AmericaMain Properties: High F..
Dielectric Strength 26.0 kV/mm
660 kV/in
IEC 60243
Solvay TECHNYL® A 205F PA66, Conditioned
Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities..
Dielectric Strength 26.0 kV/mm
660 kV/in
IEC 60243
Solvay TECHNYL® A 216 S30 PA66, 30% glass spheres, Conditioned
Description: Polyamide 66, reinforced with 30% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 S30 is used in all sectors of industry, offering an..
Dielectric Strength 26.0 kV/mm

@Thickness 2.00 mm
660 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
SABIC Innovative Plastics NORYL WCD851 PPE-TPE (Asia Pacific)
Flexible, strong flame-retardant, halogen-free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame retardant performance capable of meeting UL VW-..
Dielectric Strength 26.0 kV/mm
660 kV/in
IEC 60243-1
Polyplastics Duranex® 330HR Polybutylene Terephthalate (PBT), Hydrolysis resistant, Heat shock resistant, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Dielectric Strength 26.0 kV/mm
660 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® GM-4H PA*-MD40
Product description: Grivory GM-4H natural is a 40 % mineral reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. G..
Dielectric Strength 26.0 kV/mm
660 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® TSG-35/4 W black 9832 PA666-GF35
Product description: Grilon TSG-35/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Dielectric Strength 26.0 kV/mm
660 kV/in
IEC 60243-1
DuPont Performance Polymers Crastin® FG6129 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&lt
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6129 NC010 is an unreinforced high viscosity polybutylene..
Dielectric Strength 26.0 kV/mm
660 kV/in
IEC 60243-1
DuPont Performance Polymers Crastin® FG6130 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&lt
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6130 NC010 is an unreinforced medium high viscosity polyb..
Dielectric Strength 26.0 kV/mm
660 kV/in
IEC 60243-1
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by..
Dielectric Strength 26.0 kV/mm
660 kV/in
IEC 60243-1
DuPont Performance Polymers Crastin® S610SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&lt
Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has hig..
Dielectric Strength 26.0 kV/mm
660 kV/in
IEC 60243-1
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In..
Dielectric Strength 26.0 kV/mm
660 kV/in
CEI 60243-1
Addiplast Addinyl B2 E Flame Retardant Nylon 6
Flame retardant, halogen freeInformation provided by Addiplast.
Dielectric Strength 26.0 kV/mm

@Thickness 1.00 mm
660 kV/in

@Thickness 0.0394 in
IEC 60243
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned
Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance..
Dielectric Strength 26.0 kV/mm

@Thickness 1.00 mm
660 kV/in

@Thickness 0.0394 in
IEC 60243
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings..
Dielectric Strength 26.0 kV/mm

@Thickness 2.00 mm
660 kV/in

@Thickness 0.0787 in
ASTM D149
Beijing Chemical Industry KAIFA® MN301-G0 Nylon 66 Resin
High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
Dielectric Strength 26.0 kV/mm
660 kV/in
IEC 60243-1
DSM Arnite® TV4 460 KL PBT/PET Blend-30% Glass Reinforced (European Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Dielectric Strength 26.0 kV/mm
660 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® BRZ 334 H PA6
Product description: Grilon BRZ 334 H is a heat stabilized, medium viscosity, high impact modified PA6 extrusion grade. Grilon BRZ 334 H has the following important properties:High impact strength a..
Dielectric Strength 26.0 kV/mm

@Thickness 3.00 mm
660 kV/in

@Thickness 0.118 in
IEC 60243
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded
Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo..