| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | STN IEC 60093 |
|
Plastcom SLOVAMID 66 GF 25 FRG 5 Polyamide 66, 25% Glass Fiber, Halogen Free Flame Retardant
FeaturesPA 66 for injection moulding, chemical reinforced with 25% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal..
|
|||
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | STN IEC 60093 |
|
Plastcom SLOVASTER® B GF 20 Polybutylene Terephthalate, 20% Glass Fiber
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a..
|
|||
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS
Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications.
|
|||
| Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics Lexan® 124R PC
UL rated HB. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no l..
|
|||
| Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics Lexan® 923 PC (Asia Pacific)
Opaque colors, low viscosity, superior flame retardance. Decreased smoke and lowered toxic gas emission. UV-stabilized.
|
|||
| Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics Lexan® 923A PC
Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized.
|
|||
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
|
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant
Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
|
|||
| Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics Lexan® LI1813R PC
Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release and UV-stabilized.
|
|||
| Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East)
XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
|
|||
| Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics Lexan® 101 PC
UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated, 7.0 MFR, for thicker sections without sinks.
|
|||
| Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics Lexan® 953A PC (Asia Pacific)
Clear, tints and opaque colors, high viscosity, flame retardant with exceptional surface. UV-stabilized.
|
|||
| Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics Lexan® HP4 PC
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mol..
|
|||
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics ULTEM 1010 PEI
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer b..
|
|||
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D 257 |
|
SABIC Innovative Plastics Ultem 1010FV PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa..
|
|||
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics ULTEM HU1010 PEI
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),..
|
|||
| Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
|
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer
Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc..
|
|||
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D 257 |
|
SABIC Innovative Plastics Noryl LS175 PPE+HIPS (Europe-Africa-Middle East)
Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del..
|
|||
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM3020 PPE+PS
LNP* Thermocomp* Noryl_FM3020 compound is GR/MR 30%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness.
|
|||
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
|
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue
Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature..
|
|||
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
|
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue
Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature..
|
|||
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | 1/16''; ASTM D257 |
|
Ensinger TECAPEI® 10% Glass Reinforced, made from Ultem® 2100 PEI
TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in..
|
|||
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
|
Entec Hylex® P1017L1 HB Polycarbonate
Available in North America Additive: Mold Release Features: Good Mold Release and High Flow RoHS Compliant Form: Pellets Appearance: Clear/Transparent Information provided by Entec
|
|||
| Volume Resistivity |
1.00e+17
-
1.00e+18
ohm-cm @Temperature 23.0 °C |
1.00e+17
-
1.00e+18
ohm-cm @Temperature 73.4 °F |
ASTM D257 |
|
DuPont Performance Polymers VESPEL TP-8169 Polyimide
DuPont Vespel TP-8169 parts are specified for high-temperature applications. TP-8169 parts offer a unique balance of mechanical and thermal properties for high performance in aggressive environments..
|
|||
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
|
Beijing Chemical Industry KAIFA® HN301-G10 PA6 Resin
10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
|
Asahi Glass F-Clean® Film for Greenhouses
F-CLEAN®, produced by Asahi Glass Company, Ltd., is a Ethylene-Tetrafluoroethylene copolymer (ETFE) film used as the preferred covering material for horticultural greenhouses. High ten..
|
|||
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
|
Beijing Chemical Industry KAIFA® MN301-M30 Nylon 66 Resin
Mineral filled, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | D257 |
|
Zhejiang Juner PC-3-1 Alloy
Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
|
|||
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics Lexan® FR65 Polycarbonate Film, Flame Retardant
Lexan FR65 flame-retardant film is a clear, thin-gauge polycarbonate film with a velvet finish on one side and a matt finish on the other, and a UL94 V-0 listing to meet the stringent requirements i..
|
|||