| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | |
|
Plastcom SLOVASTER® B1 GF 20 PBT, 20% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | |
|
Ineos ABS NOVODUR® P2L-AT ABS, Injection Grade
(discontinued **)
Injection molding grade, very easy flow, antistatic, high stiffness, high gloss.Applications: Telephones, household goods, disk and video housings, office equipment.Information provided by the manuf..
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | |
|
Cookson Group Plaskon® AMC2 (132.203) Epoxy Molding Compound
(discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound specifically formulated for packaging stress-sensitive devices in DIPs, SOICs, PLCCs and small QFPs. F..
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | |
|
Ineos ABS Lustran® H607AS
Contains antistatic additives,Property data per ISO test methods.
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | Conditioned; IEC 60243-1 |
|
Lanxess Durethan® BKV 30 G H2.0 900051 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance, good UV s..
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | ASTM D149 |
|
Samyang Trirex® 3500G30 Polycarbonate, 30% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | ASTM D149 |
|
Samyang Trirex® SF3200GNH20 Polycarbonate, Reinforced Non Halogen for Printers
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.SF3200GNH20 is a reinforced, non-halogen grade for Printers.Applications: Office Machi..
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | IEC 60243 |
|
Solvay TECHNYL® A 216 V15 Black 21N PA66, 15% glass fiber, DRY
Description: Polyamide PA66, reinforced with 15% of glass fiber, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 216 V15 is used in all sectors of industry, offer..
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | dry; IEC 60243-1 |
|
EMS-Grivory Grivory® BRZ 247 W PA6
Product description: Grilon BRZ 247 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 247 W has the following important properties: High flexibi..
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | dry; IEC 60243-1 |
|
EMS-Grivory Grivory® TSG-50 FA PA666-GF50
Information provided by EMS Grivory
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® TSG-50 FA PA666-GF50
Information provided by EMS Grivory
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | DAM; IEC 60243-1 |
|
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**)
Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact ApplicationsZytel FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been develop..
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® TR 90 UV PAMACM12
Product description: Grilamid TR 90 UV natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid 90 UV natural offers outstanding propert..
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | DIN 53481/VDE 0303 |
|
BASF Elastollan® C-80A Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen..
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | IEC 60243-1 |
|
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Conditioned)
Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | IEC 60243-1 |
|
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Conditioned)
Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | IEC 243-1 |
|
Azoty Tarnow™ Tarnamid® T-27 MF30 Polyamide 6 - Mineral Reinforced
30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani..
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | IEC 243-1 |
|
Azoty Tarnow™ Tarnamid® T-27 MW30 Polyamide 6 - Mineral Reinforced
30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani..
|
|||
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | |
|
Ineos ABS NOVODUR® P3TF ABS, Injection Grade
(discontinued **)
Injection molding grade, improved flow.Applications: Automotive industry: e.g. wheel trims, instrument panel components.Information provided by the manufacturer.Novodur is produced by Styrolution (2..
|
|||