| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | |
|
Plastcom SLOVAMID 6 GF 30 FRG 4 LW PA6, 30% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°..
|
|||
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | |
|
Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
|
|||
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | 1.6mm; ASTM D149 |
|
Kingfa JH820 Modified PC
Features:Excellent balance propertiesSuper high impact strengthHigh stiffnessGood size stabilityGood surface, high glossHigh transparencyApplications:Injection moldingHousehold applianceBusiness mac..
|
|||
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | 1.6mm; ASTM D149 |
|
Kingfa JH950-402 Flame Retardant PC/ABS Alloy
Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surfaceApplications:Small household appliance cabinetControllerSocketShell of a..
|
|||
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | ASTM D149/DIN 53481 |
|
Kolon KOLEFIN® KO133MT40 M/F Reinforced Polypropylene
KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica..
|
|||
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | VDE 0303 |
|
GEHR Plastics PPS-40GF Polyphenylene Sulfide, 40% Glass Fiber
The linear polyphenylensulfide belongs to the semi-crystalline materials and offers a very high mechanical capacity, thermal and chemical resistance distinguished at the same time, high dimensional ..
|
|||
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | ASTM D149 |
|
Kolon SPESIN® KP270BL General Purpose PBT Compound Resin
Excellent waterproofnessApplications: ConnectorsInformation provided by API-Kolon.
|
|||
| Dielectric Strength | 28.0 - 30.0 kV/mm | 711 - 762 kV/in | DIN 53481 |
|
Isoflon PC Polycarbonate
Good impact resistance among transparent materialsInformation provided by Isoflon.
|
|||
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243-1 |
|
Lanxess Pocan® B 3225 901510 PBT, 20% Glass Fiber
PBT, 20% glass fibers, injection molding
|
|||
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | |
|
LG Chemical 95HCTC SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Lighter, Cosmetic Container, ToothbrushCAS No. 9003-54-7Information provided by LG Chemical
|
|||
| Dielectric Strength |
28.0
kV/mm @Thickness 1.60 mm |
711
kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
|
SABIC Innovative Plastics ULTEM 1010FC PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant. Effective June, 2007 this grade will no longer be support..
|
|||
| Dielectric Strength |
28.0
kV/mm @Thickness 1.00 mm |
711
kV/in @Thickness 0.0394 in |
IEC 60243-1 |
|
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Dry
Information provided by Unitika Ltd.
|
|||
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243-1 |
|
DSM Arnite® B427 SE/R PBT-GF35 FR(17)
35% Glass Reinforced, Flame Retardant
|
|||
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | dry; IEC 60243-1 |
|
EMS-Grivory Grivory® TSS/4 PA666
Product description: Grilon TSS/4 is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/4 has the following important properties: Good flow behaviorEas..
|
|||
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243-1 |
|
DuPont Performance Polymers Crastin® SK642FR NC010 Polybutylene Terephthalate (PBT)
15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK642FR is a 15% glass fibre reinforced flame retardant polybutylene terephthalate for injection moulding.It has a UL94 V-0 ra..
|
|||
| Dielectric Strength | 28.0 - 30.0 kV/mm | 711 - 762 kV/in | Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1 |
|
Hippe PA 66 Nylon 66
The polyamide with high degree of hardness, stiffness, scuff strength and stability of shape under heat. Preferred polyamide for components subjected to high load and heat stress in electrical, mec..
|
|||
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | |
|
Covestro Makroblend® UT-640 G Polycarbonate + Polyester Blend
Key Features:Contains FillerHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 Septembe..
|
|||
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | Breakdown |
|
Advanced Ceramics MEXIM C ACL 2091
Mexim C has been specially formulated to give an expansion closely matched to that of copper. It has high electrical insulation properties and good mechanical strength, and finds increasing applicat..
|
|||
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | CEI 60243-1 |
|
Addiplast Addinyl A2 Nylon 66
Unreinforced, medium viscosityInformation provided by Addiplast.
|
|||
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243-1 |
|
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA)
(Unverified Data**)
Ixef 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 102..
|
|||
| Dielectric Strength |
28.0
kV/mm @Thickness 2.00 mm |
711
kV/in @Thickness 0.0787 in |
ASTM D149 |
|
Beijing Chemical Industry KAIFA® MN301-G20 Nylon 66 Resin
20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Dielectric Strength | >= 28.0 kV/mm | >= 711 kV/in | Transformer Oil; Ø 93x3mm; IEC 243-1 |
|
SYNTHOS Krasten® 552M High Impact Polystyrene
High impact grade with a wide range of Applications. Processed mainly by injection moulding. Production of consumer goods and technical parts subjected to increased mechanical stress. Good results i..
|
|||
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | dry; IEC 60243-1 |
|
EMS-Grivory Grivory® TS V0 PA666
Product description: Grilon TS V0 is an unreinforced, normal viscosity, self-extinguishing Polyamid 66 + Polyamide 6 injection molding grade. Grilon TS V0 is halogen free and free of red phosphorous..
|
|||