| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | <= 1.00e+10 ohm-cm | <= 1.00e+10 ohm-cm | Teil 30; IEC 600093 / VDE 0303 |
|
Okulen® 1000 PE-UHMW, UV - stabilized
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | Moist |
|
Fujipoly Industries FLAT-5TV-10-.75 silicone rubber fusible tape
Information provided by Fujipoly Industries
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | Moist |
|
Fujipoly Industries FLAT-5TV-10-1.0 silicone rubber fusible tape
Information provided by Fujipoly Industries
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | cond.; IEC 60093 |
|
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
|
Solvay TECHNYL® C 216 V35 Black Z PA6, 35% glass fiber, Conditioned
Description: Polyamide PA6 , reinforced with 35 % of glass fiber, for injection molding.Available in: North AmericaProduct Applications: It has good mechanical properties, it is used in all sectors ..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
|
Solvay TECHNYL® C 502XT PA6, Conditioned
Description: Unreinforced polyamide 6, very high viscosity, for extrusion.Available in: Europe Product Applications: It is suitable for extruded semi-finished products, such as: Rods, profiles, shee..
|
|||
| Volume Resistivity | 1.00e+10 - 1.00e+11 ohm-cm | 1.00e+10 - 1.00e+11 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics LNP THERMOCOMP ECF62 PEI
LNP* THERMOCOMP* ECF62 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | ASTM D257 |
|
Techmer ES Statiblend® ABS LE
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Low Extractables and Semi ConductiveInformation provided by TP Composites, Inc.
|
|||
| Volume Resistivity | 1.00e+10 - 1.00e+12 ohm-cm | 1.00e+10 - 1.00e+12 ohm-cm | ASTM D257 |
|
Techmer ES Statiblend® PA6/6 GF20 AS BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Lubricant, Antistatic and Heat StabilizerFeatures: Antistatic, Heat Stabilized and Lubricate..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | |
|
Master Bond Mastersil 726 Conductive Silicone Compound for Heat Transfer
Master Bond Polymer System MasterSil 726 is a non-curing grease-like thermally conductive silicone compound. It is extremely stable, it will not dry out, cure, harden, or bleed, even after exposure ..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | dry; IEC 60093 |
|
EMS-Grivory Grivory® 2D 20 nat PA612
Product Description: Grilamid 2D 20 natural is an unmodified unreinforced, medium viscosity polyamide 612 (PA612), designed for injection molding as well as extrusion. It is characterized by the fol..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | conditioned; IEC 60093 |
|
EMS-Grivory Grivory® 2D 25 W 20 X nat PA612-I
Product Description: Grilamid 2D 25 W 20 X natural 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique pro..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | dry; IEC 60093 |
|
EMS-Grivory Grivory® 2S 20 nat PA610
Product Description: Grilamid 2S 20 natural is an unmodified medium viscosity polyamide 610 (PA610), designed for injection molding as well as extrusion. It is characterized by the following product..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | conditioned; IEC 60093 |
|
EMS-Grivory Grivory® ELX 40 HNZ TPA
Product description: Grilon ELX 40 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow moulding applications. Grilon ELX 40 H NZ has the follow..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | conditioned; IEC 60093 |
|
EMS-Grivory Grivory® XE 4181 black PA1010
Product description: Grilamid XE 4181 black 9992 is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4181 black 9992 is highly ..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
|
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Conditioned, 30% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
|
Akro-Plastic Akromid® B3 (2500) PA 6 Conditioned
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
|
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Conditioned, 60% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
|
|||
| Volume Resistivity |
1.00e+10
ohm-cm <br>@Thickness 3.00 mm
|
1.00e+10
ohm-cm <br>@Thickness 0.118 in
|
IEC 60093 |
|
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned
Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
|
BASF Ultramid® B3ZG3 BK 30564 15% Glass Filled PA6-1 (Conditioned)
Description: Impact-modified and 15% glass fiber reinforced injection-molding grade, for instance, for automotive cable conduits.Information provided by BASF
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
|
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Conditioned)
Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas..
|
|||
| Volume Resistivity |
1.00e+10
ohm-cm <br>@Temperature 100 °C
|
1.00e+10
ohm-cm <br>@Temperature 212 °F
|
|
|
Atom Adhesives AA-BOND 2104 Epoxy Adhesive
AA-BOND 2104 is a thixotropic epoxy system recommended for critical electronics, aerospace and industrial bonding, laminating and reinforcing applications requiring an adhesive with high-fill, non-s..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
|
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Conditioned)
Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability.
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
|
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Conditioned)
Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
|
BASF Ultramid® A3XZG5 BK 23187 25% Glass Filled PA66 FR (Conditioned)
Description: Impact-modified, 25% glass-fiber reinforced injection-molding grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; for compone..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | conditioned; IEC 60093 |
|
EMS-Grivory Grivory® XE 4208 black 9992 PA612-I
Product description: Grilamid XE 4208 black 9992 is a semiflexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) extrusion grade. Unique properties of Gril..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
|
BASF Ultramid® B3S BK00464 PA6 (Conditioned)
Description: Easy flowing, finely crystalline injection-molding grade for very fast processing. Uses include thin-walled technical parts (eg. housings, fittings, grips, small parts and fixing clamps..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
|
Solvay TECHNYL® 1011R PA6, Conditioned
Description: Polyamide 6, Unfilled, lubricated, for injection molding. Available in: Asia Pacific Product Applications: TECHNYL® 1011R is used in all sectors of industry, offering an excellent flow..
|
|||
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
|
Solvay TECHNYL® 1021ST PA6, Conditioned
Description: Polyamide 6, unfilled, super tough impact modified, for injection moldingAvailable in: Asia Pacific Product Applications: TECHNYL® 102ST has the highest level impact strength and balan..
|
|||