Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Volume Resistivity = 2.00e+17 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. ..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
SABIC Innovative Plastics LNP COLORCOMP DX04401H PC
LNP* COLORCOMP* DX04401H is an unfilled Polycarbonate. Added feature of this grade is: Healthcare.
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics simil..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
LG Chemical Lupoy 1200-15 Polycarbonate Resin
Description: LUPOY PC 1200-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
LG Chemical Lupoy 1201-10 Polycarbonate Resin
Description: LUPOY PC 1201-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
LG Chemical Lupoy 1300-15 Polycarbonate Resin
Description: LUPOY PC 1300-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
LG Chemical Lupoy 1301EP30 Polycarbonate Resin
Description: LUPOY PC 1301EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
LG Chemical Lupoy 1301V-7 Polycarbonate Resin
Description: LUPOY PC 1301V-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
LG Chemical Lupoy 1302-05 Polycarbonate Resin
Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
LG Chemical Lupoy NF1007F 10R Polycarbonate Resin
Description: LUPOY NF 1007F10R, eco-friendly UL94 V0/3.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
LG Chemical Lupoy NF1009F 15 Polycarbonate Resin
Description: LUPOY NF 1009F15, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpare..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
LG Chemical Lupoy 1201HP-08 Polycarbonate Resin
Description: LUPOY PC 1201HP-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
LG Chemical Lupoy 1302HP-09 Polycarbonate Resin
Description: LUPOY PC 1302HP-09 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin
Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
LG Chemical Lupoy 1302HP-21 Polycarbonate Resin
Description: LUPOY PC 1302HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
LG Chemical Lupoy 1303-15 Polycarbonate Resin
Description: LUPOY PC 1303-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
Torlon® 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate partic..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)
Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PA..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
50% RH; ASTM D257
Specialty Coating Systems Parylene HT® Poly (P-Xylylene) Coating
Parylene HT is a polymer of para-xylylene with the alpha hydrogen atoms of the N dimer replaced with fluorine. This variant of Parylene is useful in high temperature applications (short term up to 4..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Styron CALIBREâ„¢ 201-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 201-15 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Styron CALIBREâ„¢ 201-22 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Styron CALIBREâ„¢ 2061 HD 15 Polycarbonate Resin
Overview: CALIBREâ„¢ 2061 HD 15 Polycarbonate Resins are designed for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061 HD 15 Polycarbonate Resins offer a ..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Styron CALIBREâ„¢ 303V-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 300V-10 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products are avai..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Styron EMERGEâ„¢ 4330-22 Polycarbonate
EMERGEâ„¢ PC 4330-22 advanced resin is high-performance polycarbonate resin offering ultraviolet light stability, high heat resistance, toughness, and superior flow. Applications: Consumer Elec..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Styron CALIBREâ„¢ 2061-6 Polycarbonate
CALIBREâ„¢ 2061-6 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and ..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
IEC 60093
Styron CALIBREâ„¢ 302EP-22 Polycarbonate Resin
Overview: CALIBREâ„¢ 300EP-22 Series are polycarbonate resins that offer exceptional impact resistance, heat distortion resistance and optical clarity for injection molding applications. Their hi..
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Styron CALIBREâ„¢ 303 EP Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Styron CALIBREâ„¢ 303-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Styron CALIBREâ„¢ MEGARAD 2081-HD-15 2 Polycarbonate Resin
Overview: CALIBREâ„¢ MEGARAD 2081 HD-15 2 polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed ..
Copyright © lookpolymers.com All Rights Reserved